    Abstract: A method of producing a roll of a continuous web of an optical film laminate, usable in a process of laminating an optical film sheet including a polarizing film and formed to a size corresponding to that an optical panel to a surface of the optical panel being fed to a lamination position, is disclosed. The polarizing film is prepared by subjecting a laminate including a thermoplastic resin substrate and a PVA type resin layer formed on the substrate, to uniaxial 2-stage stretching to reduce a thickness of the PVA type resin layer to 10 μm or less, and causing a dichroic material to be absorbed in the PVA type resin layer. A carrier film is releasably attached to the continuous web of optical film laminate including the polarizing film, through an adhesive layer. A defect inspection is performed for the optical film laminate and the adhesive layer.

    Abstract translation: 一种制造光学膜层叠体的连续卷筒纸的方法,可用于将包括偏振膜的光学膜片层压并且形成为与所述光学板相对应的尺寸的光学膜片的工艺,以提供给被馈送的光学板的表面 公开了层压位置。 通过对形成在基板上的热塑性树脂基板和PVA型树脂层的层叠体进行单轴2阶段拉伸,将PVA类树脂层的厚度缩小到10μm以下,制作偏光膜, 二色性材料被吸收在PVA型树脂层中。 载体膜通过粘合剂层可释放地附着到包括偏振膜的光学膜层压板的连续幅材上。 对光学膜层叠体和粘合剂层进行缺陷检查。

    METHOD OF PRODUCING ROLL OF LAMINATE STRIP WITH POLARIZING FILM
    2.
    发明申请
    METHOD OF PRODUCING ROLL OF LAMINATE STRIP WITH POLARIZING FILM 有权
    用偏光膜生产层压板的方法

    公开(公告)号:US20130114139A1

    公开(公告)日:2013-05-09

    申请号:US13728473

    申请日:2012-12-27

    CPC classification number: G02B5/305 B32B41/00 B32B2457/20 G02B5/3033

    Abstract: A method of producing a roll of an optical film laminate strip including a polarizing film includes the steps of: forming a continuous web of optical film laminate including a polarizing film which consists of a polyvinyl alcohol type resin layer and has a thickness of 10 μm or less, wherein the polarizing film is formed by performing an stretching sub-step of subjecting a laminate comprising a continuous web of thermoplastic resin substrate and a polyvinyl alcohol type resin layer formed on the substrate, to a uniaxial stretching in a lengthwise direction of the laminate based on 2-stage stretching consisting of preliminary in-air stretching and in-boric-acid-solution stretching; cutting the continuous web of optical film laminate along a direction parallel to the length direction to form at least one continuous web of laminate strip having a given width; and winding the continuous web of laminate strip having the given width into a roll.

    Abstract translation: 一种制造包括偏光膜的光学膜层压条的卷的方法包括以下步骤:形成包括由聚乙烯醇型树脂层组成的并具有10μm厚度的偏振膜的光学膜层压材料的连续幅材,或者 其特征在于,所述偏光膜是通过对形成在所述基材上的聚乙烯醇类树脂层的包含连续纤维网的层叠体在层叠体的长度方向进行单轴拉伸的拉伸工序进行拉伸, 基于由初步空气中拉伸和硼酸溶液拉伸组成的2段拉伸; 沿着与长度方向平行的方向切割光学膜层压板的连续卷材以形成具有给定宽度的至少一个连续的层压条带; 并将具有给定宽度的层压带的连续卷材卷绕成卷。

    OPTICAL LAMINATE WITH POLARIZING FILM
    4.
    发明申请
    OPTICAL LAMINATE WITH POLARIZING FILM 有权
    具有极化膜的光学层压板

    公开(公告)号:US20150316696A1

    公开(公告)日:2015-11-05

    申请号:US14647534

    申请日:2014-02-06

    Abstract: An optical laminate in which a polarizing film including a polyvinyl alcohol-based resin having oriented iodine is bonded on a first surface of the polarizing film to an optical film through an optically transparent adhesive layer is provided. The polarizing film exhibits a property that a value expressed by the following formula: Aa×(Is/Ia), is 0.53 or more, where: Aa represents an absorbance; Ia represents a value obtained by integrating a distribution of integrated intensities in the thickness direction of the polarizing film; and Is represents a value obtained by integrating, a distribution of integrated intensities in the thickness direction of the polarizing film; and the adhesive layer exhibits a property that a difference between a refractive index of the adhesive layer and a refractive index in the absorption axis direction of the polarizing film at the first surface of the polarizing film is 0.08 or less.

