摘要:
A high-strength stainless steel for oil well having corrosion resistance excellent in a high-temperature environment, having excellent SSC resistance at normal temperature, and having better workability than 13% Cr steels has a chemical composition containing, by mass percent, C: at most 0.05%, Si: at most 1.0%, Mn: at most 0.3%, P: at most 0.05%, S: less than 0.002%, Cr: over 16% and at most 18%, Mo: 1.5 to 3.0%, Cu: 1.0 to 3.5%, Ni: 3.5 to 6.5%, Al: 0.001 to 0.1%, N: at most 0.025%, and O: at most 0.01%, the balance being Fe and impurities, a microstructure containing a martensite phase, 10 to 48.5%, by volume ratio, of a ferrite phase and at most 10%, by volume ratio, of a retained austenite phase, yield strength of at least 758 MPa and uniform elongation of at least 10%.
摘要:
A stainless steel for an oil country tubular good according to the invention includes, in percent by mass, 0.001% to 0.05% C, 0.05% to 1% Si, at most 2% Mn, at most 0.03% P, less than 0.002% S, 16% to 18% Cr, 3.5% to 7% Ni, more than 2% and at most 4% Mo, 1.5% to 4% Cu, 0.001% to 0.3% rare earth metal, 0.001% to 0.1% sol. Al, 0.0001% to 0.01% Ca, at most 0.05% O, and at most 0.05% N, and the balance consists of Fe and impurities. The stainless steel according to the invention includes REM and therefore has high SCC resistance in a high temperature chloride aqueous solution environment.
摘要:
The chemical composition of a stainless steel in accordance with the present invention consists of C: not more than 0.05%, Si: not more than 0.5%, Mn: 0.01 to 0.5%, P: not more than 0.04%, S: not more than 0.01%, Cr: more than 16.0 and not more than 18.0%, Ni: more than 4.0 and not more than 5.6%, Mo: 1.6 to 4.0%, Cu: 1.5 to 3.0%, Al: 0.001 to 0.10%, and N: not more than 0.050%, the balance being Fe and impurities, and satisfies Formulas (1) and (2). Also, the micro-structure thereof contains a martensitic phase and a ferritic phase having a volume ratio of 10 to 40%, and the ferritic phase distribution ratio is higher than 85%. Cr+Cu+Ni+Mo≧25.5 (1) −8≦30(C+N)+0.5Mn+Ni+Cu/2+8.2−1.1(Cr+Mo)≦−4 (2)
摘要翻译:根据本发明的不锈钢的化学组成由C:不大于0.05%,Si:不大于0.5%,Mn:0.01至0.5%,P:不大于0.04%,S:不大于 0.01%以上,Cr:16.0以上18.0%以下,Ni:4.0以上5.6%以下,Mo:1.6〜4.0%,Cu:1.5〜3.0%,Al:0.001〜0.10% N:不大于0.050%,余量为Fe和杂质,并满足式(1)和(2)。 此外,其微结构含有马氏体相和体积比为10〜40%的铁素体相,铁素体相分布比高于85%。 Cr + Cu + Ni +Mo≥25.5(1)-8≦̸ 30(C + N)+ 0.5Mn + Ni + Cu / 2 + 8.2-1.1(Cr + Mo)≦̸ -4(2)
摘要:
The problem to be solved is the provision of a high-strength stainless steel pipe having a sufficient corrosion resistance in a high-temperature carbonic acid gas environment and having an excellent sulfide stress cracking resistance at normal temperature. A high-strength stainless steel pipe consist of, by mass %, C: 0.05% or less, Si: 1.0% or less, P: 0.05% or less, S: less than 0.002%, Cr: more than 16% and 18% or less, Mo: more than 2% and 3% or less, Cu: 1% to 3.5%, Ni: 3% or more and less than 5%, Al: 0.001% to 0.1% and O: 0.01% or less, Mn: 1% or less and N: 0.05% or less, and Mn and N in the above ranges satisfy formula (1), and the balance being Fe and impurities; and the metal micro-structure of the stainless steel pipe mainly includes a martensitic phase and comprises 10 to 40% of a ferritic phase by volume fraction and 10% or less of a retained γ-phase by volume fraction. [Mn]×([N]−0.0045)≦0.001 (1) wherein the symbols of elements in formula (1) respectively represent the contents (unit: mass %) of the elements in the steel.
摘要:
A high-strength stainless steel for oil well having corrosion resistance excellent in a high-temperature environment, having excellent SSC resistance at normal temperature, and having better workability than 13% Cr steels has a chemical composition containing, by mass percent, C: at most 0.05%, Si: at most 1.0%, Mn: at most 0.3%, P: at most 0.05%, S: less than 0.002%, Cr: over 16% and at most 18%, Mo: 1.5 to 3.0%, Cu: 1.0 to 3.5%, Ni: 3.5 to 6.5%, Al: 0.001 to 0.1%, N: at most 0.025%, and O: at most 0.01%, the balance being Fe and impurities, a microstructure containing a martensite phase, 10 to 48.5%, by volume ratio, of a ferrite phase and at most 10%, by volume ratio, of a retained austenite phase, yield strength of at least 758 MPa and uniform elongation of at least 10%.
