Method for Preparing Fiber-Reinforced Parts Based on Cyanate Ester/Epoxy Blends
    7.
    发明申请
    Method for Preparing Fiber-Reinforced Parts Based on Cyanate Ester/Epoxy Blends 审中-公开
    基于氰酸酯/环氧共混物制备纤维增强部件的方法

    公开(公告)号:US20160304684A1

    公开(公告)日:2016-10-20

    申请号:US15101295

    申请日:2014-12-04

    申请人: LONZA LTD

    摘要: The invention provides a method for preparing a fiber-reinforced part based on cyanate ester or a cyanate ester/epoxy blend, comprising the steps of (i) providing a liquid mixture comprising (a) from 15 to 99.9 wt. % of at least one di- or polyfunctional cyanate ester, (b) from 0 to 84.9 wt. % of at least one di- or polyfunctional epoxy resin, and (c) from 0.1 to 25 wt. % of a metal-free catalyst; (ii) providing a fiber structure (iii) placing said fiber structure in a mold or on a substrate, (iv) impregnating said fiber structore with said liquid mixture, (v) curing said liquid mixture by applying a temperature of 30 to 300° C. Using the method of the invention it is possible to produce in a short cycle time, using composite manufacturing processes such as resin transfer molding and infusion technology, fiber reinforced composite parts based on a cyanate ester or cyanate ester/epoxy resin formulation. The fiber-reinforced parts obtainable by the above method are also an object of the invention.

    摘要翻译: 本发明提供一种制备基于氰酸酯或氰酸酯/环氧共混物的纤维增强部分的方法,包括以下步骤:(i)提供液体混合物,其包含(a)15至99.9重量% %的至少一种二官能或多官能氰酸酯,(b)0至84.9wt。 %的至少一种二官能或多官能环氧树脂,和(c)0.1至25wt。 %的无金属催化剂; (ii)提供纤维结构(iii)将所述纤维结构置于模具或基材上,(iv)用所述液体混合物浸渍所述纤维结构体,(v)通过施加30至300℃的温度固化所述液体混合物 C.使用本发明的方法,可以使用诸如树脂传递模塑和输注技术的复合制造工艺,基于氰酸酯或氰酸酯/环氧树脂制剂的纤维增强复合材料部分在短的周期内生产。 通过上述方法可获得的纤维增强部件也是本发明的目的。