Abstract:
The present invention relates to a composition that comprises a mixture of polymers, which comprises: a first polymer comprising polyphenylene sulphide, making up 55 wt % to 95 wt % of the mixture; a thermoplastic modifier, making up 5 wt % to 45 wt % of the mixture; optionally one or more functional additives, making up at most 10 wt % of the mixture, preferably at most 5 wt % of the mixture, characterised in that the thermoplastic modifier includes a second polymer which comprises a polyolefin backbone containing a group of at least one unsaturated monomer (X) and a plurality of polyamide grafts. The invention also relates to a multilayer structure including a plurality of adjacent layers, at least one of which consists of the aforementioned composition.
Abstract:
A composition including: between 45 and 94.95 wt. % of a matrix having at least one polyamide; between 0.05 and 20 wt. % of at least one prepolymer, the proportion by weight of the polyamide matrix and that of the prepolymer being respectively between 60 and 99.9 wt. % and between 40 and 0.1 wt. % in relation to the total amount of polyamide-prepolymer; between 5 and 45 wt. % of at least one impact modifier; and between 0 and 20% of an additive, said composition having a higher level of fluidity in the melted state than the same composition without prepolymer.
Abstract:
A transparent molding composition, including by weight: (a) from 30 to 90% of at least one (co)polyamide of formula PACMY/Z, (b) from 10 to 70% by weight of at least one semi-crystalline copolyamide of formula A/WS, (c) from 0 to 10% of at least one impact modifier chosen from the polyether block amides (PEBA) and the core-shell polymers, (d) from 0 to 2% by weight of at least one additive, (e) from 0 to 5% by weight of a prepolymer; the sum of the proportions of each constituent of said composition being equal to 100%, the composition having good alcohol resistance as determined by an ethanol resistance test.
Abstract:
A molding composition including by weight: (A) 45% to 90%, particularly 60% to 80%, more particularly 62.5% to 77.5% of at least one copolyamide with amide units (Bal) and polyether units (Ba2), (B) 5% to 30%, particularly 10% to 20%, more particularly 12.5% to 17.5% of carbon fibers, (C) 5% to 20%, particularly 10% to 15% of a hollow glass reinforcement, (D) 0% to 5%, preferably 0.1% to 2% of at least one additive, the sum of the proportions of each constituent (A)+(B)+(C)+(D) of the composition being equal to 100%.
Abstract:
A composition including: (A) from 29 to 74% by weight of at least one semi-crystalline aliphatic polyamide, the semi-crystalline aliphatic polyamide obtained from the polycondensation: of at least one C6 to C18 amino acid; or at least one C6 to C18 lactam; or at least one C4 to C36 diamine Ca with at least one C4 to C3 diacid Cb; (B) from 25 to 70% by weight of glass fibers mainly of silica dioxide (SiO2), aluminum oxide (Al2O3) and magnesium oxide (MgO); the glass fibers (B) having from 62 to 66% by weight of SiO2; (C) from 1 to 20% by weight of at least one impact modifier; and (D) from 0 to 2% by weight of at least one additive, excluding copper chromite, zinc sulfide, titanium dioxide, calcium carbonate and a polyolefin-based colored masterbatch; the sum of the various constituents (A) to (D) being 100% by weight.
Abstract:
The field of molded articles and fiber-reinforced thermoplastic compositions for obtaining them. The use of the reinforced thermoplastic composition for obtaining a thin molded article with reduced warpage. The composition may include: from 30 to 70% by weight of an amorphous polyamide matrix by total weight of the composition; from 30 to 70% by weight of glass fibers with a circular cross-section by total weight of the composition; and optionally additives.
Abstract:
A composition including at least two grafted copolymers having a polyolefin basic polymer chain and polyamide grafts, the polyamide grafts being 5 wt % and 35 wt % of the composition bonded to the first and second copolymer as well as a third component selected among certain polyamides, polyethylenes or polypropylenes or a mixture thereof. Also, a multilayer structure including a plurality of adjacent layers, at least one of which is the aforementioned composition.
Abstract:
The invention relates to the use of at least one prepolymer in a composition which includes: a matrix of at least one transparent semi-crystalline polyamide, and optionally at least one additive, for improving the crystallisation kinetics and reducing the warping of the composition while preserving or improving the transparency properties thereof as well as the mechanical properties thereof, in comparison with the same composition without a prepolymer, wherein the composition does not contain a nucleating agent.
Abstract:
The invention relates to a copolymer having polyamide PA blocks and polyether PE blocks, in which PA is of diamine.diacid X.Y type; X, the number of carbons of the diamine, is within the range from 6 to 14, and Y, the number of carbons of the diacid, is within the range from 6 to 18. The invention also relates to the use of the said copolymer in a process of direct adhesion between two TPE materials for increasing the peel strength between these materials.
Abstract:
The present invention relates to a molding composition comprising, by weight:
a) 20% to 60% of at least one long-chain aliphatic polyamide having a number of carbon atoms per nitrogen atom of greater than or equal to 9, said at least one polyamide having an inherent viscosity in solution of less than or equal to 1.3, as determined in accordance with the standard ISO 307:2007 at a temperature of 20° C., b) 40% to 75% of glass fibers, and c) 0% to 5% by weight, by weight of at least one additive, the sum of the proportions of each constituent of said composition being equal to 100%, with the exclusion of an amorphous polyamide and a microcrystalline polyamide.