摘要:
A rubber composition comprising the following component (A) 30-95 parts by weight, component (B) 5-70 parts by weight, component (C) 0.1-15 parts by weight and component (D) 0.01-15 parts by weight, and comprising no reinforcing filler (where the total of component (A) and component (B) is 100 parts by weight). (A) Ethylene-α-olefin-unconjugated diene copolymer rubber (B) Natural rubber (C) Organic peroxide (D) Aromatic amine
摘要:
A rubber composition containing no reinforcing agent, which comprises (A) 55 to 95 parts by weight of an ethylene-α-olefin-non-conjugated diene copolymer rubber, (B) 5 to 45 parts by weight of a natural rubber, and (C) 0.1 to 15 parts by weight of an organic peroxide, wherein the total amount of the components (A) and (B) is 100 parts by weight; a process for producing a rubber composition comprising the steps of (1) kneading at least said components (A) and (B), and (2) mixing at least the kneaded product with said component (C); a process for producing a molded article containing a vulcanized rubber composition, which comprises the above kneading step (1), the above mixing step (2), and the step (3) of molding the rubber composition at elevated temperature; and a vibration-proof material which comprises a molded article containing a vulcanized rubber composition produced according to the above-mentioned process.
摘要:
A resin composition for impact-resistant moldings with high low-temperature impact strength, and an air bag cover made of this resin composition are provided. The resin composition, or a thermoplastic elastomer composition for impact-resistant moldings, is produced by a process comprising subjecting 15 to 40% by weight of component (A), 15 to 40% by weight of component (B) and 20 to 70% by weight of component (C) (taking the total of the components (A), (B) and (C) as 100% by weigh) to a dynamic heat treatment in the presence of a crosslinking agent, said components being as specified below:(A): an ethylene-α-olefin-non-conjugated diene copolymer rubber having a density of 850 to 900 kg/m3, a Mooney viscosity (ML1+4(100° C.)) of 30 to 150, and an ethylene unit content of 30 to 90;(B): an ethylene-α-olefin-non-conjugated diene copolymer rubber having a density of 850 to 900 kg/m3 and a Mooney viscosity (ML1+4(100° C.)) of 30 to 150, and an ethylene unit content which is 0.50 to 0.95 time that of the component (A) or an iodine value which is 0.25 to 0.95 time that of the component (A);(C): a polypropylene resin.
摘要翻译:提供了具有高低温冲击强度的耐冲击成型品用树脂组合物和由该树脂组合物制成的气囊罩。 树脂组合物或耐冲击成型用热塑性弹性体组合物通过以下方法制造,该方法包括使组分(A)为15〜40重量%,(B)成分为15〜40重量%,成分(B)为20〜70重量% 的组分(C)(以组分(A),(B)和(C)的总计为100重量%)与交联剂存在下的动态热处理相比,所述组分如下所述 :(A):密度为850〜900kg / m 3的乙烯-α-烯烃 - 非共轭二烯共聚物橡胶,门尼粘度(ML< 1 + 4& (100℃))为30〜150,乙烯单元含量为30〜90; (B):密度为850〜900kg / m 3的乙烯-α-烯烃 - 非共轭二烯共聚物橡胶和门尼粘度(ML 1 + 4 SUB (100℃))为30〜150,乙烯单元含量为成分(A)的0.50〜0.95倍,碘值为成分(A)的碘值的0.25〜0.95倍。 (C):聚丙烯树脂。
摘要:
There is provided vulcanized solid rubber, which comprises a vulcanized product of an oil-extended copolymer comprising: (i) 100 parts by weight of an ethylene-&agr;-olefin-non-conjugated diene copolymer satisfying the following requirements (1) to (4), and (ii) 10 to 90 parts by weight of an extender oil: (1) a weight ratio of an ethylene unit to an &agr;-olefin unit in the ethylene-&agr;-olefin-non-conjugated diene copolymer is from 73/27 to 40/60, (2) an iodine value of the ethylene-&agr;-olefin-non-conjugated diene copolymer is from 20 to 36, (3) Mooney viscosity (ML1+4 (121° C.)) measured according to JIS-K-6300 of a blend containing 100 parts by weight of the ethylene-&agr;-olefin-non-conjugated diene copolymer and 20 parts by weight of an extender oil is from 100 to 180, and (4) a ratio of weight average molecular chain length/number average molecular chain length measured by gel permeation chromatography of the ethylene-&agr;-olefin-non-conjugated diene copolymer is from 3 to 5.
