Thick film getter paste compositions for use in moisture control
    1.
    发明授权
    Thick film getter paste compositions for use in moisture control 失效
    用于湿度控制的厚膜吸气剂糊组合物

    公开(公告)号:US07438829B2

    公开(公告)日:2008-10-21

    申请号:US10712670

    申请日:2003-11-13

    摘要: The invention is directed to a screen-printable getter composition comprising: (a) glass frit; dispersed in (b) organic medium. The invention is further directed to a screen-printable thick film getter composition comprising: (a) glass frit; and (b) desiccant material; dispersed in (c) organic medium.The present invention further relates to a getter composition utilizing low-softening temperature glasses comprising, based on weight %, 1-50% SiO2, 0-80% B2O3, 0-90% Bi2O3, 0-90% PbO, 0-90% P2O5, 0-60% Li2O, 0-30% Al2O3, 0-10% K2O, 0-10% Na2O, and 0-30% MO where M is selected from Ba, Sr, Ca, Zn, Cu, Mg and mixtures thereof. The glasses described herein may contain several other oxide constituents that can substitute glass network-forming elements or modify glass structure.

    摘要翻译: 本发明涉及一种可丝网印刷的吸气剂组合物,其包括:(a)玻璃料; 分散在(b)有机介质中。 本发明还涉及一种可丝网印刷的厚膜吸气剂组合物,其包含:(a)玻璃料; 和(b)干燥剂材料; 分散在(c)有机介质中。 本发明还涉及一种使用低软化温度玻璃的吸气剂组合物,其基于重量百分比为1-50%SiO 2,0-80%B 2 O 0〜90%的Bi 2 O 3,0〜90%的PbO,0〜90%的P 2

    Thick film getter paste compositions for use in moisture control
    2.
    发明授权
    Thick film getter paste compositions for use in moisture control 失效
    用于湿度控制的厚膜吸气剂糊组合物

    公开(公告)号:US07699999B2

    公开(公告)日:2010-04-20

    申请号:US12210300

    申请日:2008-09-15

    摘要: The invention is directed to a screen-printable getter composition comprising: (a) glass frit; dispersed in (b) organic medium. The invention is further directed to a screen-printable thick film getter composition comprising: (a) glass frit; and (b) desiccant material; dispersed in (c) organic medium.The present invention further relates to a getter composition utilizing low-softening temperature glasses comprising, based on weight %, 1-50% SiO2, 0-80% B2O3, 0-90% Bi2O3, 0-90% PbO, 0-90% P2O5, 0-60% Li2O, 0-30% Al2O3, 0-10% K2O, 0-10% Na2O, and 0-30% MO where M is selected from Ba, Sr, Ca, Zn, Cu, Mg and mixtures thereof. The glasses described herein may contain several other oxide constituents that can substitute glass network-forming elements or modify glass structure.

    摘要翻译: 本发明涉及一种可丝网印刷的吸气剂组合物,其包括:(a)玻璃料; 分散在(b)有机介质中。 本发明还涉及一种可丝网印刷的厚膜吸气剂组合物,其包含:(a)玻璃料; 和(b)干燥剂材料; 分散在(c)有机介质中。 本发明还涉及一种使用低软化温度的玻璃的吸气剂组合物,该组合物的重量百分数为1-50%SiO 2,0-80%B 2 O 3,0-90%Bi 2 O 3,0-90%PbO,0-90% P 2 O 5,0-60%Li 2 O,0-30%Al 2 O 3,0-10%K 2 O,0-10%Na 2 O和0-30%MO,其中M选自Ba,Sr,Ca,Zn,Cu,Mg和混合物 其中。 本文所述的玻璃可以包含可以代替玻璃网络形成元件或改变玻璃结构的几种其它氧化物成分。

    Thick Film Getter Paste Compositions for Use in Moisture Control
    3.
    发明申请
    Thick Film Getter Paste Compositions for Use in Moisture Control 有权
    用于水分控制的厚膜吸气剂糊组合物

    公开(公告)号:US20100102269A1

    公开(公告)日:2010-04-29

    申请号:US12649062

    申请日:2009-12-29

    IPC分类号: H01J7/18

    摘要: The invention is directed to a screen-printable getter composition comprising: (a) glass frit; dispersed in (b) organic medium. The invention is further directed to a screen-printable thick film getter composition comprising: (a) glass frit; and (b) desiccant material; dispersed in (c) organic medium.The present invention further relates to a getter composition utilizing low-softening temperature glasses comprising, based on weight %, 1-50% SiO2, 0-80% B2O3, 0-90% Bi2O3, 0-90% PbO, 0-90% P2O5, 0-60% Li2O, 0-30% Al2O3, 0-10% K2O, 0-10% Na2O, and 0-30% MO where M is selected from Ba, Sr, Ca, Zn, Cu, Mg and mixtures thereof. The glasses described herein may contain several other oxide constituents that can substitute glass network-forming elements or modify glass structure.

