摘要:
An image division unit divides an original image. Each divided image is assigned an identifier, and additional information for generating an image corresponding to each divided image. An image distribution unit transmits the divided image and a reference drawing to a corresponding image generation terminal device. The image generation terminal device displays the reference drawing, generates an image corresponding to the received divided image, and transmit the generated image to an image distribution device. The image generation unit generates an entire image by integrating images received from a plurality of image generation terminal devices.
摘要:
There are provided a method for producing a magnesium alloy sheet having good press formability and a magnesium alloy coil stock obtained by coiling the magnesium alloy sheet. After a raw material sheet 1 composed of a magnesium alloy is preheated to 280° C. or less, the heated raw material sheet 1 is rolled with a reduction roll 3 and the obtained long rolled sheet is coiled. The surface temperature of the reduction roll 3 is set to be 230° C. or more and 290° C. or less. The preheating, rolling, and coiling are repeatedly performed in a continuous manner. By setting both the temperatures of the raw material sheet 1 and reduction roll 3 to be certain temperatures, the rolling property of the raw material sheet can be improved and the raw material sheet can be properly rolled in a continuous manner. In addition, a variation in temperature in the width direction of the reduction roll can be suppressed and uniform rolling can be performed, resulting in the production of a long magnesium alloy sheet. In this magnesium alloy sheet, working strain is sufficiently introduced by rolling and an increase in the size of crystal grains is suppressed. Thus, the magnesium alloy sheet has good press formability. Furthermore, a coil stock in which telescoping is not easily caused and that has good appearance is obtained.
摘要:
Provided are a rolled Mg alloy material which has a wide width and whose mechanical properties are uniform in a width direction, a Mg alloy structural member produced by plastically working the rolled Mg alloy material, and a method for producing the rolled Mg alloy material. The method for producing a rolled Mg alloy material includes rolling a Mg alloy material with a reduction roll. The Mg alloy material has a width of 1,000 mm or more, and the reduction roll has three or more regions in the width direction. The temperature is controlled in each of the regions so that a difference between a maximum temperature and a minimum temperature is 10° C. or less in the width direction of a surface of the reduction roll. The variation in the rolled state in the width direction can be reduced by reducing a difference in temperature over the width direction of the reduction roll. As a result, it is possible to produce a rolled Mg alloy material whose mechanical properties are substantially uniform in the width direction.
摘要:
A method of manufacturing a thermally-assisted magnetic recording head includes: providing a light source unit including a laser diode; providing a slider having a thermally-assisted magnetic recording head section thereon, the thermally-assisted magnetic recording head section including a magnetic pole, an optical waveguide, and a plasmon generator, the magnetic pole and the optical waveguide both extending toward an air bearing surface, the plasmon generator being located between the magnetic pole and the optical waveguide; driving the laser diode to allow a light beam to be emitted therefrom, the light beam including both a TE polarization component and a TM polarization component; performing an alignment between the light source unit and the thermally-assisted magnetic recording head section, based on a light intensity distribution of the TE polarization component in the light beam which has been emitted from the laser diode and then passed through the optical waveguide; and bonding the light source unit to the slider after the alignment is completed.
摘要:
An antenna includes: a dipole antenna; and a parasitic element arranged in parallel to the dipole antenna and having a linear structure and a meander structure, wherein a directivity and a return loss of the dipole antenna are controlled by setting a distance between the dipole antenna and the parasitic element and a shape and size of the meander structure.
摘要:
There are provided a method for producing a magnesium alloy sheet having good press formability and a magnesium alloy coil stock obtained by coiling the magnesium alloy sheet. After a raw material sheet 1 composed of a magnesium alloy is preheated to 280° C. or less, the heated raw material sheet 1 is rolled with a reduction roll 3 and the obtained long rolled sheet is coiled. The surface temperature of the reduction roll 3 is set to be 230° C. or more and 290° C. or less. The preheating, rolling, and coiling are repeatedly performed in a continuous manner. By setting both the temperatures of the raw material sheet 1 and reduction roll 3 to be certain temperatures, the rolling property of the raw material sheet can be improved and the raw material sheet can be properly rolled in a continuous manner. In addition, a variation in temperature in the width direction of the reduction roll can be suppressed and uniform rolling can be performed, resulting in the production of a long magnesium alloy sheet. In this magnesium alloy sheet, working strain is sufficiently introduced by rolling and an increase in the size of crystal grains is suppressed. Thus, the magnesium alloy sheet has good press formability. Furthermore, a coil stock in which telescoping is not easily caused and that has good appearance is obtained.
摘要:
Provided is a method for manufacturing a thermally-assisted magnetic recording head including a light source unit with a light source and a slider with an optical system. The method comprises steps of: adhering by suction the light source unit with a back holding jig; moving the back holding jig, then aligning a light-emission center of the light source with a light-receiving end surface of the optical system in directions within a slider back surface of the slider; bringing the light source unit into contact with the slider back surface, with a suction surface of the back holding jig tilted from the normal to the slider back surface; applying a load to a load application surface of the unit substrate by a loading means to bring a joining surface of the light source unit into conformity with the slider back surface; and bonding the light source unit and the slider. This method can improve the conformity, thereby achieving adequately strong junction and adequately high accuracy in position.
摘要:
A method for manufacturing a thermally-assisted magnetic recording head is provided, in which a light source unit including a light source and a slider including an optical system are bonded. A unit substrate is made of a material transmitting light having a predetermined wavelength, and an adhesion material layer is formed on the light source unit and/or the slider. The manufacturing method includes: aligning the light source unit and the slider in such a way that a light from the light source can enter the optical system and the adhesion material layer is sandwiched therebetween; irradiating the adhesion material layer with a light including the predetermined wavelength through the unit substrate; and bonding them. The adhesion material layer melted by the light including the predetermined wavelength and transmitted through the unit substrate can ensure high alignment accuracy as well as higher bonding strength and less change with time.
摘要:
An outer ring, an inner ring and a roller serving as a bearing component that adopts as a source material a steel ensuring a large fracture toughness value and also having an alloy element added thereto in a reduced amount and also provides sufficient wear resistance, are configured of a steel containing 0.15-0.3% by mass of carbon, 0.15-0.7% by mass of silicon, and 0.15-1.0% by mass of manganese, with a remainder of iron and an impurity, and have a raceway/rolling contact surface included in a region having a carbon enriched layer and a nitrogen enriched layer. In the nitrogen enriched layer the raceway/rolling contact surface has a nitrogen concentration equal to or larger than 0.3% by mass.
摘要:
A martensitic stainless steel pipe, which comprises specified quantities of C, Si, Mn, P, S, Cr, Ni, Al, N, Cu, Ti, V, Mo, Nb, B and Ca, and the balance being Fe and impurities, has satisfactory toughness at a high strength of 650 MPa or more by yield strength and also excellent hot workability. Therefore, it can be used as a high-strength martensitic stainless steel pipe for carbon dioxide gas corrosion resistant use, to be used in oil and/or gas well environments containing no hydrogen sulfide but carbon dioxide gas. This high-strength martensitic stainless steel pipe is an inexpensive martensitic stainless steel pipe, which does not require an addition of large quantities of expensive elements such as Ni and Mo, and moreover does not require the control of the content of P to a value less than 0.010% by mass.