Use of amphiphilic copolymers as agents for improving the thermal stability and UV resistance of chlorinated and filled thermoplastic materials, process for the fabrication of the said materials
    15.
    发明授权
    Use of amphiphilic copolymers as agents for improving the thermal stability and UV resistance of chlorinated and filled thermoplastic materials, process for the fabrication of the said materials 有权
    使用两亲共聚物作为改善氯化和填充热塑性材料的热稳定性和抗紫外线性的试剂,用于制造所述材料的方法

    公开(公告)号:US08741997B2

    公开(公告)日:2014-06-03

    申请号:US13513027

    申请日:2010-12-06

    摘要: The present invention consists of the use, in a chlorinated and filled thermoplastic composition containing at least one chlorinated thermoplastic resin and at least one mineral filler, as an agent improving the thermal stability and UV resistance of the said composition, of a linear amphiphilic copolymer characterized in that: it consists of at least one hydrophilic monomer and at least one hydrophobic monomer, it has an average molar mass by weight of between 5,000 g/mol and 20,000 g/mol and a polymolecularity index less than or equal to 3, and preferentially an average molar mass by weight of between 10,000 g/mol and 15,000 g/mol, and a polymolecularity index less than or equal to 2.5. It also concerns a manufacturing process for a chlorinated and filled thermoplastic composition implementing the said copolymer, as well as the composition obtained directly by the said process.

    摘要翻译: 本发明包括在含有至少一种氯化热塑性树脂和至少一种矿物填料的氯化和填充的热塑性组合物中作为改善所述组合物的热稳定性和抗紫外线性的试剂,使用线性两亲共聚物,其特征在于 其特征在于:它由至少一种亲水性单体和至少一种疏水单体组成,平均摩尔质量重量为5,000g / mol至20,000g / mol,多分子指数小于或等于3,优先 平均摩尔质量重量在10,000g / mol至15,000g / mol之间,多分子指数小于或等于2.5。 它还涉及实施所述共聚物的氯化和填充的热塑性组合物的制造方法,以及通过所述方法直接获得的组合物。