摘要:
The copolymer rubber composition comprises 60 to 75% by weight of a copolymer rubber (1) and 40 to 25% by weight of a copolymer rubber (2), and exhibits a difference in iodine value of 5 to 30 between the copolymer rubber (1) and the copolymer rubber (2). The copolymer rubber (1) is an ethylene-α-olefin-nonconjugated polyene copolymer rubber having an ethylene unit of 50 mol % to 70 mol %, an α-olefin unit of 50 mol % to 30 mol %, and an iodine value of 10 to 30, and the copolymer rubber (2) is an ethylene-α-olefinic copolymer rubber having an ethylene unit of more than 70 mol % and 95 mol % or less, an α-olefin unit of less than 30 mol % and 5 mol % or more, and an iodine value of 0 to 8.
摘要:
A rubber composition comprising: (A) at least one copolymer ingredient selected from the group consisting of ethylene/&agr;-olefin copolymer rubber and ethylene/&agr;-olefin/unconjugated diene copolymer rubber, (B) nickel diisobutyldithiocarbamate, and (C) carbon black, and not containing any compound having zinc; a vulcanized rubber composition obtained by vulcanizing the rubber composition; and a heat-resistant rubber product using the vulcanized rubber composition.
摘要:
The copolymer rubber composition comprises 60 to 75% by weight of a copolymer rubber (1) and 40 to 25% by weight of a copolymer rubber (2), and [iodine value of the copolymer rubber (1)−iodine value of the copolymer rubber (2)] is 5 to 30. The copolymer rubber (1) is an ethylene-α-olefin-nonconjugated polyene copolymer rubber having an ethylene unit of 50 mol % to 70 mol %, an α-olefin unit of 50 mol % to 30 mol %, and an iodine value of 15 to 45, and the copolymer rubber (2) is an ethylene-α-olefinic copolymer rubber having an ethylene unit of more than 70 mol % and 95 mol % or less, an α-olefin unit of less than 30 mol % and 5 mol % or more, and an iodine value of 10 to 30.
摘要:
There is provided a rubber composition containing the following components: (A): an ethylene-α-olefin-nonconjugated polyene copolymer rubber, (B): a natural rubber, (C): an organic peroxide, (D): an aromatic amine compound, and (E): silica.
摘要:
A rubber composition containing (A) an ethylene-&agr;-olefin based copolymer rubber having an intrinsic viscosity [&eegr;] of 2.0-10.0 as determined in xylene at 70° C., (B) a softening agent, and (C) a filler, which composition is superior in heat resistance and fatigue resistance, is obtained by a process including the steps of dividing component (A) into portions (A1) and (A2), dividing component (B) into portions (B1) and (B2), dividing component (C) into portions (C1) and (C2), kneading portions (A1), (B1) and (C1) together to obtain a first blend, adding portions (A2), (B2) and (C2) to the first blend to obtain a second blend and kneading the second blend to obtain the rubber composition.
摘要:
A rubber composition which contains the following components (A)-(D) and is free from any zinc-containing compounds that would cause trouble at the time of use of the final products: (A): an ethylene-&agr;-olefin copolymer rubber and/or ethylene-&agr;-olefin-non-conjugated diene copolymer rubber, (B): magnesium oxide, (C): carbon black, (D): at least one compound selected from the following compounds (D-1)-(D-3): (D-1): compounds containing a thio group and a carboxylic acid ester group in the molecule, (D-2): compounds containing a phenolic hydroxyl group in the molecule, (D-3): compounds containing an acyl group and an imino group in the molecule, provides vulcanized products including radiator hoses, heater hoses and radiator packings with improved age resistance.