公开(公告)号:US09567451B2
公开(公告)日:2017-02-14
申请号:US13991377
申请日:2011-11-25
申请人: Masaki Satou , Takashi Shirokawa , Makoto Ashiura , Yoshihiro Kameda , Ayumi Naka , Keisuke Maejima
发明人: Masaki Satou , Takashi Shirokawa , Makoto Ashiura , Yoshihiro Kameda , Ayumi Naka , Keisuke Maejima
IPC分类号: B60C1/00 , C08C19/44 , C08L15/00 , C08K7/00 , C08C19/25 , C08G81/02 , C08K3/36 , C08L7/00 , C08L9/00
CPC分类号: C08K7/00 , B60C1/00 , B60C1/0016 , C08C19/25 , C08C19/44 , C08G81/02 , C08K3/36 , C08L7/00 , C08L9/00 , C08L15/00 , Y02T10/862
摘要: A rubber composition for use in tire treads comprises a diene rubber including not less than 40% by weight of a modified conjugated diene polymer rubber and, per 100 parts by weight of the diene rubber, from 66 to 110 parts by weight of a filler. The filler comprises not less than 50% by weight of silica. The modified conjugated diene polymer rubber is obtained by copolymerizing a conjugated diene monomer unit and an aromatic vinyl monomer unit in a hydrocarbon solvent using an organic active metal compound as an initiator. A resulting active conjugated diene polymer chain thereof has a terminal modified group, obtained by reacting at least one type of compound having a functional group that is reactable with the active terminal of the polymer chain. Moreover, the terminal modified group has a functional group that interacts with the silica.
摘要翻译: 用于轮胎胎面的橡胶组合物包括二烯橡胶,其包含不小于40重量%的改性共轭二烯聚合物橡胶,并且相对于每100重量份的二烯橡胶,含有66至110重量份的填料。 填料包含不少于50重量%的二氧化硅。 改性共轭二烯聚合物橡胶通过使用有机活性金属化合物作为引发剂在烃溶剂中共轭共轭二烯单体单元和芳族乙烯基单体单元而获得。 所得到的活性共轭二烯聚合物链具有末端改性基团,其通过使至少一种具有可与聚合物链的活性末端反应的官能团的化合物反应而获得。 此外,末端改性基团具有与二氧化硅相互作用的官能团。
-
公开(公告)号:US09416252B2
公开(公告)日:2016-08-16
申请号:US13991398
申请日:2011-11-25
申请人: Ayumi Naka , Takashi Shirokawa , Makoto Ashiura , Yoshihiro Kameda , Masaki Satou , Keisuke Maejima
发明人: Ayumi Naka , Takashi Shirokawa , Makoto Ashiura , Yoshihiro Kameda , Masaki Satou , Keisuke Maejima
CPC分类号: C08K7/00 , B60C1/0016 , C08C19/44 , C08K3/36 , C08L7/00 , C08L9/00 , C08L15/00 , Y02T10/862
摘要: A rubber composition comprises a diene rubber including not less than 25% by weight of a modified conjugated diene polymer rubber and, per 100 parts by weight of the diene rubber, from 25 to 65 parts by weight of a filler, the filler comprising not less than 50% by weight of silica. The silica has a DBP absorption number of 190 to 250 ml/100 g, an N2SA of 194 to 225 m/g, and a CTAB of 185 to 215 m2/g. A ratio of the N2SA to the CTAB is from 0.9 to 1.4. The modified conjugated diene polymer rubber has a terminal modified group including a functional group that interacts with the silica. In the modified conjugated diene polymer rubber, aromatic vinyl unit content is from 38% to 48% by weight, vinyl unit content is from 20% to 35%, and weight-average molecular weight is from 600,000 to 1,000,000.