    摘要翻译: 本发明涉及一种可丝网印刷的吸气剂组合物,其包括:(a)玻璃料; 分散在(b)有机介质中。 本发明还涉及一种可丝网印刷的厚膜吸气剂组合物,其包含:(a)玻璃料; 和(b)干燥剂材料; 分散在(c)有机介质中。 本发明还涉及一种使用低软化温度的玻璃的吸气剂组合物,该组合物的重量百分数为1-50%SiO 2,0-80%B 2 O 3,0-90%Bi 2 O 3,0-90%PbO,0-90% P 2 O 5,0-60%Li 2 O,0-30%Al 2 O 3,0-10%K 2 O,0-10%Na 2 O和0-30%MO,其中M选自Ba,Sr,Ca,Zn,Cu,Mg和混合物 其中。 本文所述的玻璃可以包含可以代替玻璃网络形成元件或改变玻璃结构的几种其它氧化物成分。

    Thick film getter paste compositions for use in moisture control
    4.
    发明授权
    Thick film getter paste compositions for use in moisture control 有权
    用于湿度控制的厚膜吸气剂糊组合物

    公开(公告)号:US07943059B2

    公开(公告)日:2011-05-17

    申请号:US12649062

    申请日:2009-12-29

    摘要: The invention is directed to a screen-printable getter composition comprising: (a) glass frit; dispersed in (b) organic medium. The invention is further directed to a screen-printable thick film getter composition comprising: (a) glass frit; and (b) desiccant material; dispersed in (c) organic medium.The present invention further relates to a getter composition utilizing low-softening temperature glasses comprising, based on weight %, 1-50% SiO2, 0-80% B2O3, 0-90% Bi2O3, 0-90% PbO, 0-90% P2O5, 0-60% Li2O, 0-30% Al2O3, 0-10% K2O, 0-10% Na2O, and 0-30% MO where M is selected from Ba, Sr, Ca, Zn, Cu, Mg and mixtures thereof. The glasses described herein may contain several other oxide constituents that can substitute glass network-forming elements or modify glass structure.

    摘要翻译: 本发明涉及一种可丝网印刷的吸气剂组合物,其包括:(a)玻璃料; 分散在(b)有机介质中。 本发明还涉及一种可丝网印刷的厚膜吸气剂组合物,其包含:(a)玻璃料; 和(b)干燥剂材料; 分散在(c)有机介质中。 本发明还涉及一种使用低软化温度的玻璃的吸气剂组合物,该组合物的重量百分数为1-50%SiO 2,0-80%B 2 O 3,0-90%Bi 2 O 3,0-90%PbO,0-90% P 2 O 5,0-60%Li 2 O,0-30%Al 2 O 3,0-10%K 2 O,0-10%Na 2 O和0-30%MO,其中M选自Ba,Sr,Ca,Zn,Cu,Mg和混合物 其中。 本文所述的玻璃可以包含可以代替玻璃网络形成元件或改变玻璃结构的几种其它氧化物成分。

    Thick film getter paste compositions for use in moisture control
    6.
    发明申请
    Thick film getter paste compositions for use in moisture control 失效
    用于湿度控制的厚膜吸气剂糊组合物

    公开(公告)号:US20050104032A1

    公开(公告)日:2005-05-19

    申请号:US10712670

    申请日:2003-11-13

    摘要: The invention is directed to a screen-printable getter composition comprising: (a) glass frit; dispersed in (b) organic medium. The invention is further directed to a screen-printable thick film getter composition comprising: (a) glass frit; and (b) desiccant material; dispersed in (c) organic medium. The present invention further relates to a getter composition utilizing low-softening temperature glasses comprising, based on weight %, 1-50% SiO2, 0-80% B2O3, 0-90% Bi2O3, 0-90% PbO, 0-90% P2O5, 0-60% Li2O, 0-30% Al2O3, 0-10% K2O, 0-10% Na2O, and 0-30% MO where M is selected from Ba, Sr, Ca, Zn, Cu, Mg and mixtures thereof. The glasses described herein may contain several other oxide constituents that can substitute glass network-forming elements or modify glass structure.

    摘要翻译: 本发明涉及一种可丝网印刷的吸气剂组合物,其包括:(a)玻璃料; 分散在(b)有机介质中。 本发明还涉及一种可丝网印刷的厚膜吸气剂组合物,其包含:(a)玻璃料; 和(b)干燥剂材料; 分散在(c)有机介质中。 本发明还涉及一种使用低软化温度玻璃的吸气剂组合物,其基于重量百分比为1-50%SiO 2,0-80%B 2 O 0〜90%的Bi 2 O 3,0〜90%的PbO,0〜90%的P 2