Abstract:
The present invention provides a method for producing a thermoplastic film which makes it possible to improve the optical properties of the thermoplastic film obtained by stretching and a thermoplastic film manufactured thereby. The transverse stretching section in which a cellulose acylate film is transversely stretched includes: a preheating zone, a transverse stretching zone, a cooling zone and a thermal relaxation zone, and the cellulose acylate film having been cooled in the cooling zone is immediately subjected to thermal relaxation treatment in the thermal relaxation zone.
Abstract:
The present invention provides a method for producing a cellulose acylate film which can prevent the generation of foreign matter problems and can produce a high-quality film. A cellulose acylate resin is molten in a twin-screw extruder and extruded from a die to form a cellulose acylate film. The average residence time of the resin in the extruder is set at 5 minutes or less.
Abstract:
According to the present invention, the adaptability to producing the cellulose acylate film and the surface properties of the cellulose acylate film produced by means of the melt film-forming method can be remarkably improved. Accordingly, there is also improved the surface properties of a stretched cellulose acylate film produced by stretching such an unstretched cellulose acylate film.
Abstract:
There is provided a method for producing a thermoplastic film that has a small distribution of retardation and excels in optical properties. In the method for producing a thermoplastic film by after extruding a molten resin from a die into a sheet, and cooling and solidifying the extruded sheet on a rotating cooling drum, peeling the cellulose acylate film off the cooling drum, and taking off the film with a take-off roller, the tension of the cellulose acylate film at the take-off roller is set to 0.02 kgf/mm 2 or lower.
Abstract translation:提供了具有较小的延迟分布和光学性能优异的热塑性薄膜的制造方法。 在通过将模具中的熔融树脂挤出成片材之后制造热塑性膜的方法,并将挤出的片材冷却并固化在旋转的冷却滚筒上,将纤维素酰化物膜从冷却滚筒上剥离,并且用 取出辊时,取出辊上的纤维素酰化物膜的张力设定为0.02kgf / mm 2以下。
Abstract:
According to the present invention, the film is cooled little by little by controlling the surface temperature of the cooling drums so that the surface temperature of the cooling drums downstream is lower than that of the cooling drums upstream, whereby it is prevented from slipping and shrinking on the surface of the cooling drums. Thus, defects can be prevented from occurring in the film, whereby a high-quality thermoplastic film for optical applications can be produced.
Abstract:
According to the present invention, a cellulose acylate film having high thickness precision and no streaks can be formed by producing a film with a cellulose acylate resin by means of the polishing roller method, and a high-performance optical film, which is free from the retardation distribution, can be produced by subsequently stretching the cellulose acylate film thus obtained within a magnification range from 1 or more and 2.5 or less.
Abstract:
There is provided a method for producing a thermoplastic film, which can suppress the occurrence of residual strain in the film caused by the polishing roller method to prevent the occurrence of stretch non-uniformity in stretching operation and provide a film that has excellent optical characteristics. The molten resin extruded from a die into a sheet is fed between a pair of polishing rollers and cooled while being held and pressed between them so that a cellulose acylate film is formed. The surface of the polishing roller is made up of a fluorine resin.
Abstract:
It is an object to provide a method of manufacturing a thermoplastic film capable of improving optical properties of the thermoplastic film obtained by drawing it and to provide the thermoplastic film. In a transverse drawing process part 30 for drawing a thermoplastic film 16 in a transverse direction is constituted by a preheating zone T1 and transverse drawing zones T2, T3 and cooling zones T4, T5, and the steps of the transverse drawing zone T3 and performed thereafter (cooling zone T4 and T5) are maintained at a glass transition temperature Tg or less. The temperature of the preheating zone T1 is set to be higher than that of the cooling zone T4 and falls within the range of -10 C to +30 C relative to those of the transverse drawing zones T2 and T3.
Abstract:
An unstretched cellulose acylate film hardly breakable upon stretching can be produced by melt film forming and as a result, a highly oriented stretched cellulose acylate film can be obtained. Using an extruder with a screw compression ratio of 2.5 to 4.5 and an L/D of 20 to 50, a cellulose acylate resin is extruded into a sheet at an extrusion temperature of 190 °C to 240 °C from a die to a cooling drum, and solidified by cooling to prepare an unstretched cellulose acylate film 16, which is then stretched to produce a stretched cellulose acylate film.
Abstract:
A method of producing a thermoplastic film, which can increase uniformity of Re and Rth of a thermoplastic film obtained by stretching, and which can provide a thermoplastic film having few display irregularities when the film is incorporated into a liquid crystal display device as a retardation film, and a thermoplastic film produced by the method are provided. In a tenter, both ends in the width direction of the film are held with clips and the film is simultaneously stretched in the traveling direction A and the width direction B. By this, a thermoplastic film in which the number of adhesion marks is 10 marks/m2 or less, the in-plane retardation Re is 0 nm to 500 nm and the retardation Rth in the thickness direction is 30 nm to 500 nm is produced.
Abstract translation:一种制造热塑性膜的方法,其可以提高通过拉伸获得的热塑性膜的Re和Rth的均匀性,并且当将膜结合到作为相位差膜的液晶显示装置中时,可以提供具有少量显示不规则性的热塑性膜 ,并且提供通过该方法制造的热塑性膜。 在拉幅机中,膜的宽度方向的两端用夹子保持,并且膜沿行进方向A和宽度方向B同时拉伸。由此,粘合标记数为10分的热塑性膜 / m 2以下时,面内相位差Re为0nm〜500nm,厚度方向的延迟Rth为30nm〜500nm。