Abstract:
Provided is a polycarbonate resin composition containing 1-20 parts by weight of an amorphous thermoplastic resin having a glass transition temperature of not lower than 110° C., and 1-50 parts by weight of plate-shaped fillers having a number average major axis length of 0.5-45 μm, with respect to 100 parts by weight of a matrix resin component containing 35-95 wt % of a polycarbonate resin and 5-65 wt % of a thermoplastic polyester resin.
Abstract:
A molded body 1 includes a rib part 3 standing on a back surface 2b opposite to a design surface 2a of a main body 2 of the molded body 1. A reduced thickness part 4 is formed on the back surface 2b of the main body 2, the ratio D/T is 0.975 to 1.07 where D is the diameter of a circle that passes through base ends 3b of both side faces 3a of the rib part 3 and is in contact with the design surface 2a of the main body 2 positioned between the base ends 3b, and T is the thickness of the main body 2 at an outer side of the reduced thickness part 4, and t
Abstract:
A method of improving flowability of polycarbonate or polyarylate includes mixing the polycarbonate or the polyarylate with a flowability improver including a polyester. The polyester is a polycondensate of monomers including a bisphenol component (B) and a dicarboxylic acid component (C) at a molar ratio satisfying (B):(C)=45:55-55:45. The polyester includes a portion derived from the bisphenol component (B) and the dicarboxylic acid component (C) in an amount of 50 mol % or more.
Abstract:
A resin composition including 40 parts by weight or more and less than 95 parts by weight of a polycarbonate resin and 5 parts by weight or more and less than 60 parts by weight of a polyester-polyether copolymer as a base resin, wherein the polyester-polyether copolymer is a copolymer which is obtained by a polymerization using a germanium compound catalyst, includes aromatic polyester units and modified polyether units represented by the following general formula 1, and has an IV value within a range of 0.30 to 1.00 can be well-balanced in moldability, heat resistance, impact resistance, and low linear expansion property, without deteriorating a surface appearance of a molding obtained therefrom.
Abstract:
A moulded body 1 includes a rib part 3 standing on a back surface 2b opposite to a design surface 2a of a main body 2 of the moulded body 1. A reduced thickness part 4 is formed on the back surface 2b of the main body 2, the ratio D/T is 0.975 to 1.07 where D is the diameter of a circle that passes through base ends 3b of both side faces 3a of the rib part 3 and is in contact with the design surface 2a of the main body 2 positioned between the base ends 3b, and T is the thickness of the main body 2 at an outer side of the reduced thickness part 4, and t
Abstract:
A resin composition including 40 parts by weight or more and less than 95 parts by weight of a polycarbonate resin and 5 parts by weight or more and less than 60 parts by weight of a polyester-polyether copolymer as a base resin, wherein the polyester-polyether copolymer is a copolymer which is obtained by a polymerization using a germanium compound catalyst, includes aromatic polyester units and modified polyether units represented by the following general formula 1, and has an IV value within a range of 0.30 to 1.00 can be well-balanced in moldability, heat resistance, impact resistance, and low linear expansion property, without deteriorating a surface appearance of a molding obtained therefrom.