Soluble aniline conducting polymers
    3.
    发明授权
    Soluble aniline conducting polymers 失效
    可溶性苯胺导电聚合物

    公开(公告)号:US5932144A

    公开(公告)日:1999-08-03

    申请号:US916333

    申请日:1997-08-22

    IPC分类号: C08G73/02 H01B1/12 C08G65/38

    摘要: A soluble aniline conducting polymer characterized in that said conductive polymer comprises as a repeating unit an alkoxyl group-substituted aminobenzenesulfonic acid, its alkali metal salts, ammonium salts and/or substituted ammonium salts, and is a solid having a weight average molecular weight of about 1900 or more at room temperature, a conductive composition and electric conductor comprising the same, and a method for producing a soluble aniline conducting polymer having a weight average molecular weight of 10,000 t 3,240,000 characterized by polymerizing at least one compound (1) selected from the group consisting of an acidic group-substituted aniline, its alkali metal salts, ammonium salts and substituted ammonium salts in a solution containing a basic compound (2) using an oxidizing agent.

    摘要翻译: 一种可溶性苯胺导电聚合物,其特征在于所述导电聚合物包含烷氧基取代的氨基苯磺酸,其碱金属盐,铵盐和/或取代的铵盐作为重复单元,并且是重均分子量约为 1900以上,导电性组合物和含有该导电性组合物的电导体,以及制造重均分子量为10000t 3,240,000的可溶性苯胺导电聚合物的方法,其特征在于,聚合至少一种选自以下的化合物(1): 在使用氧化剂的碱性化合物(2)的溶液中由酸性基团取代的苯胺,其碱金属盐,铵盐和取代的铵盐组成的组。

    Soluble alkoxy-group substituted aminobenzenesulfonic acid aniline
conducting polymers
    4.
    发明授权
    Soluble alkoxy-group substituted aminobenzenesulfonic acid aniline conducting polymers 失效
    可溶性烷氧基取代氨基苯磺酸苯胺导电聚合物

    公开(公告)号:US5589108A

    公开(公告)日:1996-12-31

    申请号:US361577

    申请日:1994-12-22

    IPC分类号: C08G73/02 H01B1/12 H01B1/00

    摘要: A soluble aniline conducting polymer characterized in that said conductive polymer comprises as a repeating unit an alkoxyl group-substituted aminobenzenesulfonic acid, its alkali metal salts, ammonium salts and/or substituted ammonium salts, and is a solid having a weight average molecular weight of about 1900 or more at room temperature, a conductive composition and electric conductor comprising the same, and a method for producing a soluble aniline conducting polymer having a weight average molecular weight of 10,000 t 3,240,000 characterized by polymerizing at least one compound (1) selected from the group consisting of an acidic group-substituted aniline, its alkali metal salts, ammonium salts and substituted ammonium salts in a solution containing a basic compound (2) using an oxidizing agent.

    摘要翻译: 一种可溶性苯胺导电聚合物,其特征在于所述导电聚合物包含烷氧基取代的氨基苯磺酸,其碱金属盐,铵盐和/或取代的铵盐作为重复单元,并且是重均分子量约为 1900以上,导电性组合物和含有该导电性组合物的电导体,以及制造重均分子量为10000t 3,240,000的可溶性苯胺导电聚合物的方法,其特征在于,聚合至少一种选自以下的化合物(1): 在使用氧化剂的碱性化合物(2)的溶液中由酸性基团取代的苯胺,其碱金属盐,铵盐和取代的铵盐组成的组。

    METHOD FOR GIVING ELECTRIC CONDUCTIVITY TO MATERIAL, METHOD FOR PRODUCING CONDUCTIVE MATERIAL, AND CONDUCTIVE MATERIAL
    5.
    发明申请
    METHOD FOR GIVING ELECTRIC CONDUCTIVITY TO MATERIAL, METHOD FOR PRODUCING CONDUCTIVE MATERIAL, AND CONDUCTIVE MATERIAL 审中-公开
    生产电导率材料的方法,制造导电材料的方法和导电材料

    公开(公告)号:US20100090170A1

    公开(公告)日:2010-04-15

    申请号:US12446643

    申请日:2007-10-24

    申请人: Masashi Uzawa

    发明人: Masashi Uzawa

    IPC分类号: H01B1/12

    摘要: Disclosed is a method for giving electric conductivity to a material, by which a conductive material having excellent water resistance and sufficient antistatic properties even at a low temperature and a low humidity can be easily obtained at low cost. In the method, electric conductivity is given to a base material (A) having a nitrogen-containing functional group by soaking the base material (A) in a liquid containing a conductive polymer (B) having at least one kind of sulfonic group and carboxyl group while holding the liquid at a temperature in the range of from 30 to 130° C. A conductive material to be obtained by such a method is also disclosed.

