Abstract:
The organic-inorganic composite of the present invention includes an organic compound having a carbonyl group, an inorganic compound containing a metal component, and a silver component. The ratio of the number of metal atoms in the inorganic compound to the number of carbon atoms in the organic compound is from 0.04 to 1.60, and the ratio of the number of silver atoms in the silver component to the number of carbon atoms in the organic compound is from 0.07 to 0.55. The organic-inorganic composite may include, for example, an inorganic compound having a metal matrix structure containing a metal M and oxygen, an organic compound having a carbonyl group, and silver ions. The carbonyl group is bonded to a side chain R1 of the organic compound and has an end group R2.
Abstract:
An AlN monocrystal plate disclosed herein may include: a first surface in a thickness direction; and a second surface opposing the first surface. A metal component containing region may be disposed substantially parallel to the first surface in an intermediate portion between the first surface and the second surface. In the metal component containing region, a plurality of metal components may be introduced and distributed. A type of the metal components may be Ga.
Abstract:
A structural body 10 includes a porous partition portion 14 forming a plurality of cells 12 each of which is used as a flow path of a mixed gas as a fluid; a function layer 16 provided on each inside surface 15 of the partition portion 14; a protective layer 18 provided on each inside surface end portion 15a of the inside surface 15; and a sealing portion 19 provided on each end surface 17 of the partition portion 14. The function layer 16 contains metal ions, and is transformed by light. The protective layer 18 is a length B (mm) from an end surface 11 of the structural body 10 and a maximum length A (mm) of an opening of the cell 12 satisfy the relationship of B/A≧0.4.
Abstract:
A composite substrate includes: a base substrate and an α-Ga2O3 crystal film that is provided on the base substrate, has a thickness of 10 μm or more, and has at least one alkali metal element content of 1.2×1015 atoms/cm3 or more and 1.0×1018 atoms/cm3 or less.
Abstract:
A gallium oxide single crystal particle according to the present invention is an α-Ga2O3 single crystal particle and has a diameter and a height that exceed 100 μm.
Abstract:
A transparent sealing member is provided with minute recesses at least in the surface of the member from which light from an optical element is emitted. The average width of the minute recesses is 0.1 μm to 2.0 μm, the average depth of the minute recesses is 5 nm to 50 nm, and the average frequency of occurrence of the minute recesses is 100000 to 3000000 recesses per 1 mm2.
Abstract:
A production method for zeolite powder includes disintegrating zeolite seed crystals in a silica unsaturated alkali solution containing an alkali source, preparing a silica saturated alkali solution by adding a silica source to the silica unsaturated alkali solution containing the zeolite seed crystals, and synthesizing zeolite powder by hermetically heating the silica saturated alkali solution.
Abstract:
A zeolite film structure comprising a support, a zeolite film and a protective film. The zeolite film is formed on a surface of the support. The protective film is formed on a surface of the zeolite film. The protective film is configured from organic-nonorganic hybrid silica or carbon. An average thickness of the protective film is less than or equal to 172 nanometers and greater than or equal to 44 nanometers.