摘要:
The invention relates to the use of phyllosilicates for improving the chemicals resistance, reducing the swelling, and improving the stress-cracking resistance of styrene copolymers, and to corresponding styrene copolymers, and to a process for their preparation.
摘要:
Thermoplastic molding compositions comprising (A) 5 to 98%-wt., based on components (A) through (E), of at least one elastomeric graft copolymer, (B) 1 to 90%-wt., based on components (A) through (E), of a further copolymer, (C) 1 to 70%-wt., based on components (A) though (D), of an elastomeric block copolymer composed of at least one block CA (hard phase) having copolymerized units of a vinylaromatic monomer, and at least one elastomeric block C(B/A) (soft phase) having copolymerized units of a vinylaromatic monomer, and of a diene, (D) 0 to 300%-wt., based on components (A) through (C), of a polycarbonate, and (E) 0 to 30%-wt., based on components (A) through (E), of conventional additives and processing aids, are useful for producing films, moldings or fibers.
摘要:
A thermoplastic molding composition having little intrinsic color is produced from a graft copolymer and a thermoplastic polymer. The graft copolymer is produced from a soft elastomeric particulate graft base obtained by polymerization of a conjugated diene alone or with a small amount of a monoethylenically unsaturated monomer, upon which is grafted a vinylaromatic monomer and acrylonitrile and optionally another monoethylenically unsaturated monomer. The thermoplastic polymer is a copolymer of a vinylaromatic monomer and acrylonitrile and optionally an additional monoethylenically unsaturated monomer. The thermoplastic molding composition has a low level of intrinsic color coupled with good mechanical properties and can be processed by, for example, extrusion, injection molding, calendaring, blow molding, compression molding, or sintering.
摘要:
The molding composition comprises components A to C and, if desired, D: a: as component A, from 20 to 94% by weight of a hard component made from one or more copolymers of styrene and/or &agr;-methylstyrene with acrylonitrile, where the proportion of acrylonitrile is from 10 to 50% by weight, b: from 5 to 70% by weight of at least one graft copolymer B, made from b1: as component B1, from 10 to 90% by weight of at least one elastomeric particulate graft base with a glass transition temperature below 0° C., and b2: as component B2, from 10 to 90% by weight of at least one graft made from a copolymer of styrene and/or &agr;-methylstyrene with acrylonitrile, where the proportion of acrylonitrile is from 10 to 50% by weight, c: as component C, from 0.1 to 10% by weight of at least one three-block copolymer of the formula X-Y-X with a central block Y made from propylene oxide units with an average molecular weight in the range from 2000 to 4000 and terminal blocks X made from ethylene oxide units whose average proportion in the three-block copolymer is from 2 to 35% by weight, where the total weight of components A to C is 100% by weight, and d: as component D, from 0 to 10% by weight, based on the total weight of components A to C, of other conventional auxiliaries and fillers.
摘要:
The invention relates to thermoplastic molding compositions, comprising A) from 35 to 95% by weight of at least one graft copolymer A), which is obtainable via reaction of A1) from 5 to 95% by weight of a polymer A1), which is obtained from at least one dicarboxylic anhydride a11) and from at least one vinylaromatic comonomer a12), and A2) from 5 to 95% by weight of a polyamide A2), B) from 5 to 40% by weight of at least one ungrafted or grafted, non-particulate rubber without core-shell structure B), which has functional groups which can react with the end groups of component A), C) from 0 to 50% by weight of at least one particulate or fibrous filler or particulate or fibrous reinforcing material C), D) from 0 to 60% by weight of at least one copolymer D) composed of vinyl aromatic monomers d1) and of comonomers d2), and E) from 0 to 40% by weight of at least one other additive E), where the entirety of components A) to E) gives 100% by weight, and also to processes for preparation of the thermoplastic molding compositions, to the use of the thermoplastic molding compositions for production of moldings, of foils, of fibers, or of foams, and finally to the moldings, foils, fibers, and foams obtainable from the thermoplastic molding compositions.
