Abstract:
The present invention relates to an absorbent structure suitable in, or being an adult or infant diaper or feminine hygiene article, comprising a water-absorbing material comprising water-absorbing particles that comprise a film coating, comprising an elastic film-forming polymer and a coalescing agent.The invention also relates to an absorbent structure comprising a water absorbent material obtainable by a process of: a) spray-coating water-absorbing polymeric particles with an elastic film-forming polymer in a fluidized bed reactor at a temperature in the range from 0° C. to 150° C. and b) heat-treatment of the coated polymeric particles at a temperature above 50° C., wherein in step a) and/or b) a coalescing agent is added.
Abstract:
The invention concerns water-absorbing polymeric particles possessing high saline flow conductivity in the swollen state which comprise insoluble metal sulfates as synergistic fillers, and also a process for their production and their use.
Abstract:
The present invention relates to a process for postcrosslinking water-absorbing polymeric particles in the absence of oxidizing gases, to the water-absorbing polymers preparable by the process and to their use in hygiene articles and packaging materials.
Abstract:
(Meth)acrylate salt polymers are prepared by free-radical polymerization of (meth)acrylate salt with or without other monomers in an aqueous medium by using a supersaturated aqueous solution of (meth)acrylate salt. The resulting highly concentrated reaction mixtures are notable for their high solids content and increased space-time yield.
Abstract:
The invention relates to finely divided water-absorbing polymeric particles having high fluid transportation and absorption performance, the Centrifuge Retention Capacity (CRC) being not less than 26 g/g, the absorbency under a load of 4.83 kPa (AUL 1.7 psi) not less than 23 g/g and the Transportation Value (TV) not less than 15,000 cm3s, the Transportation Value (TV) being the product of Saline Flow Conductivity (SFC) and wicking absorption after 60 minutes (DA60) multiplied by 107, and wherein the wicking absorption after 60 minutes (DA60) is the weight of 0.9% by weight sodium chloride solution absorbed by 70 g of the water-absorbing polymeric particles in 60 minutes, wherein the water-absorbing polymeric particles are situated, during measurement, in a circularly round vessel which has an internal diameter of 6 cm and is sealed at its lower end by a sieve base of 36 μm mesh size, and the sieve base is in atmospheric contact with 0.9% by weight sodium chloride solution, processes for their preparation and also their use in hygiene articles and packaging materials.
Abstract:
The present invention relates to a process for postcrosslinking water-absorbing polymeric particles in the absence of oxidizing gases, to the water-absorbing polymers preparable by the process and to their use in hygiene articles and packaging materials.
Abstract:
The present invention relates to novel (meth)acrylic esters of polyalkoxylated glycols of the formula where AO is independently at each instance is —O—CHR3-CHR4- or —CHR3-CHR4-O— where R3 and R4 are independently H, linear or branched C1-C8-alkyl, p1 is 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20, 21, 22, 23, 24, 25, 26, 27, 28, 29, 30, 31, 32, 33, 34, or 35, p2 is 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20, 21, 22, 23, 24, 25, 26, 27, 28, 29, 30, 31, 32, 33, 34, or 35, n is 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20, 21, 22, 23, 24, 25, 26, 27, 28, 29, 30, 31, 32, 33, 34, 35, 36, 37, 38, 39, 40, 41, 42, 43, 44, 45, 46, 447, 48, 49, 50, 51, 52, 53, 54, 55, 56, 57, 58, 59, 60, 61, 62, 63, 64, 65, 66, 67, 68, 69, 70, 71, 72, 73, 74, 75, 76, 77, 78, 79, 80, 81, 82, 83, 84, 85, 86, 87, 88, 89, 90, 91, 92, 93, 94, 95, 96, 97, 98, 99, 100, R1 and R2 are independently H or CH3, wherein there is at least one AO in (AO)p1 and also at least one AO in (AO)p2 where R3 and R4 are not both H at one and the same time, a simplified process for preparing these esters and use of reaction mixtures thus obtainable.
Abstract:
Described is a water absorbent comprising (a) particles of a water absorbent polymer, and (b) a nitrogenous polymer containing from 5 to 17 mol/kg, based on the total weight of the nitrogenous polymer, of protonatable nitrogen atoms. The water absorbent possesses an improved property profile featuring high absorptive capacity, improved fluid transmission and high wet strength.
Abstract:
The present invention relates to a water absorbing material obtainable by a process comprising the steps of bringing particles of a non surface-crosslinked water-absorbing polymer in contact with a) at least one postcrosslinker, b) 10-1000 ppm, based on the non surface-crosslinked water-absorbing polymer, of at least one Nitrogen-containing water-soluble polymer of which the Nitrogen can be protonated, and c) at least one hydrophobic polymer and heat-treating the particles thus obtained at a temperature in the range from 120° C. to 300° C. and a method for the production thereof.
Abstract:
To prepare superabsorbents with a low residual monomer content, a salt of urea with an inorganic acid is added to the monomer mixture before or during the polymerization or to the polymer after the polymerization but before a heat treatment which follows the polymerization.