摘要:
A silicone rubber composition is obtained by blending (A) 100 parts by weight of an organopolysiloxane composition of the addition reaction curing type with (B) about 30-400 parts by weight of aluminum hydroxide which has been surface treated with an organosilane or organosilazane substantially free of an aliphatic unsaturated group or a partial hydrolyzate thereof so that the aluminum hydroxide has 0.01-2% by weight of carbon affixed thereto. The composition maintains silicone rubber properties even though it is loaded with large amounts of aluminum hydroxide. It cures into a silicone rubber having improved high-voltage electrical insulating properties and thus suited for use as high-voltage electrical insulators.
摘要:
A mixture of a first aluminum hydroxide surface treated with a silicon-containing compound and having a mean particle size of 5-20 &mgr;m and a second aluminum hydroxide surface treated with a silicon-containing compound and having a mean particle size of 0.1-2.5 &mgr;m is blended in a silicone rubber composition comprising an organopolysiloxane, finely divided silica, and an organic peroxide. The silicone rubber composition cures into silicone rubber having sufficiently improved properties to serve as high-voltage electrical insulators, even when exposed to air polluted conditions or rigorous weather conditions.
摘要:
A silicone rubber composition is obtained by blending (A) 100 parts by weight of an organopolysiloxane composition of the organic peroxide or addition reaction curing type, with (B) 30-400 parts by weight of aluminum hydroxide which has been surface treated so as to bear 1.0.times.10.sup.-6 to 2.0.times.10.sup.-4 mol/gram of vinyl groups. The composition does not lose rubber strength even though it is loaded with large amounts of aluminum hydroxide. It cures into a silicone rubber having satisfactory physical properties and improved high-voltage electrical insulating properties and thus suited for use as high-voltage electrical insulators.
摘要:
A silicone rubber composition contains (A) 100 parts by weight of an organopolysiloxane composition of the organic peroxide or addition reaction curing type, (B) 20-400 parts by weight of aluminum hydroxide, and (C) 1-20 parts by weight of an organopolysiloxane of formula (I): R.sup.1.sub.a (OX).sub.b SiO.sub.(4-a-b)/2 wherein R.sup.1 is a monovalent hydrocarbon group, at least 10 mol % of the R.sup.1 groups being phenyl, X is hydrogen or a monovalent hydrocarbon group, a and b are positive numbers satisfying the range: 1.0.ltoreq.a
摘要翻译:硅橡胶组合物含有(A)100重量份的有机过氧化物或加成反应固化型的有机基聚硅氧烷组合物,(B)20-400重量份的氢氧化铝,和(C)1-20重量份的 式(I)的有机聚硅氧烷:R1a(OX)bSiO(4-ab)/ 2其中R1是一价烃基,R 1基团的至少10摩尔%为苯基,X为氢或一价烃基, 和b是满足以下范围的正数:1.0 aa <2.0,1
摘要:
A silicone rubber composition comprising (A) 100 parts by weight of an organopolysiloxane composition of the organic peroxide or addition curing type, (B) 1-100 parts by weight of finely divided silica, and (C) 30-500 parts by weight of aluminum hydroxide is suitable for use as a high-voltage electrical insulator. The aluminum hydroxide (C) has a water-soluble sodium ion content of up to 0.01% by weight and exhibits pH 6.5-8.0 and an electrical conductivity of up to 50 .mu.s/cm when measured as a 30 wt % water slurry and preferably has been treated to be hydrophobic. The composition cures into a silicone rubber having improved high-voltage electrical insulating properties even under rigorous conditions.