摘要:
The invention relates to thermoplastic molding compositions, comprising A) from 35 to 95% by weight of at least one graft copolymer A), which is obtainable via reaction of A1) from 5 to 95% by weight of a polymer A1), which is obtained from at least one dicarboxylic anhydride a11) and from at least one vinylaromatic comonomer a12), and A2) from 5 to 95% by weight of a polyamide A2), B) from 5 to 40% by weight of at least one ungrafted or grafted, non-particulate rubber without core-shell structure B), which has functional groups which can react with the end groups of component A), C) from 0 to 50% by weight of at least one particulate or fibrous filler or particulate or fibrous reinforcing material C), D) from 0 to 60% by weight of at least one copolymer D) composed of vinyl aromatic monomers d1) and of comonomers d2), and E) from 0 to 40% by weight of at least one other additive E), where the entirety of components A) to E) gives 100% by weight, and also to processes for preparation of the thermoplastic molding compositions, to the use of the thermoplastic molding compositions for production of moldings, of foils, of fibers, or of foams, and finally to the moldings, foils, fibers, and foams obtainable from the thermoplastic molding compositions.
摘要:
Thermoplastic molding materials containing the following ingredients with regard to components A-F: A) 5-70 wt. % of at least one graft copolymer A) consisting of a rubber elastic base with a glass transition temperature below 0° and a grafted overlay made of a styrene compound and acrylonitrile or methacrylonitrile or mixture thereof in addition to, optionally, other monoethylenically unsaturated monomers, B) 29-90 wt. % of a hard copolymer made of at least one styrene compound, acrylonitrile or methacrylonitrile or mixtures thereof and, optionally, other monoethylenically unsaturated monomers, C) 0-5 wt. % of at least one three-block copolymer X-Y-X with a middle block Y propylenoxide units and terminal block X made of ethyleneoxide units, D) 0.01-5 wt. % of at least one butylated reaction product of cresol with dicyclopentadiene, E) 0.01-5 wt. % of at least one thiocarboxylic acid ester, F) 0.01-5 wt. % of at least one alkaline metal salt or alkaline earth metal salt of a C6-C20carboxylic acid, G) 0-30 wt. % in relation to constituents A)-G), of other usual additives. The moulding materials exhibit a db* -value, after exposure to the atmosphere, of less than +5,0 after 100 hours of exposure to light and the atmosphere according to ISO 4892/2, method A, black temperature 65° C. colour measurement according to CIE-Lab in accordance with DIN 6174 and DIN 5033.
摘要:
Propylene copolymers grafted with .alpha.,.beta.-ethylenically unsaturated carboxylic acids or carboxylic acid derivatives and consisting ofa.sub.1) a random propylene copolymer (A.sub.1) containing from 0.1 to 15% by weight of polymerized C.sub.2 -C.sub.10 -alk-1-enes or ofa.sub.2) a propylene copolymer (A.sub.2) comprising a random propylene copolymer (I) containing from 0.1 to 15% by weight of polymerized C.sub.2 -C.sub.10 -alk-1-enes and a random propylene copolymer (II) containing from 15 to 80% by weight of polymerized C.sub.2 -C.sub.10 -alk-1-enes or ofa.sub.3) a propylene copolymer (A.sub.3) comprising a propylene homopolymer (III) and a random propylene copolymer (IV) containing from 15 to 80% by weight of polymerized C.sub.2 -C.sub.10 -alk-1-enes,are obtainable by reacting the monomer to be grafted with the propylene copolymer (A.sub.1), (A.sub.2) or (A.sub.3) at from 1 to 300 bar, from 0.01 to 1.0% by weight of the monomer to be grafted, where both stated concentrations are based on the propylene copolymer, being added to the molten propylene copolymer in the presence of from 0.005 to 0.5% by weight of a free radical initiator and the grafting reaction being carried out at from 200.degree. to 350.degree. C.
摘要:
The present invention relates to a process for preparation of copolymers A) comprising A1) one or more vinylaromatic monomers, A2) one or more vinyl cyanides, and A3) one or more dicarboxylic anhydrides via bulk polymerization or via solution polymerization,an important feature of the invention being that the polymerization is carried out in the presence of from 0.01 to 0.5% by weight of water, based on the total weight of the polymerization mixture.The present invention further relates to the copolymers A), to thermoplastic molding compositions comprising the copolymers A), to the use of the copolymers A) and of the thermoplastic molding compositions, and also to the moldings, foils, fibers, or foams obtainable from the copolymers A) or from the thermoplastic molding compositions.
摘要:
Semi-finished GMT sheet material of GMT recyclate in which more than 50% by weight of the glass fibers are more than 2 mm in length and which is produced by extruding GMT recyclate particles without significant comminution of the glass fibers.