White laminated polyester film for metallic plate lamination work
    2.
    发明授权
    White laminated polyester film for metallic plate lamination work 失效
    白色层压聚酯薄膜,用于金属板层压工作

    公开(公告)号:US06420010B1

    公开(公告)日:2002-07-16

    申请号:US09077837

    申请日:1998-06-04

    IPC分类号: B32B530

    摘要: The invented film comprises a layer A composed of a copolyester A, a layer B composed of a copolyester B, and a layer C composed of copolyester C. Layer A is laminated to one side of the layer B. Layer C is laminated to the other side of Layer B. Copolyester A contains 0-15 wt % of rutile titanium oxide (average particle diameter 0.1-0.5 &mgr;m). Copolyester B contains 10-50 wt % of the rutile titanium oxide. Copolyester C contains 0-15 wt % of the rutile titanium oxide. Each of Copolyester A, B, and C has a melting point of 210-245° C. The intrinsic viscosity (&eegr;A) of the polymer part of copolyester A, the intrinsic viscosity (&eegr;B) of the polymer part of copolyester B, and the intrinsic viscosity (&eegr;C) of the polymer part of copolyester C satisfy the following relationship. 0.46≦&eegr;B≦0.66, |&eegr;A-&eegr;B|

    摘要翻译: 本发明的薄膜包括由共聚酯A,由共聚聚酯B构成的层B和由共聚聚酯C组成的层C构成的层A.层A层叠在层B的一侧。层C层压到另一层 B层。共聚酯A含有0-15重量%的金红石型氧化钛(平均粒径0.1-0.5μm)。 共聚酯B含有10-50重量%的金红石氧化钛。 共聚酯C含有0-15重量%的金红石氧化钛。 共聚酯A,B和C的共聚物的熔点为210-245℃。共聚酯A的聚合物部分的特性粘度(ηaA),共聚酯B的聚合物部分的特性粘度(etaB) 共聚聚酯C的聚合物部分的特性粘度(η)满足以下关系。 0.46 <= etaB = 0.66,| etaA-etaB | <0.15,| etaC-etaB | <0.15和| etaA-etaC | <0.15。 整个层叠膜的表观密度(rho)与计算出的密度(rho0)的比例满足以下公式:0.75 <= rho / rho0 <= 1.00。 计算出的密度(rho0)由各共聚酯的聚合物部分的密度,金红石型氧化钛的密度,各层的厚度,各共聚酯中的金红石型氧化钛的浓度以及共聚酯层的数量来计算。