摘要翻译: 橡胶组合物包括二烯橡胶,其包含不小于25重量%的改性共轭二烯聚合物橡胶,并且相对于每100重量份的二烯橡胶,25至65重量份的填料,所述填料不少于 超过50重量%的二氧化硅。 二氧化硅的DBP吸收值为190〜250ml / 100g,N 2 SA为194〜225m 2 / g,CTAB为185〜215m 2 / g。 N2SA与CTAB的比例为0.9〜1.4。 改性共轭二烯聚合物橡胶具有包含与二氧化硅相互作用的官能团的末端改性基团。 在改性共轭二烯聚合物橡胶中,芳香族乙烯基单元含量为38〜48重量%,乙烯基单元含量为20〜35重量%,重均分子量为60万〜100万。
-
公开(公告)号:US20140011909A1
公开(公告)日:2014-01-09
申请号:US13991377
申请日:2011-11-25
申请人: Masaki Satou , Takashi Shirokawa , Makoto Ashiura , Yoshihiro Kameda , Ayumi Naka , Keisuke Maejima
发明人: Masaki Satou , Takashi Shirokawa , Makoto Ashiura , Yoshihiro Kameda , Ayumi Naka , Keisuke Maejima
IPC分类号: C08K7/00
CPC分类号: C08K7/00 , B60C1/00 , B60C1/0016 , C08C19/25 , C08C19/44 , C08G81/02 , C08K3/36 , C08L7/00 , C08L9/00 , C08L15/00 , Y02T10/862
摘要: A rubber composition for use in tire treads comprises a diene rubber including not less than 40% by weight of a modified conjugated diene polymer rubber and, per 100 parts by weight of the diene rubber, from 66 to 110 parts by weight of a filler. The filler comprises not less than 50% by weight of silica. The modified conjugated diene polymer rubber is obtained by copolymerizing a conjugated diene monomer unit and an aromatic vinyl monomer unit in a hydrocarbon solvent using an organic active metal compound as an initiator. A resulting active conjugated diene polymer chain thereof has a terminal modified group, obtained by reacting at least one type of compound having a functional group that is reactable with the active terminal of the polymer chain. Moreover, the terminal modified group has a functional group that interacts with the silica.
摘要翻译: 用于轮胎胎面的橡胶组合物包括二烯橡胶,其包含不小于40重量%的改性共轭二烯聚合物橡胶,并且相对于每100重量份的二烯橡胶,含有66至110重量份的填料。 填料包含不少于50重量%的二氧化硅。 改性共轭二烯聚合物橡胶通过使用有机活性金属化合物作为引发剂在烃溶剂中共轭共轭二烯单体单元和芳族乙烯基单体单元而获得。 所得到的活性共轭二烯聚合物链具有末端改性基团,其通过使至少一种具有可与聚合物链的活性末端反应的官能团的化合物反应而获得。 此外,末端改性基团具有与二氧化硅相互作用的官能团。
-
公开(公告)号:US20130338255A1
公开(公告)日:2013-12-19
申请号:US13991398
申请日:2011-11-25
申请人: Ayumi Naka , Takashi Shirokawa , Makoto Ashiura , Yoshihiro Kameda , Masaki Satou , Keisuke Maejima
发明人: Ayumi Naka , Takashi Shirokawa , Makoto Ashiura , Yoshihiro Kameda , Masaki Satou , Keisuke Maejima
IPC分类号: C08K7/00
CPC分类号: C08K7/00 , B60C1/0016 , C08C19/44 , C08K3/36 , C08L7/00 , C08L9/00 , C08L15/00 , Y02T10/862
摘要: A rubber composition comprises a diene rubber including not less than 25% by weight of a modified conjugated diene polymer rubber and, per 100 parts by weight of the diene rubber, from 25 to 65 parts by weight of a filler, the filler comprising not less than 50% by weight of silica. The silica has a DBP absorption number of 190 to 250 ml/100 g, an N2SA of 194 to 225 m/g, and a CTAB of 185 to 215 m2/g. A ratio of the N2SA to the CTAB is from 0.9 to 1.4. The modified conjugated diene polymer rubber has a terminal modified group including a functional group that interacts with the silica. In the modified conjugated diene polymer rubber, aromatic vinyl unit content is from 38% to 48% by weight, vinyl unit content is from 20% to 35%, and weight-average molecular weight is from 600,000 to 1,000,000.
