1.
公开(公告)号:US12214571B2
公开(公告)日:2025-02-04
申请号:US18231487
申请日:2023-08-08
Applicant: SHOWA DENKO PACKAGING CO., LTD.
Inventor: Kenji Yoshino , Makoto Karatsu , Takashi Nagaoka
IPC: B32B15/00 , B32B7/12 , B32B15/085 , B32B27/18 , B32B37/12 , B32B38/00 , B65D65/40 , H01M10/0525 , H01M50/105 , H01M50/202 , H01M50/231
Abstract: A molding packaging material is capable of ensuring good slipperiness to secure good formability when molding the molding packaging material and is less likely to cause white powder on a surface of the packaging material. The molding packaging material includes a substrate layer as an outer layer, a heat fusible resin layer as an inner layer, and a metal foil layer arranged between the two layers. The heat fusible resin layer is composed of a single layer or a multi-layer. The innermost layer of the heat fusible resin layer is made of a resin composition containing a heat fusible resin, an anti-blocking agent, a slip agent, and a fluoropolymer-based lubricant.
-
公开(公告)号:US10290840B2
公开(公告)日:2019-05-14
申请号:US14289751
申请日:2014-05-29
Applicant: Showa Denko Packaging Co., Ltd.
Inventor: Kenji Yoshino
Abstract: A battery packaging material includes a stretched heat-resistant resin film layer as an outer layer which is laminated and integrated on one surface of an aluminum foil layer through a first adhesive layer; and a non-stretched thermoplastic resin film layer which is laminated and integrated as an inner layer on the other surface of the aluminum foil layer through a second adhesive layer, in which the second adhesive layer is an adhesive layer which is formed by a dry lamination method and whose melting point is 60° C. to 100° C., the adhesion strength of the inner layer and the aluminum foil layer is 3.0 N/15 mm width or more at 80° C., and the adhesion strength is 2.0 N/15 mm width or less at 120° C.
-
3.
公开(公告)号:US11766848B2
公开(公告)日:2023-09-26
申请号:US16644569
申请日:2018-08-17
Applicant: SHOWA DENKO PACKAGING CO., LTD.
Inventor: Kenji Yoshino , Makoto Karatsu , Takashi Nagaoka
IPC: B23B15/00 , B32B15/085 , H01M50/231 , H01M50/202 , B32B7/12 , B32B27/18 , B32B37/12 , B32B38/00 , B65D65/40 , H01M10/0525 , H01M50/105
CPC classification number: B32B15/085 , B32B7/12 , B32B27/18 , B32B37/12 , B32B38/0036 , B65D65/40 , H01M10/0525 , H01M50/105 , H01M50/202 , H01M50/231 , B32B2307/30 , B32B2457/10 , B32B2553/00
Abstract: Provided is a molding packaging material which is capable of ensuring good slipperiness to secure good formability when molding the molding packaging material and is less likely to cause white powder on a surface of the packaging material. The molding packaging material includes a substrate layer 2 as an outer layer, a heat fusible resin layer 3 as an inner layer, and a metal foil layer 4 arranged between the two layers. The heat fusible resin layer 3 is composed of a single layer or a multi-layer. The innermost layer of the heat fusible resin layer 3 is made of a resin composition containing a heat fusible resin, an anti-blocking agent, a slip agent, and a fluoropolymer-based lubricant.
-
公开(公告)号:US11446902B2
公开(公告)日:2022-09-20
申请号:US16647285
申请日:2018-06-28
Applicant: SHOWA DENKO PACKAGING CO., LTD.
Inventor: Kenji Yoshino , Yuji Minamibori , Katsumi Tanaka
IPC: B32B15/09 , B32B7/12 , B32B27/36 , C09J175/06 , H01M50/10 , B32B37/12 , B32B37/16 , B32B38/00 , H01M50/121 , H01G11/78 , H01M50/105 , H01M50/131 , C09J175/04 , H01M50/124 , B65D65/40 , H01M50/116 , H01M50/119 , H01M50/126 , H01M50/129 , B32B15/20
Abstract: Provided is a molding packaging material capable of sealing without causing sealing failure, significantly reducing cleaning frequency of a seal bar to improve productivity, and preventing occurrence of delamination. The molding packaging material includes a PBT terephthalate (PBT) layer 2, a heat fusible resin layer 3, and a metal foil layer 4 between the two layers. The PBT layer 2 and the metal foil layer 4 are bonded via an outer adhesive layer 5. The outer adhesive layer 5 is formed of a urethane adhesive cured film composed of a polyester polyol, a polyfunctional isocyanate compound, and polyhydric alcohol. The polyester polyol contains a dicarboxylic acid component, the dicarboxylic acid component includes an aromatic dicarboxylic acid. The dicarboxylic acid component contains an aromatic dicarboxylic acid. The content rate of the aromatic dicarboxylic acid in the dicarboxylic acid component is 40 mol % to 80 mol %. The Young's modulus of the cured film of the urethane adhesive is 70 MPa to 400 MPa. The PBT layer has tensile strength of 100 MPa to 300 MPa.
-
公开(公告)号:US09425449B2
公开(公告)日:2016-08-23
申请号:US14050504
申请日:2013-10-10
Applicant: Showa Denko Packaging Co., Ltd.
Inventor: Kenji Yoshino
CPC classification number: H01M2/1241 , H01M2/02 , H01M2/0217 , H01M2/026 , H01M2/0262 , H01M2/0267 , H01M2/0287
Abstract: An outer packaging material for a battery includes a heat resistant stretched resin film layer as an outer layer integrally laminated on one of surfaces of an aluminum foil layer via a first adhesive layer. A thermoplastic unstretched resin film layer as an inner layer is integrally laminated on the other surface of the aluminum foil layer via a second adhesive layer. An adhesive strength between the inner layer and the aluminum foil layer is 4N/15 mm-width to 30N/15 mm-width, and an adhesive strength between the outer layer and the aluminum foil layer is 2N/15 mm-width to 14N/15 mm-width. As a thermoplastic unstretched resin film constituting the inner layer, a thermoplastic unstretched resin film having a sealing strength of two sheets of the thermoplastic unstretched resin films arranged one on the other and heat sealed exceeding 30N/15 mm-width but not exceeding 110N/15 mm-width is used.
Abstract translation: 电池用外包装材料通过第一粘合剂层,在铝箔层的一个表面上整体地层压作为外层的耐热拉伸树脂膜层。 作为内层的热塑性未拉伸树脂膜层通过第二粘合层一体地层压在铝箔层的另一个表面上。 内层和铝箔层之间的粘合强度为4N / 15mm宽至30N / 15mm宽,外层和铝箔层之间的粘合强度为2N / 15mm宽至14N / 15毫米宽。 作为构成内层的热塑性未拉伸树脂薄膜,将热塑性未拉伸树脂薄膜的热塑性未拉伸树脂薄膜彼此排列并且热封超过30N / 15mm宽但不超过110N / 15的热塑性未拉伸树脂薄膜 使用mm宽度。
-
-
-
-