摘要:
Methods for cementing a subterranean well and maintaining zonal isolation involve preparing a cement slurry that contains water, an inorganic cement and an expanding agent. The slurry is placed in the annular region between casing and the formation or between two casing strings. After the cement sets, the expanding agent reacts and causes the set cement to be in a state of compression within the annular region. The casing dimensions may fluctuate in response to a temperature change, a pressure change, a mechanical disturbance resulting from a well intervention, or mud contamination or a combination thereof. The expanding agent may further react and maintain a state of compression within the annular region. The state of compression in the annular region may be monitored by acoustic impedance measurements.
摘要:
An about 5/8 inch to 3/4 inch thick low weight, low density gypsum panel with fire resistance capabilities sufficient to provide a Thermal Insulation Index of at least 17.0 minutes which when subjected to U419 test procedures will not fail for at least 30 minutes and, in selected embodiments, also has outstanding water resistance properties.
摘要:
The invention relates to a gypsum plaster-based material, in particular a gypsum plasterboard intended for the interior decoration of dwellings, containing a mixture of casein and activated carbon. The invention also relates to the use of said material in order to reduce the amount of volatile organic compounds in the atmosphere inside dwellings, offices or public buildings.
摘要:
A method of finishing an interior wall includes the steps of preparing a substrate of building panels comprising gypsum, cement or combinations thereof, said substrate having a surface, followed by applying a coating to the substrate, said coating comprising 1-30% by weight of a latex emulsion binder, 30-80% by weight calcium sulfate hemihydrate, up to about 8% by weight of a set inhibiting agent and 20-60% by weight water.
摘要:
The present invention is directed to ready to use (wet) and setting (dry) repair products with antistatic additives having reduced persistent airborne dust particulates upon sanding thereof. Such wet and dry repair products include, in part, an antistatic additive(s) that can reduce or eliminate the static charge that forms in dust particulates when dried repair products, such as spackling compounds, cementitious materials, and joint compounds, are sanded, for example. In turn, this can help reduce the quantity of airborne dust particulates, the time in which they are suspended, and the distance they travel in a given room or job site. In one example, a repair product for use as a dry repair compound can include an anti-static additive, which can include a cationic charge, and optionally a metal complex. In another example, the repair product further includes water to define a wet or ready to use repair product.