INSULATION LAYER FOR CABLES
    5.
    发明申请
    INSULATION LAYER FOR CABLES 审中-公开
    绝缘层电缆

    公开(公告)号:US20140349110A1

    公开(公告)日:2014-11-27

    申请号:US14362997

    申请日:2012-12-05

    Applicant: Borealis AG

    Abstract: The present invention is directed to a new cable having at least one insulation layer, to a process for producing such cable as well as to the use of a soluble a-nucleating agent (NA) for increasing the crystallization temperature of a polymer composition (PC) being part of an insulation layer of such a cable and the use of such a cable as communication cable and/or electrical cable.

    Abstract translation: 本发明涉及一种具有至少一个绝缘层的新电缆,制造这种电缆的方法以及使用可溶性α-成核剂(NA)来增加聚合物组合物(PC)的结晶温度 )是这种电缆的绝缘层的一部分,以及使用这种电缆作为通信电缆和/或电缆。

    Polypropylene composition suitable for primerless painting

    公开(公告)号:US10392492B2

    公开(公告)日:2019-08-27

    申请号:US15100176

    申请日:2014-12-01

    Applicant: Borealis AG

    Abstract: The present invention is directed to a polypropylene composition (C), an article comprising the polypropylene composition (C) and the use of the polypropylene composition (C) to reduce paintability failure of a molded article. The polypropylene composition (C) comprises (a) 40.0 to 80.0 wt. %, based on the total weight of the composition, of a propylene copolymer (R-PP) having: (a1) a comonomer content in the range of 1.5 to 8.0 wt. %, and (a2) a melt flow rate MFR2 (230 ° C.) measured according to ISO 1133 in the range of 5.0 to 100.0 g/10 min, and (b) 20.0 to 40.0 wt. %, based on the total weight of the composition, of a mineral filler (F) being selected from the group consisting of talcum, wollastonite, kaolin, and mica, wherein the polypropylene composition (C) has a melt flow rate MFR2 (230 ° C.) measured according to ISO 1133 in the range of 5.0 to 45.0 g/10 min.

    Process for the preparation of polypropylene with improved productivity
    8.
    发明授权
    Process for the preparation of polypropylene with improved productivity 有权
    生产率提高的聚丙烯制备方法

    公开(公告)号:US09512246B2

    公开(公告)日:2016-12-06

    申请号:US14418808

    申请日:2013-07-30

    Applicant: Borealis AG

    Abstract: A process for the preparation of a polypropylene in a sequential polymerization process including a pre-polymerization reactor and at least two polymerization reactors connected in series. The polymerization in the at least two polymerization reactors takes place in the presence of a Ziegler-Natta catalyst. The Ziegler-Natta catalyst includes (a) a pro-catalyst that has a compound of a transition metal, a compound of a metal which metal is selected from one of the groups 1 to 3 of the periodic table (IUPAC), and an internal electron donor, (b) a co-catalyst, and (c) an external donor. The Ziegler-Natta catalyst is present in the pre-polymerization reactor. Ethylene and propylene are fed to the pre-polymerization reactor in a feed rate ratio of 0.5 to 10.0 g/kg.

    Abstract translation: 一种在顺序聚合方法中制备聚丙烯的方法,包括预聚合反应器和至少两个串联的聚合反应器。 在至少两个聚合反应器中的聚合在齐格勒 - 纳塔催化剂存在下进行。 齐格勒 - 纳塔催化剂包括(a)具有过渡金属化合物的前催化剂,金属选自元素周期表第1至3族之一的金属化合物(IUPAC)和内部 电子给体,(b)助催化剂,和(c)外部供体。 齐格勒 - 纳塔催化剂存在于预聚合反应器中。 乙烯和丙烯以0.5至10.0g / kg的进料速率比进料到预聚合反应器中。