Abstract:
In a female crimp terminal including a pressure-bonding section for permitting pressure-bonding and connection to an aluminum core wire of an insulated wire, the pressure-bonding section is configured in a hollow sectional shape by a plate material, and a long length direction weld portion in a long length direction is welded, a forward part in the hollow sectional shape is caused to take an almost flat plate-shaped sealing shape and a width direction weld portion in a width direction is welded.
Abstract:
In an electrical wire connecting structure and a method of manufacturing the electrical wire connecting structure, a terminal having a tube-shaped portion of 2.0 mm in inner diameter is prepared for an electrical wire having a conductor cross-sectional area of 0.72 to 1.37 mm2, the electrical wire 13 is inserted into an electrical wire insertion port of the tube-shaped portion of the electrical wire, and the tube-shaped portion and the core wire portion of the electrical wire are compressed to be crimp-connected to each other. Furthermore, a terminal having a tube-shaped portion of 3.0 mm in inner diameter is prepared for an electrical wire having a conductor cross-sectional area of 1.22 to 2.65 mm2, the electrical wire is inserted into the electrical wire insertion port of the tube-shaped portion 25 of the electrical wire, and the tube-shaped portion and the core wire portion of the electrical wire are compressed to be crimp-connected to each other.
Abstract:
The present disclosure provides an aluminum alloy wire or the like which can secure a high conductivity and a moderately low yield strength, and realize both a high elongation and a moderate tensile strength.An aluminum alloy wire of the present disclosure contains 0.10 to 1.00% by mass of Mg, 0.10 to 1.20% by mass of Si, 0.10 to 1.40% by mass of Fe, 0 to 0.10% by mass of Ti, 0 to 0.030% by mass of B, 0 to 1.00% by mass of Cu, 0 to 1.00% by mass of Mn, 0 to 1.00% by mass of Cr, 0 to 0.50% by mass of Zr, and 0 to 0.50% by mass of Ni, the balance being Al and 0.30% by mass or less of impurities. Coarse crystal grains are present in a vertical cross-sectional structure of the wire taken in a lengthwise direction of the wire. The greatest grain size of the coarse crystal grains as measured in the lengthwise direction of the wire is equal to or greater than a diameter of the wire. A proportion of an area of the coarse crystal grains to the total of the areas of all the crystal grains within a range of the vertical cross-sectional structure in which the vertical cross-sectional structure is measured, is 50% or more. Elongation of the wire is 10% or more.
Abstract:
An aluminum alloy wire rod having a composition comprising Mg: 0.10-1.00 mass %, Si: 0.10-1.00 mass %, Fe: 0.01-1.40 mass %, Ti: 0.000-0.100 mass %, B: 0.000-0.030 mass %, Cu: 0.00-1.00 mass %, Ag: 0.00-0.50 mass %, Au: 0.00-0.50 mass %, Mn: 0.00-1.00 mass %, Cr: 0.00-1.00 mass %, Zr: 0.01-0.50 mass %, Hf: 0.00-0.50 mass %, V: 0.00-0.50 mass %, Sc: 0.00-0.50 mass %, Co: 0.00-0.50 mass %, and Ni: 0.00-0.50 mass %. Mg/Si ratio is greater than 1. A dispersion density of compound particles having a particle size of 20 nm to 1000 nm is greater than or equal to 1 particle/μm2. In a distribution of the compound particles in the aluminum alloy wire rod, a maximum dispersion density of the compound particles is less than or equal to five times a minimum dispersion density of the compound particles.
Abstract:
An aluminum alloy wire rod comprising 0.1-1.0 mass % Mg; 0.1-1.0 mass % Si; 0.01-1.40 mass % Fe; 0.01-0.50 mass % Zr; 0.000-0.100 mass % Ti; 0.000-0.030 mass % B; 0.00-1.00 mass % Cu; 0.00-0.50 mass % Ag; 0.00-0.50 mass % Au; 0.00-1.00 mass % Mn; 0.00-1.00 mass % Cr; 0.00-0.50 mass % Hf; 0.00-0.50 mass % V; 0.00-0.50 mass % Sc; 0.00-0.50 mass % Co; and 0.00-0.50 mass % Ni, a Mg/Si ratio being greater than 1, wherein a dispersion density of an Mg2Si compound having a particle size of 0.5 μm to 5.0 μm is less than or equal to 3.0×10−3 particles/μm2, and in the sectional structure, a concentration of each of Mg and Si other than a compound is less than or equal to 2.00 mass %.
