摘要:
A process is proposed for production of low-emission moldings for continuous operating temperatures >50° C. composed of a thermoplastic molding composition comprising A) from 10 to 99.9% by weight of polybutylene terephthalate or a mixture thereof with polyethylene terephthalate and/or polypropylene terephthalate, B) from 0.1 to 50% by weight of at least one terpolymer obtainable from b1) at least one vinylaromatic monomer, b2) at least one C1-C4-alkyl (meth)acrylate or (meth)acrylonitrile, and b3) from 0.1 to 10% by weight, based on the total weight of components b1) to b3), of at least one monomer which comprises an α,β-unsaturated anhydride, and C) from 0 to 60% by weight of other additives, where the total of the percentages by weight of the components (A) to (C) is 100%, via injection molding, which comprises carrying out the injection molding by means of a vented plastifying unit with a cylinder with inlet aperture for the thermoplastic molding composition, with a screw which conveys and plastifies the thermoplastic molding composition within a screw channel, and with one or more vents for discharge of volatile content from the plastified thermoplastic molding composition from the screw channel outward from the vented plastifying unit.
摘要:
Metalizable foils or sheets produced from a plastics mixture comprising, components A, B, C, and D, which gives a total of 100% by weight, a from 5 to 50% by weight of a thermoplastic polymer as component A, b from 50 to 95% by weight of a metal powder with an average particle diameter of from 0.01 to 100 μm where the normal electrode potential of the metal in acidic solution is more negative than that of silver, as component B, c from 0 to 10% by weight of a dispersing agent as component C, and d from 0 to 40% by weight of fibrous or particulate fillers or their mixtures as component D, wherein the tensile strain at break of component A is greater by a factor of from 11 to 100 than the tensile strain at break of the plastics mixture comprising components A, B, and, if present, C and D, and wherein the tensile strength of component A is greater by a factor of from 0.5 to 4 than the tensile strength of the plastics mixture comprising components A, B, and, if present, C and D.