Abstract:
The present invention provides aqueous compositions for treating fluff pulp comprising (i) one or more acrylic acid polymers containing phosphinate groups and having a weight average molecular weight of from 1,000 to 6,000 and (ii) from 5 to 50 wt. %, based on the total solids weight of the aqueous compositions, of one or more polyethylene glycols, having a formula weight of from 150 to 7,000, or, preferably, from 200 to 600. The present invention also provides individualized, intrafiber crosslinked cellulosic fibers comprising the cellulosic fiber and, in cured form, the aqueous compositions, as well as methods of making the individualized, intrafiber crosslinked cellulosic fibers.
Abstract:
The present invention provides telomeric copolymers of acrylic and methacrylic acid which further comprise an olefin polymerization residue and have one or more phosphorus acid groups wherein the phosphorus acid group comprises one or more phosphorus atom in the +1 oxidation state or in the +3 oxidation state, or both. In addition the present invention provides methods of making the telomeric copolymers comprising aqueous solution copolymerizing a monomer mixture comprising acrylic acid and methacrylic acid in the presence of a phosphorus acid group containing reactant having a phosphorus atom in the +1 oxidation state, and thermally treating the resulting telomeric copolymer at 175° C. or higher for a sufficient time to decarboxylate the copolymer.
Abstract:
The present invention provides aqueous compositions for treating fluff pulp comprising (i) one or more acrylic acid polymers containing phosphinate groups and having a weight average molecular weight of from 1,000 to 6,000 and (ii) from 5 to 50 wt. %, based on the total solids weight of the aqueous compositions, of one or more polyethylene glycols, having a formula weight of from 150 to 7,000, or, preferably, from 200 to 600. The present invention also provides individualized, intrafiber crosslinked cellulosic fibers comprising the cellulosic fiber and, in cured form, the aqueous compositions, as well as methods of making the individualized, intrafiber crosslinked cellulosic fibers.
Abstract:
The present invention provides thermosetting aqueous binder compositions comprising one or more reducing sugar, one or more diprimary diamine or poly(primary amine), and from 7 to 45 wt. %, based on total solids, of one or more polysaccharide having a dextrose equivalent (DE) value of from 5 to 30. The compositions provide treated articles, such as fiberglass mat. The binders provide articles having a dramatically reduced binder weight loss upon cure and a reduction in cure energy needed to achieve early dry strength.
Abstract:
The present disclosure provides for a coating formulation that includes a pigment, an organic aqueous emulsion and an organophosphonic acid of the formula: where R is a saturated or unsaturated alkyl having 2 to 10 carbon atoms or a substituted or unsubstituted aryl having 5 to 10 carbon atoms. The coating formulation can be used in forming a topcoat in an exterior insulation and finish system (EIFS). The present disclosure also provides for a method of forming a topcoat on a surface of the EIFS that helps to protect the underlayment of the EIFS against both weathering and moisture while helping to maintain color retention.
Abstract:
The present invention provides methacrylic acid polymer modified aqueous urea formaldehyde resin (UF resin) binder compositions useful in making a treated glass mat, e.g. for roofing shingles, wherein the methacrylic acid polymer comprises the reaction product of at least 50 wt. %, based on the total weight of monomers used to make the methacrylic acid polymer, of methacrylic acid or its salts, or mixtures thereof, a water-soluble phosphorous or sulfur containing compound and the remainder of a carboxylic acid group containing monomer, such as acrylic acid. The methacrylic acid polymers have at least one of a phosphite group, hypophosphite group, phosphinate group, diphosphinate group, and/or sulfonate group and enable modified UF resins to have early strength development even when the binder compositions comprise from 0.1 to less than 5 wt. % of the polymer modifier, based on total solids of the UF resin and the polymer modifier.
Abstract:
The present invention provides modified urea formaldehyde (UF) resin binder compositions and mineral fiber mats having an emulsion polymer modifier comprising, in copolymerized form, from 5 to 25 wt. % of co polymerized carboxylic acid functional monomers. The emulsion polymers have a measured glass transition temperature (DSC) ranging from −40° C. to 70° C. and a large average particle size. Further, the emulsion polymers comprise less than 30% of the copolymerized acid in neutralized form and do not excessively thicken aqueous compositions containing them. The modified UF resin binder compositions enable good dilution stability in use and high tensile strength in products containing them.
Abstract:
The present invention provides compositions comprising particles or agglomerates of one or more phosphorus oxide telomer or cotelomer ((co)telomer) of one or more unsaturated carboxylic acids or anhydrides having a mean average particle size of from 2 μm to 1 mm, preferably from 5 to 500 μm, preferably, comprising at least one carboxylic acid anhydride group. In addition, the present invention provides methods comprising aqueous solution addition polymerizing a monomer mixture of one or more unsaturated carboxylic acid in the presence of a phosphorus oxide acid or salt compound, drying the resulting copolymer at a temperature of from 120 to 230° C. and reducing its particle size to make a phosphorus oxide (co)telomer particle or agglomerate; the methods may further comprise reacting the (co)telomer particle or agglomerate with one or more polyether polyol, alkyl polyether polyol, polyether amine or alkyl polyether amine, with heating, to form a comb polymer useful, e.g. as a superplasticizer or dispersant.
Abstract:
The present invention provides hypophosphite (co)telomers of methacrylic anhydride having a weight average molecular weight of from 1,000 to 20,000, and having, on average, at least one phosphorus atom bound to two carbon atoms, and at least one carboxylic acid or salt group.
Abstract:
The present invention provides telomeric copolymers of acrylic and methacrylic acid which further comprise an olefin polymerization residue and have one or more phosphorus acid groups wherein the phosphorus acid group comprises one or more phosphorus atom in the +1 oxidation state or in the +3 oxidation state, or both. In addition the present invention provides methods of making the telomeric copolymers comprising aqueous solution copolymerizing a monomer mixture comprising acrylic acid and methacrylic acid in the presence of a phosphorus acid group containing reactant having a phosphorus atom in the +1 oxidation state, and thermally treating the resulting telomeric copolymer at 175° C. or higher for a sufficient time to decarboxylate the copolymer.