Abstract:
An aluminum alloy wire rod has a composition consisting of 0.1-1.0 mass % Mg; 0.1-1.0 mass % Si; 0.01-1.40 mass % Fe; 0.000-0.100 mass % Ti; 0.000-0.030 mass % B; 0.00-1.00 mass % Cu; 0.00-0.50 mass % Ag; 0.00-0.50 mass % Au; 0.00-1.00 mass % Mn; 0.00-1.00 mass % Cr; 0.00-0.50 mass % Zr; 0.00-0.50 mass % Hf; 0.00-0.50 mass % V; 0.00-0.50 mass % Sc; 0.00-0.50 mass % Co; 0.00-0.50 mass % Ni; and the balance being Al and incidental impurities, wherein at least one or none of Ti, B, Cu, Ag, Au, Mn, Cr, Zr, —Hf, V, Sc, Co and Ni is contained in the composition. A dispersion density of an Mg2Si compound having a particle size of 0.5 μm to 5.0 μm is less than or equal to 3.0×10−3 particles/μm2. In a sectional structure, a concentration of each of Si and Mg other than a compound is less than or equal to 2.00 mass %.
Abstract:
In an electrical wire connecting structure and a method of manufacturing the electrical wire connecting structure, a terminal having a tube-shaped portion of 2.0 mm in inner diameter is prepared for an electrical wire having a conductor cross-sectional area of 0.72 to 1.37 mm2, the electrical wire 13 is inserted into an electrical wire insertion port of the tube-shaped portion of the electrical wire, and the tube-shaped portion and the core wire portion of the electrical wire are compressed to be crimp-connected to each other. Furthermore, a terminal having a tube-shaped portion of 3.0 mm in inner diameter is prepared for an electrical wire having a conductor cross-sectional area of 1.22 to 2.65 mm2, the electrical wire is inserted into the electrical wire insertion port of the tube-shaped portion 25 of the electrical wire, and the tube-shaped portion and the core wire portion of the electrical wire are compressed to be crimp-connected to each other.
Abstract:
A metal member includes a base material composed of one of copper and a copper alloy, a white metal layer provided on the base material at a part or an entirety thereof, and an oil film provided on the white metal layer. The white metal layer has a thickness of 0.01 μm to 0.80 μm. A surface of the white metal layer has an arithmetic mean roughness of 0.6 μm to 1.2 μm. The oil film has an electric double-layer capacitance of 1.5 μF/cm2 to 7.0 μF/cm2.
Abstract translation:金属构件包括由铜和铜合金中的一种构成的基材,在其一部分或全部设置在基材上的白色金属层和设置在白色金属层上的油膜。 白色金属层的厚度为0.01μm〜0.80μm。 白色金属层的表面的算术平均粗糙度为0.6μm〜1.2μm。 油膜的电双层电容为1.5μF/ cm 2〜7.0μF/ cm 2。
Abstract:
An aluminum alloy wire rod has a composition consisting of Mg: 0.10 to 1.00 mass %, Si: 0.10 to 1.00 mass %, Fe: 0.01 to 1.40 mass %, Ti: 0.000 to 0.100 mass %, B: 0.000 to 0.030 mass %, Cu: 0.00 to 1.00 mass %, Ag: 0.00 to 0.50 mass %, Au: 0.00 to 0.50 mass %, Mn: 0.00 to 1.00 mass %, Cr: 0.00 to 1.00 mass %, Zr: 0.00 to 0.50 mass %, Hf: 0.00 to 0.50 mass %, V: 0.00 to 0.50 mass %, Sc: 0.00 to 0.50 mass %, Co: 0.00 to 0.50 mass %, Ni: 0.00 to 0.50 mass %, and the balance: Al and incidental impurities. A dispersion density of compound particles having a size of 20-1000 nm is 1 particle/μm2 or higher. In a distribution of the compound particles in the aluminum alloy wire rod, a maximum dispersion density of the compound particles is less than or equal to five times a minimum dispersion density of the compound particles.
Abstract:
An aluminum alloy wire rod has a composition consisting of 0.10-1.00 mass % Mg; 0.10-1.00 mass % Si; 0.01-1.40 mass % Fe; 0.000-0.100 mass % Ti; 0.000-0.030 mass % B; 0.00-1.00 mass % Cu; 0.00-0.50 mass % Ag; 0.00-0.50 mass % Au; 0.00-1.00 mass % Mn; 0.00-1.00 mass % Cr; 0.00-0.50 mass % Zr; 0.00-0.50 mass % Hf; 0.00-0.50 mass % V; 0.00-0.50 mass % Sc; 0.00-0.50 mass % Co; 0.00-0.50 mass % Ni; and the balance being Al and incidental impurities, wherein at least one of Ti, B, Cu, Ag, Au, Mn, Cr, Zr, Hf, V, Sc, Co and Ni is contained in the composition or none of Ti, B, Cu, Ag, Au, Mn, Cr, Zr, Hf, V, Sc, Co and Ni is contained in the composition. A precipitate free zone exists inside a crystal grain, and the precipitate free zone has a width of less than or equal to 100 nm.