Manufacturing method of steel sheet for cans
    22.
    发明授权
    Manufacturing method of steel sheet for cans 失效
    罐头钢板的制造方法

    公开(公告)号:US08372221B2

    公开(公告)日:2013-02-12

    申请号:US13141129

    申请日:2009-12-22

    IPC分类号: C21D8/02

    摘要: A method provides a slab by continuous casting of a steel having a component composition of, in mass %, C: 0.005% or less, Mn: 0.05 to 0.5%, Al: 0.01 to 0.10%, N: 0.0010 to 0.0070%, B: 0.15×N to 0.75×N (0.15 to 0.75 in terms of B/N), and one or both of Nb: 4×C to 20×C (4 to 20 in terms of Nb/C) and Ti: 2×C to l0×C (2 to 10 in terms of Ti/C), and the balance of Fe and inevitable impurity elements; rough rolling the slab; finish rolling the rough-rolled slab wherein 5% or more and less than 50% of the total amount of rolling reduction in the finish rolling is hot-rolled at a temperature lower than the Ar3 transformation point; winding the hot-rolled steel sheet at a winding temperature of 640 to 750 ° C.; pickling the coiled steel sheet; cold rolling the pickled steel sheet at a rolling reduction rate of 88 to 96%; and annealing the cold-rolled steel sheet in a temperature range of higher than 400 ° C. to a temperature that is 20 ° C. lower than the recrystallization temperature.

    摘要翻译: 通过连续铸造具有质量%C:0.005%以下,Mn:0.05〜0.5%,Al:0.01〜0.10%,N:0.0010〜0.0070%,B :0.15×N〜0.75×N(B / N为0.15〜0.75),Nb:4×C〜20×C(Nb / C为4〜20),Ti:2× C至10×C(以Ti / C计2至10),余量为Fe和不可避免的杂质元素; 粗轧板坯; 将精轧中的压下量的5%以上且小于等于50%的粗轧板进行精轧,在低于Ar 3相变点的温度下进行热轧, 在640〜750℃的卷绕温度下卷绕热轧钢板。 酸洗卷板钢板; 以88%〜96%的压下率冷轧酸洗钢板; 并在高于400℃的温度范围内对冷轧钢板退火至比再结晶温度低20℃的温度。

    STEEL SHEET FOR CANS WITH EXCELLENT SURFACE PROPERTIES AFTER DRAWING AND IRONING AND METHOD FOR PRODUCING THE SAME
    23.
    发明申请
    STEEL SHEET FOR CANS WITH EXCELLENT SURFACE PROPERTIES AFTER DRAWING AND IRONING AND METHOD FOR PRODUCING THE SAME 有权
    用于绘制和熨烫后具有优异表面特性的罐的钢板及其制造方法

    公开(公告)号:US20120018055A1

    公开(公告)日:2012-01-26

    申请号:US13259589

    申请日:2010-03-25

    摘要: A component composition contains, by % by mass, 0.0016 to 0.01% of C, 0.05 to 0.60% of Mn, and 0.020 to 0.080% of Nb so that the C and Nb contents satisfy the expression, 0.4≦(Nb/C)×(12/93)≦2.5. In addition, the amount of Nb-based precipitates is 20 to 500 ppm by mass, the average grain diameter of the Nb-based precipitates is 10 to 100 nm, and the average crystal grain diameter of ferrite is 6 to 10 μm. Nb is added to ultra-low-carbon steel used as a base, and the amount and grain diameter of the Nb-based precipitates are controlled to optimize the pinning effect. Grain refinement of ferrite is achieved by specifying the Mn amount, thereby achieving softening and excellent resistance to surface roughness of steel.

    摘要翻译: 组分组成按质量计含有0.0016-0.01%的C,0.05-0.60%的Mn和0.020-0.080%的Nb,使得C和Nb含量满足表达式0.4≦̸(Nb / C) ×(12/93)≦̸ 2.5。 此外,Nb系析出物的含量为20〜500质量ppm,Nb系析出物的平均粒径为10〜100nm,铁素体的平均结晶粒径为6〜10μm。 将Nb添加到用作基底的超低碳钢中,并且控制Nb基沉淀物的量和晶粒直径以优化钉扎效果。 通过规定Mn量实现铁素体的晶粒细化,从而实现软化和优异的钢表面粗糙度。

    MANUFACTURING METHOD OF STEEL SHEET FOR CANS
    24.
    发明申请
    MANUFACTURING METHOD OF STEEL SHEET FOR CANS 失效
    CANS钢板制造方法

    公开(公告)号:US20110272066A1

    公开(公告)日:2011-11-10

    申请号:US13141129

    申请日:2009-12-22

    IPC分类号: C21D8/02

    摘要: A method provides a slab by continuous casting of a steel having a component composition of, in mass %, C: 0.005% or less, Mn: 0.05 to 0.5%, Al: 0.01 to 0.10%, N: 0.0010 to 0.0070%, B: 0.15×N to 0.75×N (0.15 to 0.75 in terms of B/N), and one or both of Nb: 4×C to 20×C (4 to 20 in terms of Nb/C) and Ti: 2×C to 10×C (2 to 10 in terms of Ti/C), and the balance of Fe and inevitable impurity elements; rough rolling the slab; finish rolling the rough-rolled slab wherein 5% or more and less than 50% of the total amount of rolling reduction in the finish rolling is hot-rolled at a temperature lower than the Ar3 transformation point; winding the hot-rolled steel sheet at a winding temperature of 640 to 750° C.; pickling the coiled steel sheet; cold rolling the pickled steel sheet at a rolling reduction rate of 88 to 96%; and annealing the cold-rolled steel sheet in a temperature range of higher than 400° C. to a temperature that is 20° C. lower than the recrystallization temperature.

