摘要:
A polymer composition comprises at least two polymer components, the first component having an ATREF peak temperature, Tpeak1, and a viscosity average molecular weight, Mv1, and the second component having an ATREF peak temperature, Tpeak2, and a viscosity average molecular weight, Mv2, wherein the temperature differential between Tpeak2 and Tpeak1 decreases with increased composition density and Mv1/Mv2 is less than or equal to 1.2. the composition is further characterized as having a Mw/Mn of less than or equal to 3.3, an I10/I2>6.6, and a composition density less than 0.945 gram/cubic centimeter.
摘要翻译:聚合物组合物包含至少两种聚合物组分,第一组分具有ATREF峰温度T max 1和粘度平均分子量M 1 v 1,并且第二组分 具有ATREF峰值温度T 2峰2和粘度平均分子量M 2 V 2,其中T 2峰2和T 2之间的温差, SUB> peak1 SUB>随着组成密度的增加而降低,并且M 1/2 / M 2 V 2小于或等于1.2。 该组合物进一步被表征为具有小于或等于3.3的M SUB / 2,组成密度小于0.945克/立方厘米。
摘要:
The present invention pertains to an ethylene interpolymer composition characterized as having a narrow molecular weight distribution (MWD) and optimized compositional uniformity, a process for making such a composition and a fabricated article made from such composition. The novel composition is characterized as having at least two polymer components, the first component having an ATREF peak temperature, Tpeak1 and a viscosity average molecular weight, Mv1, and the second component having an ATREF peak temperature, Tpeak2, and a viscosity average molecular, Mv2, wherein the temperature differential between Tpeak2 and Tpeak1 decreases with iincreased composition density and Mv1/Mv2 is less than or equal to 1.2. The novel composition exhibits high, balanced toughness properties, good processibility and surprisingly improved optical properties and is particularly well-suited for use in applications such as lamination films trash can liners and heavy duty shipping bags, especially as a blown film.
摘要:
The subject invention provides a film having at least one layer comprising an interpolymer of ethylene and at least one comonomer selected from the group consisting of C3-C20 &agr;-olefins, dienes, and cycloalkenes, wherein the interpolymer is characteried as having a high degree of processability good optical performance, and good mechanical properties. The subject invention further provides film fabrication processes and polymer compositions which are useful in preparing the subject films.
摘要:
The invention provides an apparatus for polymer chromatography, comprising at least one column that comprises a first stationary phase comprising one of the following: A) a material comprising at least one non-carbon atom, excluding glass or a metal, selected from molybdenum sulfide MoS2, tungsten sulfide WS2, silicon carbide SiC, boron nitride BN, or combinations thereof, or B) glass, or a metal, or combinations thereof, and a material comprising at least one non-carbon atom selected from molybdenum sulfide MoS2, tungsten sulfide WS2, silicon carbide SiC, boron nitride BN, or combinations thereof. The invention also provides a method for polymer chromatography, comprising introducing a solution, comprising a polymer, into a liquid flowing through a first stationary phase, and wherein the first stationary phase comprises one of foregoing materials (A) or (B).
摘要:
The instant invention provides an ethylene/alpha-olefin interpolymer suitable for use in fiber applications, and fibers made therefrom. The ethylene/alpha-olefin interpolymer according to the present invention has a CDBI of less than 60%, and comprises at least two fractions in crossfractionation of the ethylene/alpha-olefin interpolymer, eluting from 85° C. to 90° C. and from 90° C. to 95° C., comprising a weight fraction ratio of >0.68 and a molecular weight homogeneity index of greater than 0.65; wherein the weight fraction ratio is the ratio of the weight of polymer in each fraction divided by the weight of polymer eluting between 95° C. and 100° C. and the molecular weight homogeneity index is the ratio of the weight average molecular weight of the polymer in the fraction divided by the weight average molecular weight of the polymer eluting between 95° C. and 100° C., and wherein the ethylene/alpha-olefin interpolymer has a density in the range of from 0.920 to 0.965 g/cm3, and a melt index (I2) in the range of from 0.5 to 100 g/10 minutes, and melt flow ratio (I10/I2) in the range of from 5.8 to 8.
摘要:
The instant invention provides an ethylene/alpha-olefin interpolymer suitable for use in fiber applications, and fibers made therefrom. The ethylene/alpha-olefin interpolymer according to the present invention has a CDBI of less than 60%, and comprises at least two fractions in crossfractionation of the ethylene/alpha-olefin interpolymer, eluting from 85° C. to 90° C. and from 90° C. to 95° C., comprising a weight fraction ratio of >0.68 and a molecular weight homogeneity index of greater than 0.65; wherein the weight fraction ratio is the ratio of the weight of polymer in each fraction divided by the weight of polymer eluting between 95° C. and 100° C. and the molecular weight homogeneity index is the ratio of the weight average molecular weight of the polymer in the fraction divided by the weight average molecular weight of the polymer eluting between 95° C. and 100° C., and wherein the ethylene/alpha-olefin interpolymer has a density in the range of from 0.920 to 0.965 g/cm3, and a melt index (I2) in the range of from 0.5 to 100 g/10 minutes, and melt flow ratio (I10/I2) in the range of from 5.8 to 8.