    Abstract translation: 提供了一种光学层叠体,其中包括具有取向碘的聚乙烯醇系树脂的偏振膜通过光学透明粘合剂层粘合在偏振膜的第一表面上与光学膜。 该偏光膜具有下述式所表示的值:Aa×(Is / Ia)为0.53以上,其中:Aa表示吸光度; Ia表示通过对偏振膜的厚度方向的积分强度分布进行积分而得到的值; Is表示通过对偏振膜的厚度方向的积分强度的分布进行积分而得到的值; 并且粘合剂层具有粘合剂层的折射率与偏振膜的第一表面的偏振膜的吸收轴方向的折射率之间的差为0.08以下的性质。

    LAMINATE, STRETCHED LAMINATE, MANUFACTURING METHOD OF STRETCHED LAMINATE, MANUFACTURING METHOD OF OPTICAL FILM LAMINATE HAVING POLARIZING FILM USING THE SAME, AND POLARIZING FILM
    6.
    发明申请
    LAMINATE, STRETCHED LAMINATE, MANUFACTURING METHOD OF STRETCHED LAMINATE, MANUFACTURING METHOD OF OPTICAL FILM LAMINATE HAVING POLARIZING FILM USING THE SAME, AND POLARIZING FILM 审中-公开
    层压板,拉伸层压板,拉伸层压板的制造方法,使用其的极化膜的光学薄膜层压板的制造方法和极化膜

    公开(公告)号:US20160377773A1

    公开(公告)日:2016-12-29

    申请号:US15263294

    申请日:2016-09-12

    Abstract: Provided is a laminate comprising a thermoplastic resin substrate and a polyvinyl alcohol based resin layer formed on the thermoplastic resin substrate, being used to form a polarizing film of the polyvinyl alcohol based resin layer treated with a post-process comprising at least a dyeing step of dyeing the polyvinyl alcohol based resin layer with a dichroic material, the post-process being performed after the polyvinyl alcohol based resin layer formed on the thermoplastic resin substrate is stretched together with the thermoplastic resin substrate, wherein the polyvinyl alcohol based resin layer comprises a polyvinyl alcohol based resin and urea.

    Abstract translation: 提供了一种层压体,其包含热塑性树脂基材和形成在热塑性树脂基材上的聚乙烯醇类树脂层,用于形成用后处理的聚乙烯醇类树脂层的偏振膜,所述后处理至少包含染色步骤 用二向色材料对聚乙烯醇系树脂层进行染色,在形成于热塑性树脂基板上的聚乙烯醇系树脂层之后进行的后处理与热塑性树脂基材一起拉伸,其中,聚乙烯醇类树脂层包含聚乙烯醇系树脂层 醇基树脂和尿素。

    LAMINATE, STRETCHED LAMINATE, MANUFACTURING METHOD OF STRETCHED LAMINATE, MANUFACTURING METHOD OF OPTICAL FILM LAMINATE HAVING POLARIZING FILM USING THE SAME, AND POLARIZING FILM
    7.
    发明申请
    LAMINATE, STRETCHED LAMINATE, MANUFACTURING METHOD OF STRETCHED LAMINATE, MANUFACTURING METHOD OF OPTICAL FILM LAMINATE HAVING POLARIZING FILM USING THE SAME, AND POLARIZING FILM 审中-公开
    层压板,拉伸层压板,拉伸层压板的制造方法,使用其的极化膜的光学薄膜层压板的制造方法和极化膜

    公开(公告)号:US20160377772A1

    公开(公告)日:2016-12-29

    申请号:US15263293

    申请日:2016-09-12

    Abstract: Provided is a laminate comprising a thermoplastic resin substrate and a polyvinyl alcohol based resin layer formed on the thermoplastic resin substrate, being used to form a polarizing film of the polyvinyl alcohol based resin layer treated with a post-process comprising at least a dyeing step of dyeing the polyvinyl alcohol based resin layer with a dichroic material, the post-process being performed after the polyvinyl alcohol based resin layer formed on the thermoplastic resin substrate is stretched together with the thermoplastic resin substrate, wherein the polyvinyl alcohol based resin layer comprises a polyvinyl alcohol based resin and a halide.

