RESIN COMPOSITION AND DIELECTRIC LAYER AND CAPACITOR PRODUCED THEREFROM
    1.
    发明申请
    RESIN COMPOSITION AND DIELECTRIC LAYER AND CAPACITOR PRODUCED THEREFROM 审中-公开
    树脂组合物和电介质层和电容器

    公开(公告)号:US20160372269A1

    公开(公告)日:2016-12-22

    申请号:US15251214

    申请日:2016-08-30

    Abstract: The present invention provides a resin composition comprising: 1 to 20 parts by weight of a reinforcing fiber; 0.2 to 5 parts by weight of an anti-settling agent; 20 to 40 parts by weight of an epoxy resin; 0.1 to 3 parts by weight of a curing agent; and 50 to 75 parts by weight of a high dielectric constant filler. The present invention further provides a dielectric layer produced from the resin composition and a capacitor comprising the dielectric layer. In the dielectric layer made from the resin composition provided by the present invention, the fibers can be evenly dispersed and can enhance the mechanical strength of the resin composition, and cooperate with the epoxy resin to bring excellent toughness. Therefore, the mechanical strength of the produced dielectric layer can be remarkably improved, and its fragility can be effectively overcome when the dielectric layer is used in the PCB double-side etching process.

    Abstract translation: 本发明提供一种树脂组合物,其包含:1〜20重量份的增强纤维; 0.2〜5重量份的防沉降剂; 20〜40重量份的环氧树脂; 0.1〜3重量份的固化剂; 和50至75重量份的高介电常数填料。 本发明还提供由该树脂组合物制成的电介质层和包含电介质层的电容器。 在由本发明提供的树脂组合物制成的电介质层中,纤维可以均匀分散并且可以提高树脂组合物的机械强度,并与环氧树脂配合以提供优异的韧性。 因此,在PCB双面蚀刻工艺中使用电介质层时,可以显着提高所制造的电介质层的机械强度,并且可以有效克服其脆性。

    ELASTOMER COMPOSITION, ELASTOMER, METHOD FOR PREPARING ELASTOMER, AND ADHESIVE TAPE

    公开(公告)号:US20210102053A1

    公开(公告)日:2021-04-08

    申请号:US16605047

    申请日:2017-04-14

    Abstract: The present disclosure provides an elastomer composition, comprising, based on the total weight 100 wt. % of the elastomer composition: 1-50 wt. % of a modified ethylene propylene copolymer; 5-60 wt. % of a first silicone resin, the first silicone resin comprising at least one selected from the group consisting of the following: a hydroxyl-terminated silicone resin and an alkoxy-terminated silicone resin; 0.1-15 wt. % of a first crosslinking agent; 0.1-15 wt. % of a catalyst; and 10-85 wt. % of a filler. The elastomer composition provided by the present disclosure at least can be co-crosslinked in low temperature (approximately −20° C. to 60° C.) conditions. An elastomer prepared from the elastomer composition provided by the present disclosure has good mechanical properties and electrical insulation properties.

    COMPOSITE TEMPERATURE INDICATION ARTICLE AND PREPARATION METHOD AND USE THEREOF

    公开(公告)号:US20200348187A1

    公开(公告)日:2020-11-05

    申请号:US16760112

    申请日:2017-11-07

    Abstract: Disclosed is a temperature-indicating composite material product and a manufacturing method and application thereof, the temperature-indicating composite material product comprising: a porous film (1), opaque to at least a portion of visible light or opaque to at least a portion of visible light and at least a portion of ultraviolet light; and a colored composite material layer (2) located at the lower surface of the porous film (1), wherein the colored composite material layer (2) comprises a macro-molecular connecting material, a crystalline material and a colorant. Preferably, the macro-molecular connecting material is a crosslinked pressure-sensitive adhesive material, wherein the crystalline material and the colorant are dispersed in the macro-molecular connecting material, and the macro-molecular connecting material is an amorphous material or has a melting point higher than that of the crystalline material. When heated and melted, the crystalline material may migrate into the porous film (1) and fill pores therein, making the porous film (1) transparent to visible light.