摘要:
The present invention relates to sliding material provided by sintering a lead-free copper or copper alloy and contains at least one mineral selected from the group consisting of talc, mica, kaolinite mineral and montmorillonite mineral. Pb has conventionally been included in sliding materials for the purpose of obtaining conformability and seizure resistance. Despite the absence of Pb, the Pb-free copper-based sliding material and sliding parts according to the present invention have improved sliding properties.
摘要:
The present invention relates to sliding material provided by sintering a lead-free copper or copper alloy and contains at least one mineral selected from the group consisting of talc, mica, kaolinite mineral and montmorillonite mineral. Pb has conventionally been included in sliding materials for the purpose of obtaining conformability and seizure resistance. Despite the absence of Pb, the Pb-free copper-based sliding material and sliding parts according to the present invention have improved sliding properties.
摘要:
A method of producing a Pb-free copper-alloy sliding material containing 1.0 to 15.0% of Sn, 0.5 to 15.0% of Bi and 0.05 to 5.0% of Ag, and Ag and Bi from an Ag—Bi eutectic. If necessary, at least one of 0.1 to 5.0% of Ni, 0.02 to 0.2% P, 0.5 to 30.0% of Zn, and 1.0 to 10.0 mass % of at least one of a group consisting of Fe3P, Fe2P, FeB, NiB and AlN may be added.
摘要:
[Task] In the provided Cu-based sliding material, the properties equivalent to those of a Pb-containing material is attained even free of Pb, and material has stable friction coefficient.[Solution Means] A Pb-free copper-alloy sliding material contains 1.0 to 15.0% of Sn, 0.5 to 15.0% of Bi and 0.05 to 5.0% of Ag, and Ag and Bi from an Ag—Bi eutectic. If necessary, at least one of 0.1 to 5.0% of Ni, 0.02 to 0.2% P, and 0.5 to 30.0% of Zn is contained. Further, if necessary, 1.0 to 10.0 mass % of at least one of a group consisting of Fe3P, Fe2P, FeB, NiB and AlN, having an average particle diameter of 1.5 to 70 μm is contained.
摘要:
Sliding parts are made of Pb-free Cu—Bi based sintered material. The side in contact with a shaft is machined to a predetermined roughness. A number of Bi phases are present on the finished surface. Stable performance of Bi is to be exhibited. Machined sintered material covers a portion of the Bi phases. The ratio of the exposed surface area of the Bi phases is 0.5% or more relative to the area of the finished surface.
摘要:
Sliding parts are made of Pb-free Cu-Bi based sintered material. The side in contact with a shaft is machined to a predetermined roughness. A number of Bi phases are present on the finished surface. Stable performance of Bi is to be exhibited. Machined sintered material covers a portion of the Bi phases. The ratio of the exposed surface area of the Bi phases is 0.5% or more relative to the area of the finished surface.
摘要:
[Task] Seizure resistance of sliding material based on graphite-added resin is improved.[Means for Solution] A sliding material based on graphite-added resin has composition (1); graphite: average particle diameter of from 5 to 50 μm, a degree of graphitization of 0.6 or more, the number of graphite particles having a minimum diameter/maximum diameter ratio of 0.5 or more amounts to 50% or more of the total number of the graphite particles observed in a photograph of an optional cross section, content 5 to 60% by weight, as well as composition (2). balance of polyimide resin and/or polyamide-imide resin.
摘要:
A sliding material based on graphite-added resin containing 5 to 60% by weight of graphite particles having an average particle diameter of from 5 to 50 μm, and a degree of graphitization of 0.6 or more, with the balance being one or more of polyimide resin and polyamide-imide resin, and further, the number of the graphite particles having a minimum diameter/maximum diameter ratio (hereinafter referred to as “particle ratio”) of 0.5 or more amounts to 50% or more of the total number of the graphite particles observed in a photograph of an optional cross section of the sliding material based on graphite-added resin.
摘要:
Seizure resistance and wear resistance of Cu—Bi—In copper-alloy sliding material are enhanced by forming a soft phase of as pure as possible Bi. Mixed powder of Cu—In cuprous alloy powder and Cu—Bi containing Cu-based alloy powder is used. A sintering condition is set such that Bi moves outside particles of said Cu—Bi containing Cu-based powder and forms a Bi grain-boundary phase free of In, and In diffuses from said Cu—In containing Cu-based powder to said Cu—Bi containing Cu-based powder.
摘要:
When a Cu—Sn—Bi had-particle based sliding material is used for sliding, Cu of Cu matrix flows and covers up Bi phase. Seizure resistance lowers as time passes. A Pb-free sliding material preventing the reduction of seizure resistance is provided. (1) Composition: from 1 to 15% of Sn, from 1 to 15% of Bi, from 0.02 to 0.2% of P, and from 1 to 10% of hard particles having an average diameter of from 50 to 70 μm, with the balance being Cu and unavoidable impurities. (2) Structure: Bi phase and the hard particles are dispersed in the copper matrix, and all of said hard particles are bonded to the copper matrix.