Aluminum alloy clad sheet for heat exchangers
    1.
    发明授权
    Aluminum alloy clad sheet for heat exchangers 有权
    用于热交换器的铝合金包覆板

    公开(公告)号:US09012033B2

    公开(公告)日:2015-04-21

    申请号:US12798151

    申请日:2010-03-29

    摘要: An aluminum alloy clad sheet for heat exchangers includes a core material, a cladding material 1, and a cladding material 2, one side and the other side of the core material being respectively clad with the cladding material 1 and the cladding material 2, the core material containing 0.5 to 1.2% of Si, 0.2 to 1.0% of Cu, 1.0 to 1.8% of Mn, and 0.05 to 0.3% of Ti, with the balance being Al and unavoidable impurities, the cladding material 1 containing 3 to 6% of Si, 2 to 8% of Zn, and at least one of 0.3 to 1.8% of Mn and 0.05 to 0.3% of Ti, with the balance being Al and unavoidable impurities, and the cladding material 2 containing 6 to 13% of Si, with the balance being Al and unavoidable impurities, the cladding material 1 serving as the outer side of the aluminum alloy clad sheet during use.

    摘要翻译: 用于热交换器的铝合金包覆片包括芯材料,包层材料1和包覆材料2,芯材的一侧和另一侧分别包覆包层材料1和包层材料2,芯体 含有0.5〜1.2%的Si,0.2〜1.0%的Cu,1.0〜1.8%的Mn和0.05〜0.3%的Ti,余量为Al和不可避免的杂质,包层材料1含有3〜6%的 Si,2〜8%的Zn,0.3〜1.8%的Mn和0.05〜0.3%的Ti中的至少1种,余量为Al和不可避免的杂质,含有6〜13%的Si的包层材料2, 余量为Al和不可避免的杂质,包覆材料1在使用期间用作铝合金包覆板的外侧。

    Composition for forming intermediate layer containing sylylphenylene-based polymer and pattern-forming method
    3.
    发明申请
    Composition for forming intermediate layer containing sylylphenylene-based polymer and pattern-forming method 审中-公开
    用于形成含有亚苯基亚苯基聚合物的中间层的组合物和图案形成方法

    公开(公告)号:US20060263702A1

    公开(公告)日:2006-11-23

    申请号:US11432689

    申请日:2006-05-11

    IPC分类号: G03F1/00

    摘要: A composition for forming an intermediate layer is provided, having improved etching resistance, prevention of reflection of short-wavelength light (ability to absorb short-wavelength light), and low-hardening properties. The composition for forming an intermediate layer includes a silylphenylene-based polymer containing an aromatic ring (A), having a repetitive unit represented by the following general formula (1): wherein, at least one of R1 and R2 is a cross-linking group, m and n are each an integer from 0 to 20, and 1 is an integer representing the number of repetitive units; and a solvent (C).

    摘要翻译: 提供了一种用于形成中间层的组合物,具有改善的耐蚀刻性,防止短波长光的反射(吸收短波长光的能力)和低硬化性能。 用于形成中间层的组合物包括含有芳环(A)的甲硅烷基亚苯基聚合物,其具有由以下通式(1)表示的重复单元:其中R 1, 和R 2是交联基团,m和n各自为0至20的整数,1是表示重复单元数的整数; 和溶剂(C)。

    Aluminum heat exchanger excellent in corrosion resistance
    4.
    发明申请
    Aluminum heat exchanger excellent in corrosion resistance 有权
    铝合金热交换器耐腐蚀性优良

    公开(公告)号:US20050011636A1

    公开(公告)日:2005-01-20

    申请号:US10860560

    申请日:2004-06-03

    摘要: The present invention provides a heat exchanger which is assembled by brazing an aluminum fin material to the outer surface of an aluminum tube material formed by bending a sheet material, in particular, an aluminum heat exchanger which can be suitably used as an automotive heat exchanger such as a condenser or evaporator. The tube material is formed of a two-layer clad sheet which includes a core material and an Al—Zn alloy layer clad on the core material. The Al—Zn alloy layer is clad on the outer surface of the tube material and brazed to the aluminum fin material. The potential of the Al—Zn alloy layer in normal corrosive solution is 100 mV or more lower than the potential of the core material in the normal corrosive solution. The potential of the Al—Zn alloy layer in the normal corrosive solution is lower than the potential of the core material in high-concentration corrosive water. The normal corrosive solution refers to an aqueous solution containing 10 g/l of NaCl and 0.3 g/l of Na2SO4, and the high-concentration corrosive water refers to an aqueous solution in which the NaCl concentration is increased by 30 times by concentrating the above aqueous solution.