摘要:
The problem to be solved is the provision of a high-strength stainless steel pipe having a sufficient corrosion resistance in a high-temperature carbonic acid gas environment and having an excellent sulfide stress cracking resistance at normal temperature.A high-strength stainless steel pipe consist of by mass %, C: 0.05% or less, Si: 1.0% or less, P: 0.05% or less, S: less than 0.002%, Cr: more than 16% and 18% or less, Mo: more than 2% and 3% or less, Cu: 1% to 3.5%, Ni: 3% or more and less than 5%, Al: 0.001% to 0.1% and O: 0.01% or less, Mn: 1% or less and N: 0.05% or less, and Mn and N in the above ranges satisfy formula (1), and the balance being Fe and impurities; and the metal micro-structure of the stainless steel pipe mainly includes a martensitic phase and comprises 10 to 40% of a ferritic phase by volume fraction and 10% or less of a retained γ-phase by volume fraction. [Mn]×([N]−0.0045)≦0.001 (1) wherein the symbols of elements in formula (1) respectively represent the contents (unit: mass %) of the elements in the steel.
摘要:
A martensitic stainless steel for welded structures including by mass %, C: 0.001 to 0.05%, Si: 0.05 to 1%, Mn: 0.05 to 2%, P: 0.03% or less, REM: 0.0005 to 0.1%, Cr: 8 to 16%, Ni: 0.1 to 9% and sol. Al: 0.001 to 0.1%; and further including one or more elements selected from among Ti: 0.005 to 0.5%, Zr: 0.005 to 0.5%, Hf: 0.005 to 0.5%, V: 0.005 to 0.5% and Nb: 0.005 to 0.5%; and O: 0.005% or less, N: 0.1% or less, with the balance being Fe and impurities; and the P and REM content satisfies: P≦0.6×REM. This steel possesses excellent SCC (stress corrosion cracking) resistance in welded sections in Sweet environments.
摘要:
Provided is duplex stainless steel having high strength, SCC resistance and SSC resistance excellent in a high-temperature chloride environment, and capable of suppressing precipitation of a σ phase. The duplex stainless steel of the present embodiment includes, in mass %, of: C: at most 0.03%; Si: 0.2 to 1%; Mn: more than 5.0% to at most 10%; P: at most 0.040%; S: at most 0.010%; Ni: 4.5 to 8%; sol. Al: at most 0.040%; N: more than 0.2% to at most 0.4%; Cr: 24 to 29%; Mo: 0.5 to less than 1.5%; Cu: 1.5 to 3.5%; W: 0.05 to 0.2%; the balance being Fe and impurities, wherein the duplex stainless steel satisfies Formula (1): Cr+8Ni+Cu+Mo+W/2≥65 . . . (1), where a symbol of each element in Formula (1) represents a content of the element (in mass %).
摘要:
A duplex stainless steel excellent in the weldability during large heat input welding and in the stress corrosion cracking resistance in a chloride environment containing corrosive associated gases has a chemical composition consisting, by mass %, of C: 0.03% or less, Si: 0.2 to 1%, Mn: 5.0% or less, P: 0.040% or less, S: 0.010% or less, sol. Al: 0.040% or less, Ni: 4 to 8%, Cr: 20 to 28%, Mo: 0.5 to 2.0%, Cu: more than 2.0% and 4.0% or less and N: 0.1 to 0.35%, and optionally contains one or more selected from among V, Ca, Mg, B and a rare earth metal(s), with the balance being Fe and impurities; wherein the duplex stainless steel satisfies the following formulas: 2.2Cr+7Mo+3Cu>66 (1) Cr+11Mo+10Ni
摘要:
Provided is duplex stainless steel having high strength, SCC resistance and SSC resistance excellent in a high-temperature chloride environment, and capable of suppressing precipitation of a σ phase. The duplex stainless steel of the present embodiment includes, in mass %, of: C: at most 0.03%; Si: 0.2 to 1%; Mn: more than 5.0% to at most 10%; P: at most 0.040%; S: at most 0.010%; Ni: 4.5 to 8%; sol. Al: at most 0.040%; N: more than 0.2% to at most 0.4%; Cr: 24 to 29%; Mo: 0.5 to less than 1.5%; Cu: 1.5 to 3.5%; W: 0.05 to 0.2%; the balance being Fe and impurities, wherein the duplex stainless steel satisfies Formula (1): Cr+8Ni+Cu+Mo+W/2≧65 . . . (1), where a symbol of each element in Formula (1) represents a content of the element (in mass %).
摘要翻译:提供在高温氯化物环境中具有优异的高强度,耐SCC性和耐SSC性的双相不锈钢,并且能够抑制淀粉的沉淀。 相。 本实施方式的双相不锈钢以质量%计含有:C:0.03%以下, Si:0.2〜1% Mn:超过5.0%至至多10%; P:0.040%以下; S:0.010%以下; Ni:4.5〜8% 溶胶 Al:0.040%以下; N:0.2%以上0.4%以下; Cr:24〜29% Mo:0.5〜小于1.5% Cu:1.5〜3.5% W:0.05〜0.2% 余量为Fe和杂质,其中双相不锈钢满足式(1):Cr + 8Ni + Cu + Mo + W /2≥65。 。 。 (1)中,式(1)中的各元素的符号表示元素的含量(质量%)。