摘要:
The present invention relates to sliding material provided by sintering a lead-free copper or copper alloy and contains at least one mineral selected from the group consisting of talc, mica, kaolinite mineral and montmorillonite mineral. Pb has conventionally been included in sliding materials for the purpose of obtaining conformability and seizure resistance. Despite the absence of Pb, the Pb-free copper-based sliding material and sliding parts according to the present invention have improved sliding properties.
摘要:
The present invention relates to sliding material provided by sintering a lead-free copper or copper alloy and contains at least one mineral selected from the group consisting of talc, mica, kaolinite mineral and montmorillonite mineral. Pb has conventionally been included in sliding materials for the purpose of obtaining conformability and seizure resistance. Despite the absence of Pb, the Pb-free copper-based sliding material and sliding parts according to the present invention have improved sliding properties.
摘要:
A method of producing a Pb-free copper-alloy sliding material containing 1.0 to 15.0% of Sn, 0.5 to 15.0% of Bi and 0.05 to 5.0% of Ag, and Ag and Bi from an Ag—Bi eutectic. If necessary, at least one of 0.1 to 5.0% of Ni, 0.02 to 0.2% P, 0.5 to 30.0% of Zn, and 1.0 to 10.0 mass % of at least one of a group consisting of Fe3P, Fe2P, FeB, NiB and AlN may be added.
摘要:
A method of producing a Pb-free copper-alloy sliding material containing 1.0 to 15.0% of Sn, 0.5 to 15.0% of Bi and 0.05 to 5.0% of Ag, and Ag and Bi from an Ag—Bi eutectic. If necessary, at least one of 0.1 to 5.0% of Ni, 0.02 to 0.2% P, 0.5 to 30.0% of Zn, and 1.0 to 10.0 mass % of at least one of a group consisting of Fe3P, Fe2P, FeB, NiB and AlN may be added.
摘要:
[Task] In the provided Cu-based sliding material, the properties equivalent to those of a Pb-containing material is attained even free of Pb, and material has stable friction coefficient.[Solution Means] A Pb-free copper-alloy sliding material contains 1.0 to 15.0% of Sn, 0.5 to 15.0% of Bi and 0.05 to 5.0% of Ag, and Ag and Bi from an Ag—Bi eutectic. If necessary, at least one of 0.1 to 5.0% of Ni, 0.02 to 0.2% P, and 0.5 to 30.0% of Zn is contained. Further, if necessary, 1.0 to 10.0 mass % of at least one of a group consisting of Fe3P, Fe2P, FeB, NiB and AlN, having an average particle diameter of 1.5 to 70 μm is contained.
摘要:
Sliding parts are made of Pb-free Cu—Bi based sintered material. The side in contact with a shaft is machined to a predetermined roughness. A number of Bi phases are present on the finished surface. Stable performance of Bi is to be exhibited. Machined sintered material covers a portion of the Bi phases. The ratio of the exposed surface area of the Bi phases is 0.5% or more relative to the area of the finished surface.
摘要:
Sliding parts are made of Pb-free Cu-Bi based sintered material. The side in contact with a shaft is machined to a predetermined roughness. A number of Bi phases are present on the finished surface. Stable performance of Bi is to be exhibited. Machined sintered material covers a portion of the Bi phases. The ratio of the exposed surface area of the Bi phases is 0.5% or more relative to the area of the finished surface.
摘要:
[Task] Seizure resistance of sliding material based on graphite-added resin is improved.[Means for Solution] A sliding material based on graphite-added resin has composition (1); graphite: average particle diameter of from 5 to 50 μm, a degree of graphitization of 0.6 or more, the number of graphite particles having a minimum diameter/maximum diameter ratio of 0.5 or more amounts to 50% or more of the total number of the graphite particles observed in a photograph of an optional cross section, content 5 to 60% by weight, as well as composition (2). balance of polyimide resin and/or polyamide-imide resin.
摘要:
A sliding material based on graphite-added resin containing 5 to 60% by weight of graphite particles having an average particle diameter of from 5 to 50 μm, and a degree of graphitization of 0.6 or more, with the balance being one or more of polyimide resin and polyamide-imide resin, and further, the number of the graphite particles having a minimum diameter/maximum diameter ratio (hereinafter referred to as “particle ratio”) of 0.5 or more amounts to 50% or more of the total number of the graphite particles observed in a photograph of an optional cross section of the sliding material based on graphite-added resin.
摘要:
This invention achieves high-quality separation of mixed signals in situations where the relationship between the number of signal sources N and the number of sensors M is such that N>M. First, the values of the observed signal observed by M sensors are transformed into frequency domain values, and these frequency domain values are used to calculate the relative values of the observed values between the sensors at each frequency. These relative values are clustered into N clusters, and the representative value of each cluster is calculated. Then, using these representative values, a mask is produced to extract the values of the signals emitted by V (1≦V≦M) signal sources from the frequency-domain signal values, and this mask is used to extract the signal values emitted by V signal sources from these frequency-domain signal values. After that, if V=1 then the limited signal is output directly as a separated signal, while if V≧2 then the separated values are obtained from this limited signal by subjecting it to separation techniques such as ICA.