Abstract:
The present invention relates to a process for the production of a zeolitic material having a BEA-type framework structure comprising YO2 and X2O3, wherein said process comprises the steps of (1) preparing a mixture comprising one or more sources for YO2 and one or more sources for X2O3; (2) crystallizing the mixture obtained in step (1); (3) subjecting the zeolitic material having a BEA-type framework structure obtained in step (2) to an ion-exchange procedure with Cu; and (4) subjecting the Cu ion-exchanged zeolitic material obtained in step (3) to an ion-exchange procedure with Fe; wherein Y is a tetravalent element, and X is a trivalent element, wherein the mixture provided in step (1) and crystallized in step (2) further comprises seed crystals comprising one or more zeolitic materials having a BEA-type framework structure, and wherein the mixture provided in step (1) and crystallized in step (2) does not contain an organotemplate as a structure-directing agent, as well as to the zeolitic material having a BEA frame work structure per se, and to its use, in particular in a method for the treatment of NOx by selective catalytic reduction (SCR).
Abstract:
A process for the oxidation of an organic carbonyl compound comprising reacting the compound, optionally in the presence of a solvent, with hydrogen peroxide in the presence of a catalyst comprising a tin-containing zeolitic material and at least one potassium salt.
Abstract:
The present invention relates to A process for the production of a molding, comprising (I) providing a zeolitic material; (II) mixing the zeolitic material provided in step (I) with one or more binders; (III) kneading of the mixture obtained in step (II); (IV) molding of the kneaded mixture obtained in step (III) to obtain one or more moldings; (V) drying of the one or more moldings obtained in step (IV); and (VI) calcining of the dried molding obtained in step (V); wherein the zeolitic material provided in step (I) displays a water adsorption ranging from 1 to 15 wt.-% when exposed to a relative humidity of 85%, as well as to a molding obtainable or obtained according to the inventive process in addition to a molding per se and to their respective use.
Abstract:
A process for preparing an aluminum-free boron containing zeolitic material comprising the framework structure MWW (BMWW), comprising (a) hydrothermally synthesizing the BMWW from a synthesis mixture containing water, a silicon source, a boron source, and an MWW template compound obtaining the BMWW in its mother liquor, the mother liquor having a pH above 9; (b) adjusting the pH of the mother liquor, obtained in (a) and containing the BMWW, to a value in the range of from 6 to 9; (c) separating the BMWW from the pH-adjusted mother liquor obtained in (b) by filtration in a filtration device.
Abstract:
The present invention relates to a process for the production of a zeolitic material having a framework structure comprising YO2, wherein said process comprises: (1) preparing a mixture comprising one or more tetravalent elements Y in elemental form, one or more organic hydroxide salts, and one or more protic solvents; (2) reacting the mixture obtained in step (1) for converting at least part of the one or more tetravalent elements Y into an oxidic form thereof containing one or more Y—O single bonds and/or one or more Y═O double bonds; and (3) crystallizing a zeolitic material from the mixture obtained in step (2).
Abstract:
The present invention relates to a process for the preparation of a zeolitic material comprising the steps of: (1) providing a mixture comprising one or more sources for YO 2 and one or more alkenyltrialkylammonium cation R 1 R 2 R 3 R 4 N + -containing compounds as structure directing agent; and (2) crystallizing the mixture obtained in step (1) to obtain a zeolitic material; wherein Y is a tetravalent element, and wherein R 1 , R 2 , and R 3 independently from one another stand for alkyl; and R 4 stands for alkenyl, as well as to zeolitic materials which may be obtained according to the inventive process and to their use.
Abstract:
The present invention relates to a micropowder, wherein the particles of the micropowder have a Dv10 value of at least 2 micrometer and the micropowder comprises mesopores which have an average pore diameter in the range of from 2 to 50 nm and comprise, based on the weight of the micropowder, at least 95 weight-% of a microporous aluminum-free zeolitic material of structure type MWW containing titanium and zinc.
Abstract:
The present invention relates to an organotemplate-free synthetic process for the production of a zeoiitic material having a CHA-type framework structure comprising YO2, X 2 O 3 , and optionally comprising Z 2 O 5 , wherein said process comprises the steps of: (1 ) providing a mixture comprising one or more sources for YO 2 , one or more sources for X 2 O 3 , and seed crystals having a CHA framework structure, wherein the CHA framework structure of the seed crystals comprises YO 2 , X 2 O 3 , and optionally comprises Z2O5; and (2) crystallizing the mixture obtained in step (1 ); wherein Y is a tetravaient element, X is a trivalent element, and Z is a pentavalent element, wherein optionally one or more sources for Z 2 O 5 are further provided in step (1 ), and wherein if the CHA framework of the seed crystals does not contain Z 2 O 5 , the seed crystals then have a Y0 2 : X 2 O 3 molar ratio of 5 or greater than 5.