摘要翻译: 橡胶组合物包括二烯橡胶,其包含不小于25重量%的改性共轭二烯聚合物橡胶,并且相对于每100重量份的二烯橡胶,25至65重量份的填料,所述填料不少于 超过50重量%的二氧化硅。 二氧化硅的DBP吸收值为190〜250ml / 100g,N 2 SA为194〜225m 2 / g,CTAB为185〜215m 2 / g。 N2SA与CTAB的比例为0.9〜1.4。 改性共轭二烯聚合物橡胶具有包含与二氧化硅相互作用的官能团的末端改性基团。 在改性共轭二烯聚合物橡胶中,芳香族乙烯基单元含量为38〜48重量%,乙烯基单元含量为20〜35重量%,重均分子量为60万〜100万。
-
公开(公告)号:US10072138B2
公开(公告)日:2018-09-11
申请号:US13991414
申请日:2011-11-25
CPC分类号: C08L15/00 , B60C1/0016 , C08C19/25 , C08C19/44 , C08F236/10 , C08K3/36 , C08L57/02 , Y02T10/862
摘要: A rubber composition comprises a diene rubber including not less than 30% by weight of a modified conjugated diene polymer rubber and, per 100 parts by weight of the diene rubber, from 1 to 25 parts by weight of a tackifying resin, and from 25 to 80 parts by weight of a filler comprising not less than 50% by weight of silica. The modified conjugated diene polymer rubber has a terminal modified group comprising a functional group that interacts with silica. In the modified conjugated diene polymer rubber, aromatic vinyl unit content is from 38% to 48% by weight, vinyl unit content is from 20% to 35%, weight-average molecular weight is from 600,000 to 1,000,000, and glass transition temperature is from −22 to −32° C. A glass transition temperature of the tackifying resin is from 50 to 110° C. higher than the glass transition temperature of the modified conjugated diene polymer rubber.
-
公开(公告)号:US20130324638A1
公开(公告)日:2013-12-05
申请号:US13991414
申请日:2011-11-25
IPC分类号: C08L15/00
CPC分类号: C08L15/00 , B60C1/0016 , C08C19/25 , C08C19/44 , C08F236/10 , C08K3/36 , C08L57/02 , Y02T10/862
摘要: A rubber composition comprises a diene rubber including not less than 30% by weight of a modified conjugated diene polymer rubber and, per 100 parts by weight of the diene rubber, from 1 to 25 parts by weight of a tackifying resin, and from 25 to 80 parts by weight of a filler comprising not less than 50% by weight of silica. The modified conjugated diene polymer rubber has a terminal modified group comprising a functional group that interacts with silica. In the modified conjugated diene polymer rubber, aromatic vinyl unit content is from 38% to 48% by weight, vinyl unit content is from 20% to 35%, weight-average molecular weight is from 600,000 to 1,000,000, and glass transition temperature is from −22 to −32° C. A glass transition temperature of the tackifying resin is from 50 to 110° C. higher than the glass transition temperature of the modified conjugated diene polymer rubber.
摘要翻译: 橡胶组合物包括二烯橡胶,其包含不小于30重量%的改性共轭二烯聚合物橡胶,每100重量份二烯橡胶,1至25重量份增粘树脂和25至 80重量份包含不少于50重量%二氧化硅的填料。 改性共轭二烯聚合物橡胶具有包含与二氧化硅相互作用的官能团的末端改性基团。 在改性共轭二烯聚合物橡胶中,芳香族乙烯基单元含量为38〜48重量%,乙烯基单元含量为20〜35重量%,重均分子量为60万〜100万,玻璃化转变温度为 -22至-32℃。增粘树脂的玻璃化转变温度比改性共轭二烯聚合物橡胶的玻璃化转变温度高50至110℃。
-
-
-
-
-