Piezoelectric sensor and method for making the same
    8.
    发明授权
    Piezoelectric sensor and method for making the same 有权
    压电传感器及其制作方法

    公开(公告)号:US08456067B2

    公开(公告)日:2013-06-04

    申请号:US12886751

    申请日:2010-09-21

    IPC分类号: H01L41/193

    摘要: The present disclosure relates to a piezoelectric sensor. The piezoelectric sensor includes a polymer layer, a first metal layer, and a second metal layer. The polymer layer includes pyrolytic polyacrylonitrile. The first metal layer is located on a surface of the polymer layer. The first metal layer includes a first work function. The second metal layer is located on another surface of the polymer layer and includes a second work function different from the first work function. The present disclosure also relates to a method for making the piezoelectric sensor.

    摘要翻译: 本发明涉及压电传感器。 压电传感器包括聚合物层,第一金属层和第二金属层。 聚合物层包括热解聚丙烯腈。 第一金属层位于聚合物层的表面上。 第一金属层包括第一功函数。 第二金属层位于聚合物层的另一表面上,并且包括与第一功函数不同的第二功函数。 本公开还涉及一种制造压电传感器的方法。

    Modifier of lithium ion battery
    9.
    发明授权
    Modifier of lithium ion battery 有权
    锂离子电池改性剂

    公开(公告)号:US08323836B2

    公开(公告)日:2012-12-04

    申请号:US13365503

    申请日:2012-02-03

    IPC分类号: H01M2/16

    摘要: A modifier of a lithium ion battery includes a clear solution fabricated from a phosphorous source having a phosphate radical, a trivalent aluminum source, and a metallic oxide provided in a liquid phase solvent. A molar ratio of the trivalent aluminum source, the metallic oxide, and the phosphorous source is set by (MolAl+MolMetal):Molp=about 1:2.5 to about 1:4. MolAl is the amount of substance of an aluminum element in the trivalent aluminum source, MolMetal is the amount of substance of a metallic element in the metallic oxide, and Molp is the amount of substance of a phosphorous element in the phosphorous source.

    摘要翻译: 锂离子电池的改性剂包括由具有磷酸根,三价铝源和在液相溶剂中提供的金属氧化物的磷源制成的透明溶液。 三价铝源,金属氧化物和磷源的摩尔比由(MolAl + MolMetal)设定:Molp =约1:2.5至约1:4。 MolAl是三价铝源中的铝元素的物质量,MolMetal是金属氧化物中金属元素的物质量,Molp是磷源中的磷元素的物质量。