摘要:
A gas shielded arc-welding flux cored wire having a steel-made sheath filled with flux. The flux cored wire containing, by weight % based on the total weight of the wire, 1.0% or more Si--Mn ferroalloy powder having a grain size of 212 .mu.m or less; 2.0 to 7.0% TiO.sub.2 ; 0.2 to 1.5% SiO.sub.2 ; 0.1 to 1.2% ZrO.sub.2 ; and 0.01 to 0.3% fluoride (F-converted value). The powder comprises, by weight %, 0.40 to 1.20% C, 5 to 12% Si, 19 to 42% Mn, and the balance of Fe, with Si 2.gtoreq.11.89-2.92 C-0.077 Mn (Equation (1)) satisfied.
摘要:
Light which tries to enter a diffuser plate 3 at an angle which exceeds an angle at which a percentage of reflected light increases rapidly (that is, the incidence angle θ=70 degrees) is all reflected by a reflecting surface 21 and then enters the diffuser plate 3. Therefore, a pseudo light source is formed by light which was collected near a connection point between adjacent reflecting surfaces 21 out of the emitted light of the discharge lamps 1. So, the brightness between the adjacent discharge lamps 1 is increased, and it is possible to reduce unevenness in brightness. Furthermore, since the discharge lamp 1 is housed inside the reflecting surface 21 whose cross-sectional shape is a parabola, it is possible to reduce the distance between a reflecting plate 2 and the diffuser plate 3, as compared with the prior art, and to reduce the thickness dimension in the anteroposterior direction.
摘要:
A flux cored wire for gas shielded arc welding with a mixed gas comprising argon and carbon dioxide which comprises:a seam-welded steel sheath; and a core filled in the steel sheath and comprising, all in weight percent:a slag and arc stabilizer comprising 4.0 to 6.0% TiO.sub.2, 0.2 to 0.8% SiO.sub.2, 0.4 to 0.8% ZrO.sub.2, 0.2 to 0.8% Al.sub.2 O.sub.3, 0.06 to 0.25% Na.sub.2 O+K.sub.2 O, and 0.1 to 0.4% metal fluoride;an alloying agent and metal deoxidizer comprising 0.03 to 0.06% C, 0.20 to 0.80% Si, 1.50 to 2.20% Mn, and 0.30 to 0.60% Mg; andnot less than 2% Fe;in which the difference between the percentages of iron or a combination of Na and K segregated in any two quartered cross section of the wire that are defined by equations (1) and (2) in the specification are not more than 10% and not more than 0.15%, respectively.
摘要:
A method of manufacturing tubes filled with powdery and/or granular substances, such as flux-cored welding wires. A tube filled with a powdery and/or granular substance is continuously manufactured by forming a metal strip being fed in its longitudinal direction into an unwelded tube (1a) using forming rolls (2), feeding a powdery and/or granular substance (F) into the unwelded tube (1a) being formed through its opening, butt-welding together fringing edges of the opening, and reducing the diameter of the welded tube (1b). An allowable minimum heat input below which cold cracking occurs and a maximum allowable heat input above which spatters whose diameter is not smaller than 0.83 times the inside diameter of the finished tube are generated are determined in advance, and the butt welding is performed with a heat input larger than the allowable minimum heat input and smaller than the allowable maximum heat input. This eliminates the risk of breaking in reducing the diameter of the welded tube (1b) filled with the powdery and/or granular substance (F).
摘要:
An illumination light communication device includes a power supply unit controlling a load current in a light source unit to be maintained constant based on a dimming signal; an impedance unit series connected to the light source unit; a switch element parallel connected to the impedance unit to connect/disconnect the impedance unit with the light source unit; and a control unit controlling on/off of the switch element to modulate a light intensity of the light source unit such that a binary communication signal is superimposed on illumination light therefrom. The control unit controls the impedance of the impedance unit such that a difference between magnitudes of the load currents respectively when the pulse of the communication signal is superimposed and is not superimposed is maintained constant regardless of a dimming rate of the dimming signal in a range of a dimming rate equal to or greater than a predetermined level.
摘要:
An illumination light communication device includes a light source unit including light emitting elements; a power supply unit controlling a load current flowing through the light source unit to be maintained at a constant; a switch element connected in series to the light source unit; and a control unit configured to control on/off of the switch element to modulate a light intensity of illumination light from the light source unit such that a binary communication signal is superimposed on the illumination light. The control unit has a switching circuit to open/close a path between the light source unit and the power supply unit, controls on/off of the switching circuit based on a dimming signal to perform a dimming control on the light source unit by a PWM control, and allows the communication signal to be superimposed on the illumination light in synchronization with an ON time of the switching circuit.
摘要:
Light which tries to enter a diffuser plate 3 at an angle which exceeds an angle at which a percentage of reflected light increases rapidly (that is, the incidence angle θ=70 degrees) is all reflected by a reflecting surface 21 and then enters the diffuser plate 3. Therefore, a pseudo light source is formed by light which was collected near a connection point between adjacent reflecting surfaces 21 out of the emitted light of the discharge lamps 1. So, the brightness between the adjacent discharge lamps 1 is increased, and it is possible to reduce unevenness in brightness. Furthermore, since the discharge lamp 1 is housed inside the reflecting surface 21 whose cross-sectional shape is a parabola, it is possible to reduce the distance between a reflecting plate 2 and the diffuser plate 3, as compared with the prior art, and to reduce the thickness dimension in the anteroposterior direction.
摘要:
An object of the present invention is to provide an iron base Si--Mn alloy or an iron base Si--Mn--Ni alloy which can be easily crushed and can be manufactured in large quantity, and alloy powder thereof.An iron base Si--Mn--Ni alloy having good crushability and alloy powder thereof, comprising:C: 0.40 to 1.20% by weight,Si: 5.0 to 12.0% by weight,Mn: 19.0 to 42.0 % by weight, or Ni: not more than 30% by weight, and the balance being Fe, with the following equations satisfied: Si.gtoreq.11.89-2.92 C-0.077 Mn, Vickers hardness (Hv).gtoreq.550, and area ratio of dendrite structure .ltoreq.50%.An iron base Si--Mn--Ni alloy having good crushability and alloy powder thereof, comprising:C: 0.40 to 1.20% by weight,Si: 5.0 to 12.0% by weight,Mn: 19.0 to 42.0% by weight, or Ni: not more than 30% by weight, and the balance being Fe, with the following equations satisfied: Si.ltoreq.8.3 C+0.14 Mn, and relative permeability (.mu.).ltoreq.1.10.