Abstract:
The gas barrier laminate (100) of the present invention includes a base material layer (101), and a gas barrier polymer layer (103) having a thickness of from 0.01 µm to 0.45 µm provided over at least one surface of the base material layer (101) and formed by heating a mixture including a polycarboxylic acid and a polyamine compound.
Abstract:
An insulation assembly comprises an insulation pipe, an insulation umbrella group, and an insulation base. The insulation pipe has a first end and a second end opposite to the first end. The insulation umbrella group is formed on an outer wall of the insulation pipe. The insulation base is made of an insulating material and connected to the first end of the insulation pipe.
Abstract:
There is provided a composition for forming a hard coat layer which has high slippage and is excellent in water/oil repellency and also has antifouling properties such as fingerprint resistance and dirt wiping-off properties, and which is curable through ultraviolet irradiation in a nitrogen atmosphere or an air atmosphere that is generally used. A silicon-containing highly branched polymer obtained by polymerization of a monomer A having two or more radically polymerizable double bonds in a molecule and a monomer B having a polysiloxane chain and at least one radically polymerizable double bond in a molecule in the presence of a polymerization initiator D in an amount of 5 to 200% by mole relative to the number of moles of the monomer A; a curable composition comprising the highly branched polymer; a cured film obtained from the composition; and a hard coat film obtained by use of the composition.
Abstract:
An anti-fogging and anti-fouling laminate, including: a substrate; and an anti-fogging and anti-fouling layer on the substrate where a surface of the anti-fogging and anti-fouling layer is flat, wherein the anti-fogging and anti-fouling layer is a cured product obtained by curing an active energy ray curable resin composition through an active energy ray, wherein the active energy ray curable resin composition includes a hydrophilic monomer having a radically polymerizable unsaturated group and a photopolymerization initiator, wherein a content of the hydrophilic monomer having a radically polymerizable unsaturated group in the active energy ray curable resin composition is 60% by mass or more, and wherein a surface of the anti-fogging and anti-fouling layer has a pure water contact angle of 90° or more.
Abstract:
The present invention is related to PVC-free decorative surface coverings, in particular floor or wall coverings, comprising one or more polyolefin layer(s) and a cross-linked polyurethane top-layer comprising anionic or cationic salt groups. The invention is further related to a method for the production of said surface coverings.
Abstract:
A method for producing a multilayer film including a substrate and an optically anisotropic layer, the method comprising: a step of coating a surface of the substrate with a liquid crystal composition containing a polymerizable liquid crystal compound capable of expressing an inverse wavelength dispersion birefringence to form a layer of the liquid crystal composition; and a step of polymerizing the polymerizable liquid crystal compound contained in the layer of the liquid crystal composition to obtain an optically anisotropic layer, wherein the surface of the substrate has a surface free energy of 50 mN/m or less, and the liquid crystal composition has a surface tension of 26 mN/m or more.
Abstract:
A formed article comprising a gas barrier layer that is formed of a material including at least an oxygen atom, a carbon atom, and a silicon atom, the gas barrier layer including an area (A) where an oxygen atom content rate gradually decreases, and a carbon atom content rate gradually increases in a depth direction from a surface, the area (A) including a partial area (A1) and a partial area (A2), the (A1) having an oxygen atom content rate of 20 to 55%, a carbon atom content rate of 25 to 70%, and a silicon atom content rate of 5 to 20% based on the total content rate of oxygen atoms, carbon atoms, and silicon atoms, and the (A2) having an oxygen atom content rate of 1 to 15%, a carbon atom content rate of 72 to 87%, and a silicon atom content rate of 7 to 18% based on the total content rate of oxygen atoms, carbon atoms, and silicon atoms; a method of producing the same; an electronic device member; an electronic device. The formed article exhibits an excellent gas barrier capability, excellent bendability, excellent adhesion, and excellent surface flatness.
Abstract:
Provided are a transparent sheet for a solar cell, a transparent back sheet for a solar cell, and a solar cell module. This transparent sheet for a solar cell includes: a substrate film; and a first polymer layer that is disposed on one surface of the substrate film and includes a polymer A having an ultraviolet absorbing partial structure and a binder polymer B, in which the polymer A having an ultraviolet absorbing partial structure and the binder polymer B have the same kind of structural unit.
Abstract:
To provide polyimide films that contain polyimide good in solubility in solvent and excellent in workability and that are colorless, transparent and excellent in toughness, polyimide varnishes, and products and layered products using the polyimide film, the polyimide film is characterized by containing polyimide expressed by following general formula (1), and containing as A in the general formula (1), a structure expressed by following general formula (A-1), for example, structure expressed by following general formula (A-5).
Herein, in the general formula (1), A represents a bivalent organic group, B represents a tetravalent organic group, and n is 2 or more.
Abstract:
A coat layer and a substrate layer are combined to prepare a transparent laminate film; the coat layer has a surface with a maximum height of rolling circle waviness profile (W EM ) in accordance with JIS B0610 of 5 to 15 µm and an arithmetic average roughness (Ra) of not less than 0.5 µm. The transparent laminate film provides a comfortable writing experience and a reduced abrasion of a pen tip. The coat layer may have the surface with the arithmetic average roughness (Ra) of 0.5 to 5 µm. The coat layer may contain particles and a binder component. The binder component may comprise a polyfunctional (meth)acrylate, and a urethane (meth)acrylate and/or a thermoplastic elastomer. The transparent laminate film may have a total light transmittance of not less than 85%. The transparent laminate film may be disposed on a surface of a display of a pen-input device.