Abstract:
An insulating composition comprises: about 70-100 parts by volume of a polymeric material, about 5-30 parts by volume of a ceramic filler (2) which is surface-treated by a bifunctional coupling agent in an amount of about 0.1 wt % to about 4 wt % of the ceramic filler; about 0.1-5 parts by volume of a crosslinking agent; about 0-6 parts by volume of conductive powder (3); and about 0-6 parts by volume of ZnO whisker (4). A preparation method for making the insulating composition, an insulating article such as an electrical cable accessory, and a use thereof are provided.
Abstract:
Provided is a thermoplastic composite, a method for preparing a thermoplastic composite, and an injection-molded product. The thermoplastic composite comprises 35-75% by weight of a thermoplastic resin, 5-45% by weight of a non-cellulosic organic fiber, and 5-20%) by weight of hollow glass microspheres, based on 100% by weight of the total weight of the thermoplastic composite.
Abstract:
The present disclosure provides an elastomer composition, comprising, based on the total weight 100 wt. % of the elastomer composition: 1-50 wt. % of a modified ethylene propylene copolymer; 5-60 wt. % of a first silicone resin, the first silicone resin comprising at least one selected from the group consisting of the following: a hydroxyl-terminated silicone resin and an alkoxy-terminated silicone resin; 0.1-15 wt. % of a first crosslinking agent; 0.1-15 wt. % of a catalyst; and 10-85 wt. % of a filler. The elastomer composition provided by the present disclosure at least can be co-crosslinked in low temperature (approximately −20° C. to 60° C.) conditions. An elastomer prepared from the elastomer composition provided by the present disclosure has good mechanical properties and electrical insulation properties.
Abstract:
An insulating composition comprises: about 70-100 parts by volume of a polymeric material, about 5-30 parts by volume of a ceramic filler (2) which is surface-treated by a bifunctional coupling agent in an amount of about 0.1 wt % to about 4 wt % of the ceramic filler; about 0.1-5 parts by volume of a crosslinking agent; about 0-6 parts by volume of conductive powder (3); and about 0-6 parts by volume of ZnO whisker (4). A preparation method for making the insulating composition, an insulating article such as an electrical cable accessory, and a use thereof are provided.
Abstract:
Provided is a thermoplastic composite, a method for preparing a thermoplastic composite, and an injection-molded product. The thermoplastic composite comprises 35-75% by weight of a thermoplastic resin, 5-45% by weight of a non-cellulosic organic fiber, and 5-20%) by weight of hollow glass microspheres, based on 100% by weight of the total weight of the thermoplastic composite.