    摘要翻译: 通过连续铸造具有质量%C:0.005%以下,Mn:0.05〜0.5%,Al:0.01〜0.10%,N:0.0010〜0.0070%,B :0.15×N〜0.75×N(B / N为0.15〜0.75),Nb:4×C〜20×C(Nb / C为4〜20),Ti:2× C至10×C(以Ti / C计为2至10),余量为Fe和不可避免的杂质元素; 粗轧板坯; 将精轧中的压下量的5%以上且小于等于50%的粗轧板进行精轧,在低于Ar 3相变点的温度下进行热轧, 在640〜750℃的卷绕温度下卷绕热轧钢板。 酸洗卷板钢板; 以88%〜96%的压下率冷轧酸洗钢板; 并在高于400℃的温度范围内对冷轧钢板退火至比再结晶温度低20℃的温度。

    IRONING METHOD AND IRONING APPARATUS
    25.
    发明申请
    IRONING METHOD AND IRONING APPARATUS 有权
    熨烫方法和熨烫装置

    公开(公告)号:US20110114128A1

    公开(公告)日:2011-05-19

    申请号:US12934167

    申请日:2009-03-19

    IPC分类号: A47L5/14 B08B5/04

    CPC分类号: B21D22/28 B21D22/201

    摘要: An ironing apparatus includes an ironing die and an ironing punch, an injection port for injecting gas or liquid to the metal plate at a high pressure to remove substance adhered to the metal plate therefrom, a suction port for sucking the adhered substance removed from the metal plate, and a protrusion mount portion with a protrusion for preventing dispersion of the gas or the liquid. An ironing method for ironing the metal plate having the single surface or both surfaces coated with the organic resin film includes the steps of injecting the gas or the liquid from the injection port to the metal plate at the high pressure to remove the adhered substance from the metal plate, and sucking and collecting the adhered substance removed from the metal plate from the suction port. The adhered substance such as the hair may be removed by the aforementioned invention.

    摘要翻译: 熨烫装置包括熨烫模具和熨烫冲头,用于将气体或液体高压注入金属板的注入口,以除去附着在金属板上的物质,用于吸附从金属中除去的附着物质的吸入口 板和具有突起的突起安装部分,用于防止气体或液体的分散。 用于熨烫具有涂覆有机树脂膜的单面或两面的金属板的熨烫方法包括以下步骤:将来自注射口的气体或液体以高压注入金属板,以从 金属板,并且从吸入口吸收和收集从金属板除去的粘附物质。 通过上述发明可以除去毛发等附着物。

    Ironing method and ironing apparatus
    26.
    发明授权
    Ironing method and ironing apparatus 有权
    熨烫方法和熨烫设备

    公开(公告)号:US09011609B2

    公开(公告)日:2015-04-21

    申请号:US12934167

    申请日:2009-03-19

    IPC分类号: B21D22/20 B21D22/28

    CPC分类号: B21D22/28 B21D22/201

    摘要: An ironing apparatus includes an ironing die and an ironing punch, an injection port for injecting gas or liquid to the metal plate at a high pressure to remove substance adhered to the metal plate therefrom, a suction port for sucking the adhered substance removed from the metal plate, and a protrusion mount portion with a protrusion for preventing dispersion of the gas or the liquid. An ironing method for ironing the metal plate having the single surface or both surfaces coated with the organic resin film includes the steps of injecting the gas or the liquid from the injection port to the metal plate at the high pressure to remove the adhered substance from the metal plate, and sucking and collecting the adhered substance removed from the metal plate from the suction port. The adhered substance such as the hair may be removed by the aforementioned invention.

    摘要翻译: 一种熨烫装置,包括熨烫模具和熨烫冲头,用于将气体或液体高压注入金属板的注入口,以除去附着在金属板上的物质,用于吸附从金属中除去的粘附物质的吸入口 板和具有突起的突起安装部分,用于防止气体或液体的分散。 用于熨烫具有涂覆有机树脂膜的单面或两面的金属板的熨烫方法包括以下步骤:将来自注射口的气体或液体以高压注入金属板,以从 金属板,并且从吸入口吸收和收集从金属板除去的粘附物质。 通过上述发明可以除去毛发等附着物。

    METHOD FOR DESIGNING MATERIAL TO BE SUBJECTED TO CYLINDER FORMING AND PRODUCT FORMED BY PERFORMING CYLINDER FORMING
    30.
    发明申请
    METHOD FOR DESIGNING MATERIAL TO BE SUBJECTED TO CYLINDER FORMING AND PRODUCT FORMED BY PERFORMING CYLINDER FORMING 审中-公开
    将材料设计成圆筒形成的方法和通过执行气缸成型形成的产品

    公开(公告)号:US20130327116A1

    公开(公告)日:2013-12-12

    申请号:US13994103

    申请日:2011-12-13

    IPC分类号: B21C37/06

    摘要: An object of the present invention is to provide a method for designing a metal material having mechanical properties with which a specified spring back angle can be achieved after any one of metal materials having a wide variety of mechanical properties and thicknesses has been formed by performing cylinder forming and a product formed by using the method. A method for designing a material to be subjected to cylinder forming, the method including, in the design of a metal material to be subjected to cylinder forming in which the metal material is formed by performing bending forming, calculating the yield strength YP, the Young's modulus E and the thickness t of the metal material so that a spring back angle Δθ becomes a specified value when cylinder forming is performed under conditions of a radius of curvature of bending r of 5 mm or more and a bending angle θ of 90 degrees or more and 180 degrees or less and designing the metal material so that the metal material has the calculated yield strength YP and Young's modulus E.