摘要:
Thermoplastic molding compositions based on thermoplastic polyesters (a.sub.1), graft polymers incorporating acrylate rubbers as grafting bases (a.sub.2), copolymers of aromatic vinyl monomers and acrylonitrile or methacrylonitrile (a.sub.3) which contain a polymeric component (B) having carboxyl, carboxyl derivative, hydroxyl or epoxy groups or, alternatively, where graft polymers (a.sub.2) or copolymers (a.sub.3) carry such groups have a balanced range of properties.
摘要:
Thermoplastic molding compositions based on thermoplastic polyesters (a.sub.1), graft polymers incorporating acrylate rubbers as grafting base (a.sub.2) and a two-shell graft sheath, copolymers of aromatic vinyl monomers and acrylonitrile or methacrylonitrile (a.sub.3) and glass fibers (B) have a balanced range of properties.
摘要:
Thermoplastic molding composition based on thermoplastic polyesters (a.sub.1), graft polymers incorporating acrylate rubbers as grafting base (a.sub.2), copolymers of aromatic vinyl monomers and acrylonitrile or methacrylonitrile (a.sub.3) and glass fibers (B) have particularly good mechanical properties if the (meth)acrylonitrile content in component (a.sub.3), based on the total weight of (a.sub.3), is less than the (meth)acrylonitrile content of component (a.sub.22).
摘要:
The flameproofing agent content of molding compositions containing polyesters (a.sub.1), acrylate graft polymers (a.sub.2), styrene/acrylonitrile copolymers (a.sub.3) and glass fibers can be reduced without affecting the flame resistance by adding finely divided PTFE.
摘要:
Thermoplastic molding materials contain, as essential components,(A) from 2 to 97.9% by weight of a nylon,(B) from 2 to 97.9% by weight of a polyaryl ether sulfone(C) from 0.1 to 30% by weight of a polymeric component having hydroxyl groupsand in addition(D) from 0 to 50% by weight of a rubber impact modifier and(E) from 0 to 60% by weight of reinforcing fillers.
摘要:
Polypropylene/polyamide molding compositions, suitable in particular for producing moldings, advantageously consist of, in each case based on 100 parts by weight of the molding composition,A) from 10 to 89.5 parts by weight of one or more polypropylene homopolymers and/or copolymers,B) from 10 to 89.5 parts by weight of one or more polyamides,C) from 0.5 to 30 parts by weight of an ethylene copolymer as adhesion promoter,D) from 0 to 30 parts by weight of an impact modifier andE) from 0 to 60 parts by weight of a reinforcing agent and/or additive,the ethylene copolymer (C) advantageously being polymerized from, in each case based on (C),a) from 50 to 98% by weight of ethylene,b) from 1 to 45% by weight of one or more alkyl (meth)acrylates having 1 to 8 carbon atoms in the alkyl, but not tert-butyl (meth)acrylate, andc) from 1 to 40% by weight of one or more further monomers containing in bonded form a group which is reactive toward the polyamide, for example a carboxyl, carboxylic anhydride, tert-butyl carboxylate, sulfo, sulfonyl, oxazolinyl or epoxide group,and are produced by melting together components (A) to (C) and any (D) and/or (E) at from 200.degree. to 300.degree. C.
摘要:
Novel polypropylene-polyamide molding compositions which comprise, based on 100 parts by weight of the molding compositions,A) 10 to 89.9 parts by weight of one or more polypropylene homopolymer and/or copolymer,B) 10 to 89.9 parts by weight of one or more polyamide,C) 0.1 to 5.0 parts by weight of one or more olefinically unsaturated carboxylic acid and/or one or more olefinically unsaturated carboxylic acid derivate,D) 0 to 3.0 parts by weight of an impact modifier, andE) 0 to 60.0 parts by weight of a reinforcing agent and/or additive,are prepared by melting together components (A), (C) and, if desired (D) at from 200.degree. to 300.degree. C. in a first reaction step and then, in a second reaction step, introducing component (B) and, if appropriate, components (D) and/or (E) into the modified melt obtained, and melting together the components.The molding compositions obtained are used for the production of moldings.
摘要:
Thermoplastic molding compositions contain as essential components(A) from 1 to 90% by weight of a polycarbonate,(B) from 1 to 90% by weight of a polyester,(C) from 1 to 90% by weight of a polyamide,(D) from 0.5 to 30% by weight of a polymeric component having hydroxyl groups and in addition(E) from 0 to 30% by weight of an impact-modifying rubber and(F) from 0 to 60% by weight of a fibrous or particulate filler.
摘要:
Thermoplastic molding materials containA) not less than 5% by weight of a polymer component consisting of from 50 to 100% by weight of polyphenylene ethers and from 0 to 50% by weight of a styrene polymer differing from component C),B) not less than 5% by weight of a polyester,C) not less than 0.1% by weight of a copolymer consisting ofC.sub.1) not less than 20% by weight of .alpha.-olefins of 2 to 8 carbon atoms, styrene or substituted styrenes of the general formula I ##STR1## where R and R.sup.1 is alkyl of 1 to 8 carbon atoms, hydrogen and/or halogen and n is 0, 1 or 2, or a mixture of these monomers,C.sub.2) not less than 0.5% by weight of a polymerizable monomer containing epoxide groups, and/orC.sub.3) not less than 0.05% by weight of a halobenzyl-containing polymerizable monomer having the structural unit (II) ##STR2## where X is halogen and R.sup.2 and R.sup.3 are each alkyl of 1 to 8 carbon atoms or hydrogen and n is 1, 2 or 3, and/orC.sub.4) not less than 0.05% by weight of a polymerizable monomer containing oxazoline groups, andC.sub.5) from 0 to 65% by weight of acrylonitrile, methacrylonitrile and further nonionic comonomers, andD) from 0 to 40% by weight of a rubber impact modifier.
摘要:
Thermoplastic molding materials contain, as essential components,(A) from 2 to 97.9% by weight of a nylon,(B) from 2 to 97.9% by weight of a polyaryl ether ketone and(C) from 0.1 to 30% by weight of a polymeric component containing hydroxyl groupsand in addition(D) from 0 to 50% by weight of an impact-modifying rubber and(E) from 0 to 60% by weight of fibrous and/or particulate fillers.