Cordierite ceramic filter
    22.
    发明授权
    Cordierite ceramic filter 失效
    堇青石陶瓷过滤器

    公开(公告)号:US06261982B1

    公开(公告)日:2001-07-17

    申请号:US09437443

    申请日:1999-11-10

    IPC分类号: C04B35195

    摘要: A ceramic filter comprising at least 50 mass % of a cordierite aggregate having a particle size of at least 74 &mgr;m and a binder, wherein said binder comprises at least 10 mass % of a fine powder of cordierite having a particle size of less than 74 &mgr;m and &bgr;-spodumene, and the mass ratio of said &bgr;-spodumene to said fine powder of cordierite is from 0.6 to 2.5, and wherein said ceramic filter has a pressure loss coefficient m′ of at least 30×10−8 cm2 as represented by the following formula and as calculated with respect to pores having diameters corresponding to at least {fraction (1/10)} of the volume-based median pore diameter: m′=(Vp/Sp)2×(&rgr;) wherein Vp (cm3/g) is a cumulative pore specific volume, Sp (cm2/g) is a cumulative pore specific surface area, and &rgr; is a cumulative porosity.

    摘要翻译: 一种陶瓷过滤器,其包含至少50质量%的粒径为至少74μm的堇青石骨料和粘合剂,其中所述粘合剂包含至少10质量%的粒径小于74μm的堇青石细粉末 和β-锂辉石,并且所述β-锂辉石与所述堇青石细粉末的质量比为0.6至2.5,并且其中所述陶瓷过滤器具有至少30×10 -8 cm 2的压力损失系数m',如以下所示 并且相对于直径对应于基于体积的中值孔径的至少{部分(1/10)}的孔计算的其中Vp(cm 3 / g)是累积孔比体积,Sp(cm 2 / g )是累积孔比表面积,rho是累积孔隙率。

    Laminated glass structure
    25.
    发明授权
    Laminated glass structure 失效
    层压玻璃结构

    公开(公告)号:US5346770A

    公开(公告)日:1994-09-13

    申请号:US135186

    申请日:1993-10-12

    IPC分类号: B32B17/10 C03C17/38 B32B15/00

    摘要: A laminated glass structure is provided containing at least one glass sheet, a plastic layer provided at the bonding surface of the glass sheet, and a functioning layer having single-or multi-layered films between the bonding surfaces of the glass sheet and the plastic layer, with the functioning layer having a controlling layer in contact with the plastic layer, which contains as the major component an oxide including Cr and at least one of Ti, Zn, Sn, Ni, Zr, Al, Si, Mg and Fe, and wherein the controlling layer has an atomic ratio of Cr to atoms other than oxygen of 60% or lower, and the film thickness of the controlling layer is 10 .ANG. to 500 .ANG..

    摘要翻译: 提供一种夹层玻璃结构,其包含至少一个玻璃板,设置在玻璃板的接合表面处的塑料层和在玻璃板和塑料层的接合表面之间具有单层或多层膜的功能层 功能层具有与塑料层接触的控制层,其包含作为主要成分的包含Cr和Ti,Zn,Sn,Ni,Zr,Al,Si,Mg和Fe中的至少一种的氧化物,以及 其中所述控制层的Cr与氧以外的原子的原子比为60%以下,所述控制层的膜厚为10〜500埃。

    Image synthesizing device, coding device, program, and recording medium
    26.
    发明授权
    Image synthesizing device, coding device, program, and recording medium 有权
    图像合成装置,编码装置,程序和记录介质

    公开(公告)号:US09001272B2

    公开(公告)日:2015-04-07

    申请号:US13357862

    申请日:2012-01-25

    摘要: In order to prevent obstruction of a view of a subtitle due to synthesis of the subtitle onto an object area such as a person and display of the synthesized subtitle, an image synthesizing device includes: an image synthesizing unit which synthesizes a graphics object onto an image; and a display area detecting unit which outputs a display position of an area having the lowest spatial frequency; and a drawing control unit which causes the graphics object to be drawn at the display position.