    摘要翻译: 本发明提供一种热交换器,其通过将铝翅片材料钎焊到通过弯曲板材形成的铝管材料的外表面而组装,特别是铝热交换器,铝热交换器可适合用作汽车热交换器 作为冷凝器或蒸发器。 管材由包含芯材和在芯材上包覆的Al-Zn合金层的双层包覆板形成。 Al-Zn合金层被覆在管材的外表面上并钎焊到铝翅片材料上。 正常腐蚀性溶液中的Al-Zn合金层的电位比正常腐蚀性溶液中的芯材的电位低100mV。 正常腐蚀性溶液中Al-Zn合金层的电位低于高浓度腐蚀性水中芯材的电位。 正常腐蚀性溶液是指含有10g / l NaCl和0.3g / l Na 2 SO 4的水溶液,高浓度腐蚀性水是指通过浓缩上述NaCl浓度将NaCl浓度提高30倍的水溶液 水溶液。

    Antireflection Film and Optical Device
    5.
    发明申请
    Antireflection Film and Optical Device 有权
    防反射膜和光学装置

    公开(公告)号:US20120251803A1

    公开(公告)日:2012-10-04

    申请号:US13434111

    申请日:2012-03-29

    IPC分类号: B32B3/26 B32B7/02

    CPC分类号: G02B1/11 Y10T428/24942

    摘要: An object of the present invention is to provide an antireflection film and an optical device having excellent antireflection characteristics against a light beam having a wide wavelength range at a wide range of an incident angle, and also having practically sufficient durability. To achieve the above object, the present invention adopts an antireflection film having an optical two-layer structure composed of an intermediate layer provided on a base material and a low refractive index layer provided on a surface of the intermediate layer, wherein the low refractive index layer is a layer obtained by binding hollow silica by a binder, a refractive index n(1) thereof is between 1.15 and 1.24 inclusive, and a refractive index n(2) of the intermediate layer satisfies a relation in the expression (1) below assuming a refractive index of the base material n(sub). n(1)×√{square root over (n(sub))}×0.930≦n(2)≦n(1)×√{square root over (n(sub))}×0.985  (1)

    摘要翻译: 本发明的目的是提供一种抗反射膜和对具有宽波长范围的光束在入射角宽的范围内具有优异的防反射特性的光学装置,并且还具有实际上足够的耐久性。 为了实现上述目的,本发明采用具有由设置在基材上的中间层和设置在中间层的表面上的低折射率层构成的光学二层结构的抗反射膜,其中低折射率 层是通过粘合剂结合中空二氧化硅而获得的层,其折射率n(1)在1.15和1.24之间,并且中间层的折射率n(2)满足以下表达式(1)中的关系 假设基材n(sub)的折射率。 n(1)×√{平方根(n(sub))}×0.930≦̸ n(2)≦̸ n(1)×√{平方根(n(sub))}×0.985(1)

    Motor having improved mounting structure
    8.
    发明授权
    Motor having improved mounting structure 失效
    电机具有改进的安装结构

    公开(公告)号:US07709985B2

    公开(公告)日:2010-05-04

    申请号:US12076494

    申请日:2008-03-19

    申请人: Naoki Yamashita

    发明人: Naoki Yamashita

    IPC分类号: H02K5/03

    摘要: A motor having an improved mounting structure is composed of a rotor including a rotor yoke; a stator including a bearing, a bearing holder and a base plate fixed to one end portion of the bearing holder; a shaft fixed to the rotor yoke and a damping member interposed between the bearing holder and the base plate. The bearing is fixed to the bearing holder. The rotor is supported through the shaft so as to be rotatable freely with respect to the stator. The bearing holder is fixed to the base plate with having a first area in which the bearing holder directly contacts with the base plate and a second area in which the damping member is interposed between the bearing holder and the base plate.

