Abstract:
A method of fabricating p-type metal oxide semiconductor (PMOS) transistor devices on a common substrate is presented. The method provides a first portion of semiconductor material and a second portion of semiconductor material on the common substrate. The first portion of semiconductor material and the second portion of semiconductor material are insulated from each other. The method continues by creating first PMOS transistor devices using the first portion of semiconductor material. The first PMOS transistor devices include stressor regions that impart compressive stress to channel regions of the first PMOS transistor devices. The method also creates second PMOS transistor devices using the second portion of semiconductor material. The second PMOS transistor devices do not include channel stressor regions.
Abstract:
A stress-enhanced semiconductor device is provided which includes a substrate having an inactive region and an active region, a first-type stress layer overlying at least a portion of the active region, and a second-type stress layer. The active region includes a first lateral edge which defines a first width of the active region, and a second lateral edge which defines a second width of the active region. The second-type stress layer is disposed adjacent the second lateral edge of the active region.
Abstract:
A method includes receiving design data associated with an integrated circuit device. The integrated circuit device includes a first element having a corner defined therein and a second element overlapping the first element. A dimension specified for the first element in the design data is adjusted based on a distance between the second element and the corner. The integrated circuit device is simulated based on the adjusted dimension.
Abstract:
A method of forming a silicon-on-insulator semiconductor device including providing a substrate and forming a trench in the substrate, wherein the trench includes opposing side walls extending upwardly from a base of the trench. The method also includes depositing at least two insulating layers into the trench to form a shallow trench isolation structure, wherein an innermost of the insulating layers substantially conforms to the base and the two side walls of the trench and an outermost of the insulating layers spans the side walls of the trench so that a gap is formed between the insulating layers in the trench. The gap creates compressive forces within the shallow trench isolation structure, which in turn creates tensile stress within the surrounding substrate to enhance mobility of the device.
Abstract:
A method of manufacturing a semiconductor device, comprising steps of: (a) providing a semi conductor substrate including at least one dopant species-containing region extending to a surface of the substrate; (b) forming a thin liner oxide layer on the surface of the substrate; and (c) incorporating in the thin line oxide layer at least one species which substantially prevents, or at least reduces, segregation therein of the dopant species arising from movement thereinto from the at least one dopant species-containing region.
Abstract:
A method of manufacturing a semiconductor device, comprising sequential steps of: (a) providing a semiconductor substrate including a pre-selected thickness strained lattice layer of a first semiconductor material at an upper surface thereof and an underlying layer of a second semiconductor material; and (b) introducing a dopant-containing species of one conductivity type into at least one pre-selected portion of the strained lattice layer of first semiconductor material to form a dopant-containing region therein with a junction at a depth substantially equal to the pre-selected thickness, wherein the second semiconductor material of the underlying layer inhibits diffusion thereinto of the dopant-containing species from the strained lattice layer, thereby controlling/limiting the depth of the junction to substantially the pre-selected thickness of the strained lattice layer.
Abstract:
A method of reducing an effective channel length of a lightly doped drain transistor (50), includes the steps of forming a gate electrode (52) and a gate oxide (54) over a semiconductor substrate (56) and implanting a drain region (58) of the substrate (56) with a sub-amorphous large tilt angle implant to thereby supply interstitials (62) at a location under the gate oxide (54). The method also includes forming a lightly doped drain extension region (66) in the drain region (58) of the substrate (56) and forming a drain (70) in the drain region (58) and forming a source extension region (67) and a source (72) in a source region (60) of the substrate (56). Lastly, the method includes thermally treating the substrate (56), wherein the interstitials (62) enhance a lateral diffusion (84) under the gate oxide (54) without substantially impacting a vertical diffusion (86) of the extension regions (66, 67), thereby reducing the effective channel length without an increase in a junction depth of the drain (70) and the drain extension region (66) or the source (72) and the source extension region (67).
Abstract:
A semiconductor device is formed with low resistivity self aligned silicide contacts with high-K/metal gates. Embodiments include postponing silicidation of a metal layer on source/drain regions in a silicon substrate until deposition of a high-K dielectric, thereby preserving the physical and morphological properties of the silicide film and improving device performance. An embodiment includes forming a replaceable gate electrode on a silicon-containing substrate, forming source/drain regions, forming a metal layer on the source/drain regions, forming an ILD over the metal layer on the substrate, removing the replaceable gate electrode, thereby forming a cavity, depositing a high-K dielectric layer in the cavity at a temperature sufficient to initiate a silicidation reaction between the metal layer and underlying silicon, and forming a metal gate electrode on the high-K dielectric layer.
Abstract:
A semiconductor device is formed with low resistivity self aligned silicide contacts with high-K/metal gates. Embodiments include postponing silicidation of a metal layer on source/drain regions in a silicon substrate until deposition of a high-K dielectric, thereby preserving the physical and morphological properties of the silicide film and improving device performance. An embodiment includes forming a replaceable gate electrode on a silicon-containing substrate, forming source/drain regions, forming a metal layer on the source/drain regions, forming an ILD over the metal layer on the substrate, removing the replaceable gate electrode, thereby forming a cavity, depositing a high-K dielectric layer in the cavity at a temperature sufficient to initiate a silicidation reaction between the metal layer and underlying silicon, and forming a metal gate electrode on the high-K dielectric layer.
Abstract:
Apparatus for semiconductor device structures and related fabrication methods are provided. A method for fabricating a semiconductor device structure on an isolated region of semiconductor material comprises forming a plurality of gate structures overlying the isolated region of semiconductor material and masking edge portions of the isolated region of semiconductor material. While the edge portions are masked, the fabrication method continues by forming recesses between gate structures of the plurality of gate structures and forming stressor regions in the recesses. The method continues by unmasking the edge portions and implanting ions of a conductivity-determining impurity type into the stressor regions and the edge portions.