    摘要翻译: 为了防止由于将副标题合成到诸如人物的对象区域和合成字幕的显示上的副标题的视图,图像合成装置包括:图像合成单元,其将图形对象合成到图像上 ; 以及显示区域检测单元,其输出具有最低空间频率的区域的显示位置; 以及使图形对象在显示位置被绘制的绘图控制单元。

    Automotive lamp extension molding
    27.
    发明授权
    Automotive lamp extension molding 有权
    汽车灯延长成型

    公开(公告)号:US08895655B2

    公开(公告)日:2014-11-25

    申请号:US13884025

    申请日:2011-11-22

    摘要: [Problem to be Solved] The present invention has an object to provide an automotive lamp extension molding comprising a resin composition having a low specific gravity, being excellent in the balance of heat resistance and fluidity, and being excellent in gloss and brightness feeling of the surface of the molded article. [Solution] The automotive lamp extension molding according to the present invention comprises a resin composition comprising 50 to 95 mass % of a polyphenylene ether (A), and having a specific gravity in the range of 1.00 to 1.12. The reduced viscosity (measured at 30° C. using a chloroform solvent) of the (A) component is preferably 0.25 to 0.45 dl/g, and more preferably 0.25 to 0.38 dl/g.

    摘要翻译: [待解决的问题]本发明的目的是提供一种汽车灯延伸成型体,其包含具有低比重的树脂组合物,耐热性和流动性的平衡优异,并且具有优异的光泽度和亮度感 模制品的表面。 [解决方案]本发明的汽车用灯具延伸成型体包含含有50〜95质量%的聚苯醚(A),比重为1.00〜1.12的树脂组合物。 (A)成分的比浓粘度(在30℃下使用氯仿溶剂测定)优选为0.25〜0.45dl / g,更优选为0.25〜0.38dl / g。

    AUTOMOTIVE LAMP EXTENSION MOLDING
    29.
    发明申请
    AUTOMOTIVE LAMP EXTENSION MOLDING 有权
    汽车灯延伸成型

    公开(公告)号:US20130267641A1

    公开(公告)日:2013-10-10

    申请号:US13884025

    申请日:2011-11-22

    IPC分类号: C08L71/12 C08K5/13

    摘要: [Problem to be Solved] The present invention has an object to provide an automotive lamp extension molding comprising a resin composition having a low specific gravity, being excellent in the balance of heat resistance and fluidity, and being excellent in gloss and brightness feeling of the surface of the molded article.[Solution] The automotive lamp extension molding according to the present invention comprises a resin composition comprising 50 to 95 mass % of a polyphenylene ether (A), and having a specific gravity in the range of 1.00 to 1.12. The reduced viscosity (measured at 30° C. using a chloroform solvent) of the (A) component is preferably 0.25 to 0.45 dl/g, and more preferably 0.25 to 0.38 dl/g.

    摘要翻译: [待解决的问题]本发明的目的是提供一种汽车灯延伸成型体,其包含具有低比重的树脂组合物,耐热性和流动性的平衡优异,并且具有优异的光泽度和亮度感 模制品的表面。 [解决方案]本发明的汽车用灯具延伸成型体包含含有50〜95质量%的聚苯醚(A),比重为1.00〜1.12的树脂组合物。 (A)成分的比浓粘度(在30℃下使用氯仿溶剂测定)优选为0.25〜0.45dl / g,更优选为0.25〜0.38dl / g。

    Light diffusion plate and its production process
    30.
    发明授权
    Light diffusion plate and its production process 失效
    光扩散板及其生产工艺

    公开(公告)号:US07727626B2

    公开(公告)日:2010-06-01

    申请号:US11949801

    申请日:2007-12-04

    摘要: A light diffusion plate has a substrate and a light diffusion layer formed on the substrate. The light diffusion layer is composed of at least two layers: a first light diffusion layer containing a first matrix and a first light diffusion agent having a refractive index difference Δn1 of 0.04≦Δn1≦0.2 with the first matrix, and a second light diffusion layer containing a second matrix and a second light diffusion agent having a refractive index difference Δn2 of 0.005≦Δn2≦0.01 with the second matrix. The volume fraction of the first light diffusion agent in the first light diffusion layer is less than 40%, the volume fraction of the second light diffusion agent in the second light diffusion layer is at least 40% and the total thickness of the light diffusion layers is from 5 to 200 μm after curing.

    摘要翻译: 光扩散板具有形成在基板上的基板和光扩散层。 光扩散层由至少两层构成:包含第一基质的第一光扩散层和折射率差为Dgr的第一光扩散剂,n1为0.04≦̸&Dgr; n1≦̸ 0.2与第一基质,以及 第二光扩散层,其含有第二基体和第二光扩散剂,所述第二光扩散剂的折射率差为&Dgr; n2为0.005≦̸&Dgr; n2≦̸ 0.01与第二矩阵。 第一光扩散层中的第一光扩散剂的体积分率小于40%,第二光扩散层中第二光扩散剂的体积分数为40%以上,光扩散层的总厚度 固化后为5〜200μm。