Nanocrystal-sized cerium-zirconium-aluminum oxide material and method of making the same

    公开(公告)号:US12227428B2

    公开(公告)日:2025-02-18

    申请号:US17422770

    申请日:2019-12-19

    Abstract: A nanocrystal-sized cerium-zirconium-aluminum mixed oxide material includes at least 20% by mass zirconium oxide; between 5% to 55% by mass cerium oxide; between 5% to 60% by mass aluminum oxide; and a total of 25% or less by mass of at least one oxide of a rare earth metal selected from the group of lanthanum, neodymium, praseodymium, or yttrium. The nanocrystal-sized cerium-zirconium-aluminum mixed oxide exhibits hierarchically ordered aggregates having a dso particle size less than 1.5 μm, and retains at least 80% of surface area and pore volume after ageing at temperature higher than 1000° C. for at least 6 hours. The nanocrystal-sized cerium-zirconium-aluminum mixed oxide material is prepared using a co-precipitation method followed by milling the dried and calcined oxide material. The nanocrystal-sized cerium-zirconium-aluminum mixed oxide material forms a particulate filter that may be used in an exhaust system arising from a gas or diesel engine.

    INORGANIC MATERIALS FOR USE IN A LITHIUM-ION SECONDARY BATTERY

    公开(公告)号:US20220393179A1

    公开(公告)日:2022-12-08

    申请号:US17770105

    申请日:2020-10-30

    Abstract: A cell for use in an electrochemical cell, such as a lithium-ion secondary battery that includes a positive electrode with an active material that acts as a cathode and a current collector; a negative electrode with an active material that acts as an anode and a current collector; a non-aqueous electrolyte; and a separator placed between the positive and negative electrodes. At least one of the cathode, the anode, the electrolyte, and the separator includes an inorganic additive in the form of a transition phase alumina or a type of boehmite that absorbs one or more of moisture and/or hydrogen fluoride (HF) that become present in the cell. One or more cells may be combined in a housing to form a lithium-ion secondary battery. The inorganic additive may also be incorporated as a coating applied to the internal wall of the housing.

    NANOCRYSTAL-SIZED CERIUM-ZIRCONIUM-ALUMINUM OXIDE MATERIAL AND METHOD OF MAKING THE SAME

    公开(公告)号:US20220064017A1

    公开(公告)日:2022-03-03

    申请号:US17422770

    申请日:2019-12-19

    Abstract: A nanocrystal-sized cerium-zirconium-aluminum mixed oxide material includes at least 20% by mass zirconium oxide; between 5% to 55% by mass cerium oxide; between 5% to 60% by mass aluminum oxide; and a total of 25% or less by mass of at least one oxide of a rare earth metal selected from the group of lanthanum, neodymium, praseodymium, or yttrium. The nanocrystal-sized cerium-zirconium-aluminum mixed oxide exhibits hierarchically ordered aggregates having a dso particle size less than 1.5 μm, and retains at least 80% of surface area and pore volume after ageing at temperature higher than 1000° C. for at least 6 hours. The nanocrystal-sized cerium-zirconium-aluminum mixed oxide material is prepared using a co-precipitation method followed by milling the dried and calcined oxide material. The nanocrystal-sized cerium-zirconium-aluminum mixed oxide material forms a particulate filter that may be used in an exhaust system arising from a gas or diesel engine

    INORGANIC MATERIALS FOR USE IN A LITHIUM-ION SECONDARY BATTERY

    公开(公告)号:US20210273293A1

    公开(公告)日:2021-09-02

    申请号:US17278685

    申请日:2020-10-30

    Abstract: A cell for use in an electrochemical cell, such as a lithium-ion secondary battery that includes a positive electrode with an active material that acts as a cathode and a current collector; a negative electrode with an active material that acts as an anode and a current collector; a non-aqueous electrolyte; and a separator placed between the positive and negative electrodes. At least one of the cathode, the anode, the electrolyte, and the separator includes an inorganic additive in the form of one or more zeolites having a Si:Al ratio ranging from 2-50 that absorbs one or more of moisture, free transition metal ions, or hydrogen fluoride that become present in the cell. One or more of the cells may be combined in a housing to form a lithium-ion secondary battery. The inorganic additive may also be incorporated as a coating applied to the internal wall of the housing.

    METHOD OF MAKING MESOPOROUS ZIRCONIUM-BASED MIXED OXIDES

    公开(公告)号:US20190112198A1

    公开(公告)日:2019-04-18

    申请号:US16088858

    申请日:2017-03-30

    Abstract: Mesoporous, zirconium-based mixed oxides and a method of making the same comprises: injecting a polyvalent metal-containing solution into an electrolyte solution to form a mother liquor; forming a precipitate; aging the precipitate in the mother liquor to form the mixed oxides; washing the mixed oxides with an aqueous medium; drying and collecting the mixed oxides. The pH of the electrolyte solution exceeds the isoelectric point for zirconium-based mixed oxides. The mixed oxides exhibit a single particle size distribution, improved Ce02 reducibility in the presence of Rhodium, a decrease in surface area after calcination (800-1 100° C.) that is not more than 55%, and a tetragonal/cubic structure after calcination. After calcination at 1 100° C. for 10 hours in air, the mixed oxides exhibit a surface area >25 m2/g, a pore volume >0.20 cm3/g, an average pore size >30 nm, and an average crystallite size between 8-15 nm.