Abstract:
Disclosed is a polyamide composition including 30% to 99.9% by weight of a polyamide mixture as component A). Component A) includes aliphatic polyamide A1) and aliphatic copolyamide or terpolyamide A2). The weight ratio of A1) to A2) is 55:45 to 95:5. The polyamide composition also includes 0% to 60% by weight of glass fibers as component B), 0% to 2% by weight of nigrosin as component C), 0.1% to 10% by weight of at least one polyhydric alcohol including more than two hydroxyl groups and a number-average molecular weight (Mn) of less than 2000 as component D), 0% to 20% by weight of further additives as component E). The reported amounts sum to 100% by weight based on the total composition.
Abstract:
1. The invention relates to the use of polyester molding compositions composed of A) from 20 to 97.9% by weight of a thermoplastic polyester B) from 0.1 to 10% by weight of an epoxidized natural oil or fatty acid ester, or mixture of these, where the epoxide equivalent weight of component B) in accordance with DIN EN ISO 3001 is from 100 to 400 g/eq C) from 1 to 20% by weight of a metal salt of a phosphinic acid D) from 1 to 20% by weight of a melamine compound E) from 0 to 60% by weight of other additional substances, where the total of the percentages by weight of components A) to E) is 100%, for the production of stress-cracking-resistant and halogen-free flame-retardant polyester molding compositions.
Abstract:
The present invention relates to specific deoxybenzoin containing flame retardant polyesters and flame retardant thermoplastic polymer molding compositions comprising deoxybenzoin containing flame retardant polyesters as well as their preparation and use for producing moldings, fibers or foils.
Abstract:
The present invention relates to the use of aromatic P-piperazine-compounds in flame retardant polymer compositions. These compositions are especially useful for the manufacture of flame retardant compositions based on thermoplastic polymers, especially polyolefin homo- and copolymers, polycondensates, such as polyamines or polyesters and duroplastic polymers, such as polyepoxides.
Abstract:
Disclosed is a polyamide composition including 30% to 99.9% by weight of a polyamide mixture as component A). Component A) includes aliphatic polyamide A1) and aliphatic copolyamide or terpolyamide A2). The weight ratio of A1) to A2) is 55:45 to 95:5. The polyamide composition also includes 0% to 60% by weight of glass fibers as component B), 0% to 2% by weight of nigrosin as component C), 0.1% to 10% by weight of at least one polyhydric alcohol including more than two hydroxyl groups and a number-average molecular weight (Mn) of less than 2000 as component D), 0% to 20% by weight of further additives as component E). The reported amounts sum to 100% by weight based on the total composition.
Abstract:
The invention relates to the use of mica coated with at least one metal oxide as flame retardant, and also thermoplastic molding compositions provided therewith.
Abstract:
The invention relates to the use of mica coated with at least one metal oxide as flame retardant, and also thermoplastic molding compositions provided therewith.
Abstract:
1. The invention relates to the use of polyester molding compositions composed of A) from 20 to 97.9% by weight of a thermoplastic polyester B) from 0.1 to 10% by weight of an epoxidized natural oil or fatty acid ester, or mixture of these, where the epoxide equivalent weight of component B) in accordance with DIN EN ISO 3001 is from 100 to 400 g/eq C) from 1 to 20% by weight of a metal salt of a phosphinic acid D) from 1 to 20% by weight of a melamine compound E) from 0 to 60% by weight of other additional substances, where the total of the percentages by weight of components A) to E) is 100%, for the production of stress-cracking-resistant and halogen-free flame-retardant polyester molding compositions.
Abstract translation:1.本发明涉及聚酯成型组合物的使用,该组合物由以重量计0.1至10%重量的环氧化天然油或脂肪酸酯或其混合物的A)20至97.9%重量的热塑性聚酯B) ,其中根据DIN EN ISO 3001的组分B)的环氧当量为100至400g /当量C)1至20重量%的次膦酸金属盐D)1至20重量% 三聚氰胺化合物E)的重量为0至60重量%的其它另外的物质,其中组分A)至E)的重量百分比的总和为100%,用于生产耐应力开裂和卤素 - 自由阻燃聚酯成型组合物。
Abstract:
Disclosed herein is a thermoplastic molding composition which includes A) from 10 to 99.9% by weight of a thermoplastic polyamide, B) from 0.1 to 20% by weight of at least one hyperbranched polyester having an acid number in the range of from 10 to 700 mg KOH/g and a hydroxyl number in the range of from 0 to 550 mg KOH/g, C) from 0 to 50% by weight of fibrous or particulate fillers, and D) from 0 to 45% by weight of further additives, where the total of the percentages by weight of components A) to D) is 100% by weight.
Abstract:
Described herein is a method of using glass fibers having a tensile strength according to DIN ISO 527-5 of 86.0 to 92.0 GPa, a tensile elastic modulus according to DIN ISO 527-5 of 2600 to 3200 MPa and a softening point according to DIN ISO 7884-1 of 900° C. to 950° C. the method including using the glass fibers to increase the weld seam strength of shaped articles made of molding materials including thermoplastic polyamides.