Coating process
    2.
    发明授权
    Coating process 失效
    涂装工艺

    公开(公告)号:US5240744A

    公开(公告)日:1993-08-31

    申请号:US820585

    申请日:1992-01-21

    CPC分类号: C09D177/12 C09D179/02

    摘要: In the process described, cyclic polyimino ethers with .DELTA..sup.2 -oxazoline or .DELTA..sup.2 -5,6-dihydro-4H-1,3-oxazine structure are applied, alone or together with cyclic monoimino ethers of the same type, or with lactones, plus cationic polymerization catalysts, to solid surfaces and polymerized by heating. The process gives smooth, glossy coatings with high adhesive strength, hardness, and elasticity.

    摘要翻译: PCT No.PCT / EP90 / 01143 Sec。 371日期:1992年1月21日 102(e)日期1992年1月21日PCT提交1990年7月12日PCT公布。 公开号WO91 / 01354 1991年2月7日。在所述方法中,使用具有DELTA 2-恶唑啉或DELTA 2-5,6-二氢-4H-1,3-恶嗪结构的环状聚亚氨基醚单独或与 相同类型,或用内酯加上阳离子聚合催化剂,加入固体表面并通过加热进行聚合。 该工艺提供光滑,光泽的涂层,具有高粘合强度,硬度和弹性。

    Paint binders
    4.
    发明授权
    Paint binders 失效
    涂料粘合剂

    公开(公告)号:US5233020A

    公开(公告)日:1993-08-03

    申请号:US721514

    申请日:1991-07-12

    摘要: Poly-N-acylalkyleneimines corresponding to the following formula ##STR1## are used as an oxidatively crosslinking constituent in paints. In formula (I), R--CO represents the acyl radical of a mono- or polyunsaturated, aliphatic C.sub.16-22 carboxylic acid or a mixture of such radicals, R'--CO represents the acyl radical of a C.sub.1-22 carboxylic acid or a mixture of such radicals and x and y represent the percentages by weight of the particular polymer units, x assuming values of 20 to 100% and preferably 20 to 95% and y assuming values of 80 to 0% and preferably 80 to 5%. The indices m and n independently of one another may assume the value 2 or 3.

    摘要翻译: PCT No.PCT / EP90 / 00019 Sec。 371日期1991年7月12日 102(e)日期1991年7月12日PCT 1990年1月5日PCT PCT。 出版物WO90 / 08175 日期:1990年7月26日。对应于下式的聚N-酰基亚烷基亚胺(I)用作涂料中的氧化交联成分。 在式(I)中,R-CO表示单或多不饱和的脂族C 16-22羧酸或这些基团的混合物的酰基,R'-CO表示C1-22羧酸的酰基或 这些基团的混合物和x和y表示特定聚合物单元的重量百分比,假设值为20至100%,优选为20至95%,y为假定值为80至0%,优选为80至5%。 指数m和n彼此独立地可以取值2或3。

    Binder mixtures for stoving lacquers
    7.
    发明授权
    Binder mixtures for stoving lacquers 失效
    用于烤漆的粘合剂混合物

    公开(公告)号:US5512614A

    公开(公告)日:1996-04-30

    申请号:US381899

    申请日:1995-02-13

    CPC分类号: C08G73/0233 C09D167/08

    摘要: A binder mixture for stoving lacquers comprising A) at least one alkyd resin; and B) at least one poly-N-acyl alkyleneimine prepared by cationic polymerization of a monomer mixture ofa) from 10 to 90% by weight of at least one monomer corresponding to formula (I): ##STR1## in which Z is a direct bond or the group CR.sup.5 R.sup.6, R.sup.1 to R.sup.4 can be the same or different and represent H or a C.sub.1-8 alkyl group, R.sup.5 and R.sup.6 can be the same or different and represent H or a C.sub.1-2 alkyl group, R.sup.7 is a hydroxyl-containing alkyl or alkylene group of a hydroxycarboxylic acid containing 2 to 32 carbon atoms,b) from 90 to 10% by weight of at least one monomer corresponding to formula (II): ##STR2## in which Z and R.sup.1 to R.sup.6 are as defined above and R.sup.8 is the radical of an aromatic monocarboxylic acid, andc) from 0 to 80% by weight of at least one monomer corresponding formula (III): ##STR3## in which Z and R.sup.1 to R.sup.6 are as defined above, and R.sup.9 represents a non-hydroxy-substituted aliphatic radical of a carboxylic acid. The invention also relates to stoving lacquers containing the above binder mixture.

    摘要翻译: PCT No.PCT / EP93 / 02079 Sec。 371日期1995年2月13日 102(e)日期1995年2月13日PCT提交1993年8月5日PCT公布。 第WO94 / 04621号公报 日期:1994年3月3日。一种用于烘烤漆的粘合剂混合物,其包含A)至少一种醇酸树脂; 和B)通过阳离子聚合a)10至90重量%的至少一种对应于式(I)的单体:(I)的单体混合物制备的至少一种聚-N-酰基亚烷基亚胺,其中 Z是直接键或基团CR5R6,R1至R4可以相同或不同,表示H或C1-8烷基,R5和R6可以相同或不同,表示H或C1-2烷基, R7是含有2-32个碳原子的羟基羧酸的含羟基的烷基或亚烷基,b)90至10重量%的至少一种对应于式(II)的单体:其中其中 Z和R 1至R 6如上所定义,R 8是芳族单羧酸的基团,和c)0至80重量%的至少一种相应式(III)的单体:其中Z 并且R 1至R 6如上所定义,R 9表示羧酸的非羟基取代的脂肪族基团。 本发明还涉及含有上述粘合剂混合物的烘烤漆。

    Modified resins made from the reaction of epoxidized esters and resin
acids
    9.
    发明授权
    Modified resins made from the reaction of epoxidized esters and resin acids 失效
    由环氧化酯和树脂酸反应制成的改性树脂

    公开(公告)号:US5770662A

    公开(公告)日:1998-06-23

    申请号:US716144

    申请日:1996-09-18

    CPC分类号: C09J11/06 C09F1/04 C09J11/08

    摘要: A composition of matter comprising a resin obtained by a process comprising reacting at an elevated temperature an epoxidized ester of an unsaturated fatty acid with an aliphatic alcohol with a resin acid is provided. The equivalent ratio of epoxy groups of said epoxidized ester to carboxyl groups of said resin acid is in the range from 1.5:1 to 0.01:1. The resin is useful as a tackifier for adhesives and has a reduced tendency to crystallize.

    摘要翻译: PCT No.PCT / EP95 / 00862 Sec。 371日期1996年9月18日 102(e)1996年9月18日PCT 1995年3月9日PCT公布。 公开号WO95 / 25773 日期1995年9月28日提供了包含通过包括在高温下使不饱和脂肪酸的环氧化酯与脂肪醇与树脂酸反应的方法获得的树脂的组合物。 所述环氧化酯与所述树脂酸的羧基的环氧基的当量比在1.5:1至0.01:1的范围内。 该树脂可用作粘合剂的增粘剂并且具有降低的结晶倾向。