    摘要翻译: 公开了一种赋予材料导电性的方法,即使在低温和低湿度下也能够容易地获得具有优异的耐水性和足够的抗静电性能的导电材料。 在该方法中,通过将基材(A)浸渍在含有具有至少一种磺酸基和羧基的导电性聚合物(B)的液体中,赋予具有含氮官能团的基材(A)的导电性 同时将液体保持在30至130℃的温度范围内。还公开了通过这种方法获得的导电材料。

    SOLID ELECTROLYTIC CAPACITOR AND METHOD FOR MANUFACTURING SAME
    8.
    发明申请
    SOLID ELECTROLYTIC CAPACITOR AND METHOD FOR MANUFACTURING SAME 有权
    固体电解电容器及其制造方法

    公开(公告)号:US20140198428A1

    公开(公告)日:2014-07-17

    申请号:US14238703

    申请日:2011-08-17

    IPC分类号: H01G9/028 H01G9/00

    CPC分类号: H01G9/028 H01G9/0036 H01G9/15

    摘要: A solid electrolytic capacitor in which a solid electrolytic layer is formed by applying and drying a conductive-polymer solution which contains a conductive polymer that satisfies following condition (A) and which meets following condition (B) to a dielectric layer formed by oxidizing the surface of an anode metal.Condition (A): Out of one or more peaks that appear when particle size distributions are measured by a dynamic light-scattering method using a conductive-polymer solution containing 1 mass % conductive polymer, the volume average particle size in the distribution that includes the peak of the smallest particle size is smaller than 26 nm.Condition (B): A conductive-polymer solution containing the conductive polymer is applied and dried to provide a solid electrolytic layer on the dielectric layer formed by oxidizing a surface of aluminum with an electrical capacitance of 95 μF/cm2, and when a stacked aluminum electrolytic capacitor is formed using the solid electrolytic layer, the rate of exhibited capacitance of the stacked aluminum electrolytic capacitor is no less than 70%.

    摘要翻译: 一种固体电解质电容器,其中通过将包含满足以下条件(A)并满足以下条件(B)的导电聚合物的导电聚合物溶液施加并干燥以形成氧化表面形成的电介质层,形成固体电解质层 的阳极金属。 条件(A):当使用含有1质量%导电聚合物的导电聚合物溶液的动态光散射法测量粒度分布时出现的一个或多个峰中,分布中的体积平均粒径包括 最小粒径的峰值小于26nm。 条件(B):涂布含有导电性高分子的导电性高分子溶液,使其干燥,在电介质层上形成固体电解质层,该电介质层通过以95μF/ cm 2的电容氧化铝的表面而形成, 使用固体电解质层形成电解电容器,叠层铝电解电容器的电容率不小于70%。

    Method for producing soluble conductive polymer having acidic group
    9.
    发明授权
    Method for producing soluble conductive polymer having acidic group 失效
    制备具有酸性基团的可溶性导电聚合物的方法

    公开(公告)号:US5980784A

    公开(公告)日:1999-11-09

    申请号:US941742

    申请日:1997-10-01

    摘要: A method for producing a soluble conductive polymer having acidic groups, which comprises subjecting to electrolytic polymerization (a) at least one compound selected from the group consisting of acidic group-substituted anilines, acidic group-substituted pyrroles, acidic group-substituted thiophenes, acidic group-substituted furans, acidic group-substituted selenophenes, acidic group-substituted tellurophenes, acidic group-substituted isothianaphthenes, acidic group-substituted isobenzofurans, acidic group-substituted isoindolines, acidic group-substituted isobenzoselenophenes, acidic group-substituted isobenzotellurophenes, and their metal salts, ammonium salts and substituted ammonium salts in a solution containing (b) a basic compound.

    摘要翻译: 一种制备具有酸性基团的可溶性导电聚合物的方法,包括进行电解聚合(a)至少一种选自酸性基团取代的苯胺,酸性取代的吡咯,酸性取代的噻吩,酸性的取代的噻吩, 酸取代的异硫酚,酸性取代的异苯并呋喃,酸性取代的异吲哚啉,酸性取代的异苯并硒吩,酸性取代的异苯并间苯基四氟酚,及其金属 盐,铵盐和取代的铵盐在含有(b)碱性化合物的溶液中。

    Soluble alkoxy-group substituted aminobenzenesulfonic acid aniline
conducting polymers
    10.
    发明授权
    Soluble alkoxy-group substituted aminobenzenesulfonic acid aniline conducting polymers 失效
    可溶性烷氧基取代氨基苯磺酸苯胺导电聚合物

    公开(公告)号:US5700399A

    公开(公告)日:1997-12-23

    申请号:US700994

    申请日:1996-08-21

    摘要: A soluble aniline conducting polymer characterized in that said conductive polymer comprises as a repeating unit an alkoxyl group-substituted aminobenzenesulfonic acid, its alkali metal salts, ammonium salts and/or substituted ammonium salts, and is a solid having a weight average molecular weight of about 1900 or more at room temperature, a conductive composition and electric conductor comprising the same, and a method for producing a soluble aniline conducting polymer having a weight average molecular weight of 10,000 t 3,240,000 characterized by polymerizing at least one compound (1) selected from the group consisting of an acidic group-substituted aniline, its alkali metal salts, ammonium salts and substituted ammonium salts in a solution containing a basic compound (2) using an oxidizing agent.

    摘要翻译: 一种可溶性苯胺导电聚合物,其特征在于所述导电聚合物包含烷氧基取代的氨基苯磺酸,其碱金属盐,铵盐和/或取代的铵盐作为重复单元,并且是重均分子量约为 1900以上,导电性组合物和含有该导电性组合物的电导体,以及制造重均分子量为10000t 3,240,000的可溶性苯胺导电聚合物的方法,其特征在于,聚合至少一种选自以下的化合物(1): 在使用氧化剂的碱性化合物(2)的溶液中由酸性基团取代的苯胺,其碱金属盐,铵盐和取代的铵盐组成的组。