摘要翻译:一种硅橡胶组合物,其包含(A)100重量份的有机过氧化物或加成固化型的有机聚硅氧烷组合物,(B)1-100重量份的细分二氧化硅,和(C)30-500重量份的 氢氧化铝适合用作高压电绝缘体。 氢氧化铝(C)的水溶性钠离子含量高达0.01重量%,当以30重量%的水浆测定时,其pH值为6.5-8.0,电导率高达50μs/ cm 2,优选 已被处理为疏水性。 组合物即使在严格条件下也固化成具有改进的高电压电绝缘性能的硅橡胶。
摘要:
A thixotropic silicone rubber composition comprising (A) an organopolysiloxane having on the average at least two alkenyl groups in a molecule and a degree of polymerization of up to 1,200, (B) a liquid organohydrogenpolysiloxane having at least two hydrogen atoms each attached to a silicon atom, (C) aluminum hydroxide, (D) an addition reaction catalyst, (E) a thixotropic agent, and optionally (F) a tackifier cures at room temperature or elevated temperature into a silicone rubber having high strength and electrical insulating properties sufficient to serve as a high-voltage electrical insulator. The composition is so thixotropic that it may be used in repairing chipped portions of insulators.
摘要:
A release agent comprising a perfluoroalkyl ether silazane polymer or a perfluoroalkyl or perfluoroalkyl ether silazane/alkylsilazane copolymer and an organic solvent is suitable for use in molds for silicone base rubber molding. The agent offers effective, long-lasting release properties and ease of molding.
摘要:
A cationic silicone surfactant with excellent surface tension lowering properties and manufacturing method thereof were disclosed. Since a siloxane with a reactive group at one end is used as starting material for production process, the surfactant of the present invention is an AB type block copolymer which has an ideal structure as a surfactant and can exhibit excellent surface tension lowering properties in aqueous systems or solvent systems.
摘要:
An anionic silicone surfactant, with excellent surface tension lowering properties in aqueous and solvent systems, of the general formula ##STR1## wherein each R.sup.1 is an unsubstituted or halogen-substituted monovalent hydrocarbon group of 1-20 carbon atoms or a trialkylsiloxy group of 1-20 carbon atoms; R.sup.2 is an unsubstituted, halogen-substituted or hydroxyl-substituted bivalent hydrocarbon group of 1-10 carbon atoms, or a corresponding hydrocarbon group wherein no more than half of the carbon atoms are replaced by an oxygen atom; M is a Group A alkali metal or NR.sup.3 R.sup.4 R.sup.5 wherein R.sup.3, R.sup.4 and R.sup.5 are a hydrogen atom or a monovalent hydrocarbon group of 1-20 carbon atoms; and .sub.a is a number which lies in the range 0.ltoreq.a.ltoreq.20, is produced by reacting a corresponding organopolysiloxane which is terminated at one end by a silicon atom bearing a hydrogen atom with a compound of the general formula ##STR2## in the presence of a platinum catalyst, and reacting the thus-produced epoxy group-terminated organopolysiloxane with sodium or potassium bisulfite.
摘要翻译:在水性和溶剂体系中具有优异的表面张力降低性能的通式为“IMAGE”的阴离子硅氧烷表面活性剂,其中每个R 1是1-20个碳原子的未取代的或卤素取代的一价烃基或一个1-烷氧基甲硅烷氧基, 20个碳原子; R2是1-10个碳原子的未取代的,卤素取代的或羟基取代的二价烃基,或其中不超过一半的碳原子被氧原子代替的相应的烃基; M是A组碱金属或NR 3 R 4 R 5,其中R 3,R 4和R 5是氢原子或1-20个碳原子的一价烃基; 并且a是位于0 = a = 20范围内的数字是通过使一端被含有氢原子的硅原子的相应有机聚硅氧烷与通式为“IMAGE”的化合物 在铂催化剂的存在下,使由此制得的环氧基封端的有机聚硅氧烷与亚硫酸氢钠或亚硫酸氢钾反应。
摘要:
A liquid addition curing type silicone rubber composition comprising (A) an addition curing type organopolysiloxane component and (B) reinforcing silica fines having a specific surface area of 50-600 m2/g and surface treated with an organosilicon compound so as to bear 3-20% by weight of carbon on their surfaces prevents thickening after mixing and has an extended pot life.