摘要:
The present invention is a gas barrier laminate comprising a base and a gas barrier unit, the gas barrier unit comprising at least two inorganic layers, at least one of the at least two inorganic layers being a silicon oxynitride layer, the silicon oxynitride layer including a composition-gradient region that has a thickness of 25 nm or more, the composition-gradient region being a region in which a content ratio of oxygen decreases and a content ratio of nitrogen increases in a thickness direction toward the base, and a ratio of the thickness of the composition-gradient region to the thickness of the entire silicon oxynitride layer being 0.15 or more. The present invention also relates to: an electronic device member that includes the gas barrier laminate, and an electronic device that includes the electronic device member. The present invention provides: a gas barrier laminate that exhibits a very high gas barrier capability and very high bendability, an electronic device member that includes the gas barrier laminate, and an electronic device that includes the electronic device member.
摘要:
A backsheet or frontsheet having an outer layer with a melting temperature greater than or equal to 1 50°C includes at least one surface comprising a surface modification to improve adhesion between the backsheet or frontsheet and an encapsulant. The adhesion of the backsheet or frontsheet and encapsulant, after lamination, is at least 20 N/cm, preferably at least 40 N/cm or no adhesion failure. More preferably, the adhesion is at least 20 N/cm, even more preferably 40 N/cm or no adhesion failure, before and after 1,000 hours, preferably 2,000 hours, of damp heat aging at 85°C and 85% humidity.
摘要:
A film has a skin layer, a base layer, and an intermediate layer between the skin and base layers. The skin layer has styrenic block copolymer, the base layer has ethyiene/alpha-olefin copolymer, and the intermediate layer has from 12% to 50% styrene/ethylene-butadiene/styrene block copolymer. The film has a free shrink at 90°C of at least 65% and a density of at most 0.960 grams per cubic centimeter.
摘要:
A molded product and a unified molded product that are lightweight and also high in rigidity to meet the requirements from the market can be produced from a molded product comprising: a first member (I) containing a planar surface layer part and a protruding core part, and a second member (II) unified therewith, the first member (I) being of a fiber-reinforced resin (A) formed mainly of a reinforcing fiber (a1) and a matrix resin (a2), part of the threads of the reinforcing fiber (a1) extending penetratingly between the surface layer part and the core part, the part of the threads of the reinforcing fiber (a1) extending penetratingly at a rate of 400 threads/mm 2 or more through the boundary surface between the surface layer part and the core part, the reinforcing fiber (a1) having a number-average fiber length Ln of 1 mm or more, and the core part forming a hollow structure.
摘要:
A washable label may include a heat-shrinkable layer and a heat-activatable layer. The label may be attached to an item by a method including: heating a portion of the heat-activatable layer by intense visible or infrared light so as to transform the surface of the heat-activatable layer from a non-tacky state to a tacky state, and attaching the label to the item when the surface of the heat-activatable layer is in the tacky state, wherein the intensity of the light is selected such that spatially averaged temperature of the heat-shrinkable layer remains lower than the threshold shrinking temperature of the heat-shrinkable layer. The label may be easily separated from the item by heating the label such that shrinking of the heat-shrinkable layer peels at least a portion of the label away from the item.