    摘要翻译: 具有改进的安装结构的电动机由包括转子轭的转子组成; 定子,其包括轴承,轴承保持器和固定到所述轴承保持器的一个端部的基板; 固定到转子轭的轴和插入在轴承座和基板之间的阻尼构件。 轴承固定在轴承架上。 转子通过轴被支撑成可相对于定子自由旋转。 轴承座固定在基板上,其具有第一区域,轴承保持架与基板直接接触,第二区域中阻尼构件插入在轴承座和基板之间。

    Aluminum heat exchanger excellent in corrosion resistance
    9.
    发明授权
    Aluminum heat exchanger excellent in corrosion resistance 有权
    铝合金热交换器耐腐蚀性优良

    公开(公告)号:US07250223B2

    公开(公告)日:2007-07-31

    申请号:US10860560

    申请日:2004-06-03

    摘要: The present invention provides a heat exchanger which is assembled by brazing an aluminum fin material to the outer surface of an aluminum tube material formed by bending a sheet material, in particular, an aluminum heat exchanger which can be suitably used as an automotive heat exchanger such as a condenser or evaporator. The tube material is formed of a two-layer clad sheet which includes a core material and an Al—Zn alloy layer clad on the core material. The Al—Zn alloy layer is clad on the outer surface of the tube material and brazed to the aluminum fin material. The potential of the Al—Zn alloy layer in a normal corrosive solution is at least 100 mV lower than the potential of the core material in the normal corrosive solution. The potential of the Al—Zn alloy layer in the normal corrosive solution is lower than the potential of the core material in high-concentration corrosive water. The normal corrosive solution refers to an aqueous solution containing 10 g/l of NaCl and 0.3 g/l of Na2SO4, and the high-concentration corrosive water refers to an aqueous solution in which the NaCl concentration is increased by 30 times by concentrating the above aqueous solution.

    摘要翻译: 本发明提供一种热交换器,其通过将铝翅片材料钎焊到通过弯曲板材形成的铝管材料的外表面而组装,特别是铝热交换器,铝热交换器可适合用作汽车热交换器 作为冷凝器或蒸发器。 管材由包含芯材和在芯材上包覆的Al-Zn合金层的双层包覆板形成。 Al-Zn合金层被覆在管材的外表面上并钎焊到铝翅片材料上。 正常腐蚀性溶液中Al-Zn合金层的电位比正常腐蚀性溶液中芯材的电位低至少100mV。 正常腐蚀性溶液中Al-Zn合金层的电位低于高浓度腐蚀性水中芯材的电位。 正常腐蚀性溶液是指含有10g / l NaCl和0.3g / l Na 2 SO 4·4的水溶液,高浓度腐蚀性水是指 通过浓缩上述水溶液使NaCl浓度增加30倍的水溶液。

    Coating solution for forming silica film
    10.
    发明授权
    Coating solution for forming silica film 有权
    用于形成二氧化硅膜的涂层溶液

    公开(公告)号:US07153355B2

    公开(公告)日:2006-12-26

    申请号:US10964276

    申请日:2004-10-13

    IPC分类号: C09D183/04 H01L21/473

    CPC分类号: C09D183/04

    摘要: To provide a silica film-forming material having a low dielectric constant and giving a film of less undergoing change in aging, a coating solution for forming a silica film includes a hydrolysis product of a mixture comprising: a tetraalkoxysilane; and at least one of a monoalkyltrialkoxysilane and a dialkyldialkoxysilane, and an ammonium salt represented by formula (I): wherein R1 represents an alkyl group having from 6 to 30 carbon atoms, R2 represents an alkyl group having from 1 to 5 carbon atoms, and X represents CH3COO, SO3H or OH.

    摘要翻译: 为了提供具有低介电常数的二氧化硅成膜材料,并且产生较小的老化变化的膜,用于形成二氧化硅膜的涂布溶液包括混合物的水解产物,其包含:四烷氧基硅烷; 和至少一种单烷基三烷氧基硅烷和二烷基二烷氧基硅烷,以及由式(I)表示的铵盐:其中R 1表示具有6至30个碳原子的烷基,R 2, / SUP>表示具有1至5个碳原子的烷基,X表示CH 3 COO,SO 3 H或OH。