摘要:
An ethylenic polymer comprising amyl groups from about 0.1 to about 2.0 units per 1000 carbon atoms as determined by Nuclear Magnetic Resonance and both a peak melting temperature, Tm, in ° C., and a heat of fusion, Hf, in J/g, as determined by DSC Crystallinity, where the numerical values of Tm and Hf correspond to the relationship Tm≧(0.2143*Hf)+79.643. An ethylenic polymer comprising at least one preparative TREF fraction that elutes at 95° C. or greater using a Preparative Temperature Rising Elution Fractionation method, where at least one preparative TREF fraction that elutes at 95° C. or greater has a gpcBR value greater than 0.05 and less than 5 as determined by gpcBR Branching Index by 3D-GPC, and where at least 5% of the ethylenic polymer elutes at a temperature of 95° C. or greater based upon the total weight of the ethylenic polymer.
摘要:
An ethylenic polymer comprising amyl groups from about 0.1 to about 2.0 units per 1000 carbon atoms as determined by Nuclear Magnetic Resonance and both a peak melting temperature, Tm, in ° C., and a heat of fusion, Hf, in J/g, as determined by DSC Crystallinity, where the numerical values of Tm and Hf correspond to the relationship Tm>(0.2143*Hf)+79.643. An ethylenic polymer comprising at least one preparative TREF fraction that elutes at 95° C. or greater using a Preparative Temperature Rising Elution Fractionation method, where at least one preparative TREF fraction that elutes at 95° C. or greater has a gpcBR value greater than 0.05 and less than 5 as determined by gpcBR Branching Index by 3D-GPC, and where at least 5% of the ethylenic polymer elutes at a temperature of 95° C. or greater based upon the total weight of the ethylenic polymer.
摘要:
The instant invention is a high-density polyethylene compositions, and method of making the same. The high-density polyethylene composition of the instant invention includes a first component, and a second component. The first component is a high molecular weight ethylene alpha-olefin copolymer having a density in the range of 0.915 to 0.940 g/cm3, and a melt index (I21) in the range of 0.5 to 10 g/10 minutes. The second component is a low molecular weight ethylene polymer having a density in the range of 0.965 to 0.980 g/cm3, and a melt index (I2) in the range of 50 to 1500 g/10 minutes. The high-density polyethylene composition has a melt index (I2) of at least 1, a density in the range of 0.950 to 0.960 g/cm3, and g′ of equal or greater than 1. The method of producing a high-density polyethylene composition include the following steps: (1) introducing ethylene, and an alpha-olefin comonomer into a first reactor; (2) copolymerizing the ethylene with the alpha-olefin comonomer in the first reactor thereby producing a first component, wherein the first component being a high molecular weight ethylene alpha-olefin copolymer having a density in the range of 0.915 to 0.940 g/cm3, and a melt index (I21) in the range of 0.5 to 10 g/10 minutes; (3) introducing the first component and additional ethylene into a second reactor; (4) polymerizing the additional ethylene in the second reactor thereby producing a second component, wherein the second component being a low molecular weight ethylene polymer having a density in the range of 0.965 to 0.980 g/cm3, and a melt index (I2) in the range of 50 to 1500 g/10 minutes; and (5) thereby producing the high-density polyethylene composition, wherein the high-density polyethylene composition having a melt index (I2) of at least 1, a density in the range of 0.950 to 0.960 g/cm3, and g′ of equal or greater than 1.
摘要:
The present invention pertains to a continuous process and polymerization system characterized by separate injection of catalyst and make-up feed, an ethylene interpolymer composition characterized as having broad molecular weight distribution (MWD) and optimized compositional uniformity, a process for making such a composition and a fabricated article made from such composition. The novel composition is characterized as having a melt flow ratio, I10/I2, from 8 to 30, a Mw/Mn of greater than 4 as determined by gel permeation chromatography, a melt index, I2, from 0.01 to 1000 grams/10 minutes, preferably greater that 0.1 to 10 grams/10 minutes, and a density less than 0.945 g/cm3. The novel composition exhibits good processibility and improved toughness properties, especially excellent film tear and impact resistance, and is particularly well-suited for use in applications such as high performance trash can liners and heavy duty shipping bags.