Process for the continuous synthesis of methylamines
    12.
    发明授权
    Process for the continuous synthesis of methylamines 有权
    连续合成甲胺的方法

    公开(公告)号:US07435855B2

    公开(公告)日:2008-10-14

    申请号:US11629801

    申请日:2005-06-16

    IPC分类号: C07C209/14

    CPC分类号: C07C209/16 C07C211/04

    摘要: Process for the continuous synthesis of methylamines by reaction of methanol and/or dimethyl ether with ammonia in the presence of a heterogeneous catalyst, wherein the catalyst used is a shaped body which comprises a microporous material and at least one organosilicon compound as binder and can be produced by a process comprising the steps (I) preparation of a mixture comprising the microporous material, the binder, a pasting agent and a solvent, (II) mixing and densification of the mixture, (III) shaping of the densified mixture to give a shaped body, (IV) drying of the shaped body and (V) calcination of the dried shaped body.

    摘要翻译: 在多相催化剂存在下,通过甲醇和/或二甲醚与氨的反应连续合成甲胺的方法,其中使用的催化剂是成形体,其包含微孔材料和至少一种有机硅化合物作为粘合剂,并且可以是 通过包括步骤(I)制备包含微孔材料,粘合剂,粘贴剂和溶剂的混合物的方法制备的方法制备,(II)混合和混合物的致密化,(III)使致密混合物成形,得到 (IV)成型体的干燥和(V)干燥成型体的煅烧。

    Shaped Catalyst Bodies with Characteristics of Ion Exchangers
    15.
    发明申请
    Shaped Catalyst Bodies with Characteristics of Ion Exchangers 审中-公开
    具有离子交换器特征的成型催化剂体

    公开(公告)号:US20100160667A1

    公开(公告)日:2010-06-24

    申请号:US12376975

    申请日:2007-08-07

    摘要: Processes comprising: (a) providing a shaped body having a surface and comprising a metal oxide, and impregnating the shaped body with a liquid comprising an unsaturated compound; (b) subjecting the impregnated shaped body to thermolysis under an inert gas atmosphere at a temperature of 250 to 400° C., such that at least 10% by weight of the unsaturated compound is thermalized to form a layer of a high molecular weight polyaromatic on at least a portion of the surface of the shaped body; and (c) reacting the shaped body with a reagent to functionalize the polyaromatic layer, wherein the shaped body has a smallest dimension in any spatial direction of at least 1 mm to provide a shaped catalyst body having ion- exchange properties; shaped catalyst bodies prepared thereby and uses therefor as catalysts.

    摘要翻译: 方法包括:(a)提供具有表面并包含金属氧化物的成形体,并用包含不饱和化合物的液体浸渍成形体; (b)使浸渍的成形体在惰性气体气氛下在250-400℃的温度下进行热分解,使得至少10重量%的不饱和化合物被热化以形成高分子量多芳族化合物 在所述成形体的表面的至少一部分上; 和(c)使成形体与试剂官能化以使多芳族化合物官能化,其中成形体在任何空间方向上具有至少1mm的最小尺寸以提供具有离子交换性能的成形催化剂体; 由此制备的催化剂体作为催化剂。