    Abstract translation: 提供了一种层压体,其包含热塑性树脂基材和形成在热塑性树脂基材上的聚乙烯醇类树脂层,用于形成用后处理的聚乙烯醇类树脂层的偏振膜,所述后处理至少包含染色步骤 用二向色材料对聚乙烯醇系树脂层进行染色,在形成于热塑性树脂基板上的聚乙烯醇系树脂层之后进行的后处理与热塑性树脂基材一起拉伸,其中,聚乙烯醇类树脂层包含聚乙烯醇系树脂层 醇基树脂和卤化物。

    METHOD OF PRODUCING ROLL OF LAMINATE STRIP WITH POLARIZING FILM
    8.
    发明申请
    METHOD OF PRODUCING ROLL OF LAMINATE STRIP WITH POLARIZING FILM 审中-公开
    用偏光膜生产层压板的方法

    公开(公告)号:US20160103258A1

    公开(公告)日:2016-04-14

    申请号:US14970113

    申请日:2015-12-15

    CPC classification number: G02B5/305 B32B41/00 B32B2457/20 G02B5/3033

    Abstract: Disclosed is a method of producing a roll of an optical film laminate strip including a polarizing film which has a thickness of 10 μm or less. The method comprises the steps of: forming a continuous web of optical film laminate including a polarizing film which consists of a polyvinyl alcohol type resin layer and has a thickness of 10 μm or less, wherein the polarizing film is formed by performing an stretching sub-step of subjecting a laminate comprising a continuous web of thermoplastic resin substrate and a polyvinyl alcohol type resin layer formed on the substrate, to a uniaxial stretching in a lengthwise direction of the laminate based on 2-stage stretching consisting of preliminary in-air stretching and in-boric-acid-solution stretching, to attain a stretching ratio of 5 to 8.5 to thereby reduce a thickness of the polyvinyl alcohol type resin layer to 10 μm or less, and an absorption sub-step of causing a dichroic material to be absorbed in the polyvinyl alcohol type resin layer; cutting the continuous web of optical film laminate along a direction parallel to the length direction to form at least one continuous web of laminate strip having a given width; and winding the continuous web of laminate strip having the given width into a roll.

    Abstract translation: 公开了一种制造包括厚度为10μm以下的偏光膜的光学膜层叠条的卷的方法。 该方法包括以下步骤:形成包括由聚乙烯醇型树脂层组成的厚度为10μm以下的偏振膜的光学膜层叠体的连续纤维网,其中通过进行拉伸子层而形成偏振膜, 将包含热塑性树脂基材的连续纤维网和形成在基材上的聚乙烯醇型树脂层的层压体在基于预备的空气内拉伸的2段拉伸和层压板的长度方向上的单轴拉伸下进行的步骤 硼酸 - 酸溶液拉伸,达到5〜8.5的拉伸比,从而将聚乙烯醇型树脂层的厚度减小到10μm以下,以及使二色性材料吸收的吸收子步骤 在聚乙烯醇型树脂层中; 沿着与长度方向平行的方向切割光学膜层压板的连续卷材以形成具有给定宽度的至少一个连续的层压条带; 并将具有给定宽度的层压带的连续卷材卷绕成卷。

    METHOD FOR PRODUCING POLARIZER
    10.
    发明申请
    METHOD FOR PRODUCING POLARIZER 有权
    生产极化剂的方法

    公开(公告)号:US20140016198A1

    公开(公告)日:2014-01-16

    申请号:US13933032

    申请日:2013-07-01

    Abstract: A method for producing a polarizer (20) comprises the steps of: (A) stretching a polyvinyl alcohol-based resin layer (10) to obtain a stretched layer (14); (B) immersing the stretched layer (14) in a dyeing liquid (23) containing iodine to obtain a dyed layer (18) in which absorbance thereof determined from a tristimulus value Y is from 0.4 to 1.0 (transmittance T=40% to 10%); and (C) removing a part of iodine adsorbed in the dyed layer (18) so that the absorbance of the dyed layer (18) decreases by 0.03 to 0.7, provided that the absorbance of the dyed layer (18) is controlled so that it does not become less than 0.3.

    Abstract translation: 一种偏光镜(20)的制造方法,其特征在于,包括以下工序:(A)拉伸聚乙烯醇类树脂层(10),得到拉伸层(14)。 (B)将拉伸层(14)浸渍在含有碘的染色液(23)中,得到由三色刺激值Y求出的吸光度为0.4〜1.0的透明层(18),透光率T = 40〜10 %); 以及(C)除去吸附在染色层(18)中的一部分碘,使得染色层(18)的吸光度减少0.03至0.7,只要染色层(18)的吸光度被控制,使得 不会小于0.3。