Resin composition for imprinting
    1.
    发明授权

    公开(公告)号:US12129392B2

    公开(公告)日:2024-10-29

    申请号:US17627051

    申请日:2020-07-13

    摘要: Provided is a resin composition for imprinting excellent in imprint properties and optical properties such as high refractive index and low haze. The invention relates to a resin composition for imprinting containing: (A) a polysiloxane resin represented by the following formula (1): (R1SiO3/2)a(R22SiO2/2)b(R33SiO1/2)c(SiO4/2)d wherein R1, R2, and R3 are each independently a hydrogen atom, a hydroxy group, an alkoxy group, a C1-C12 hydrocarbon group, or a C1-C12 substituent having one or more crosslinkable functional groups, with at least one of R1, R2, or R3 being a C1-C12 substituent having one or more crosslinkable functional groups, and when a plurality of R1s, R2s, or R3s are present, they may be different from one another; and a, b, c, and d are numbers satisfying the following conditions: 0.001≤a≤1.00, 0≤b≤0.999, 0≤c≤0.30, 0≤d≤0.30, and a+b+c+d=1.0; and (B) a fine particulate inorganic oxide, wherein the ratio by weight of the sum of the polysiloxane resin (A) and optionally an alkoxysilane compound and a curable resin to the fine particulate inorganic oxide (B) is 0.2 to 2.5.

    Rubber composition for tire
    4.
    发明授权

    公开(公告)号:US12104046B2

    公开(公告)日:2024-10-01

    申请号:US18576038

    申请日:2022-03-25

    摘要: A rubber composition contains 10-50 parts by mass of a thermoplastic resin in 100 parts by mass of a diene rubber containing 60 mass % or more of a styrene-butadiene rubber having a styrene content of 5-30 mass % and a vinyl content of 10-35 mass %. In a mixture containing the diene rubber and the thermoplastic resin in a mass ratio of 1:1, a difference (Tga−Tgm) between a theoretical value (Tga) of a glass transition temperature of the mixture calculated based on an average glass transition temperature (Tg1) of the diene rubber and a glass transition temperature (Tg2) of the thermoplastic resin, and a measurement value (Tgm) of a glass transition temperature of the mixture, is lower than 5° C., and a difference (Tg2−Tg1) is 50-105° C. An amount of the thermoplastic resin is 30 mass % or more in 100 mass % total of a plasticizer component contained in the rubber composition.