Aluminum casting alloy for high strength/high temperature applications
    21.
    发明授权
    Aluminum casting alloy for high strength/high temperature applications 失效
    铝合金高强度/高温应用

    公开(公告)号:US5120372A

    公开(公告)日:1992-06-09

    申请号:US610647

    申请日:1990-11-08

    Abstract: An aluminum casting alloy consisting of, by weight, of 7.0-13.0% copper, 0.4-1.2% manganese, 0.21-40% vanadium, 0.31-0.70% zirconium; impurities limited to: less than to 0.6% Si, less than 0.8% Fe, less than 0.2% zinc, less than 0.1% Mn, less than 0.2% Ni, and the remainder being essentially aluminum. There is an absence of titanium, cobalt, molybdenum, tungsten, chromium, boron, tantalum, and niobium. The alloy has, at room temperature, a UTS of about 61 ksi, a YS of about 49 ksi, a tensile elongation of about 6%, and tensile modulus elasticity of about 11.5 MSI, a compressive yield strength of about 53 ksi, a compressive modulus of elasticity of about 18 MSi; high temperature physical properties at 500.degree. F., after 1000 hours exposure to 500.degree. F., comprise a tensile strength of 33 ksi or greater, a tensile yield strength of 23 ksi or greater, a tensile elongation of about 9%, and tensile modulus of elasticity of 10 msi. The alloy is fabricated by a) squeeze casting an aluminum alloy melt of such character; (b) extracting the solidified casting from the die and heat treating the casting to dissolve all alloying elements (i.e., 995.degree.-1018.degree. F. for 7-20 hours); and (c) aging the solution treated casting to achieve improved strength characteristics (i.e., in the range of 340.degree.-400.degree. F. for 5-20 hours).

    Aluminum casting alloy for high strength/high temperature applications
    22.
    发明授权
    Aluminum casting alloy for high strength/high temperature applications 失效
    铝铸造合金,用于高强度/高温应用

    公开(公告)号:US5115770A

    公开(公告)日:1992-05-26

    申请号:US802594

    申请日:1991-12-05

    Abstract: An aluminum casting alloy consisting of, by weight, of 7.0-13.0% copper, 0.4-1.2% manganese, 0.21-0.40% vanadium, 0.31-0.70% zirconium; impurities limited to: less than to 0.6% Si, less than 0.8% Fe, less than 0.2% zinc, less than 0.1% Mn, less than 0.2% Ni, and the remainder being essentially aluminum. There is an absence of titanium, cobalt, molybdenum, tungsten, chromium, boron, tantalum, and niobium. The alloy has, at room temperature, a UTS of about 61 ksi, a YS of about 49 ksi, a tensile elongation of about 6%, and tensile modulus elasticity of about 11.5 MSi, a compressive yield strength of about 53 ksi, a compressive modulus of elasticity of about 18 MSi; high temperature physical properties at 500.degree. F., after 1000 hours exposure to 500.degree. F., comprise a tensile strength of 33 ksi or greater, a tensile yield strength of 23 ksi or greater, a tensile elongation of about 9%, and tensile modulus of elasticity of 10 msi. The alloy is fabricated by a) squeeze casting an aluminum alloy melt of such character; (b) extracting the solidified casting from the die and heat treating the casting to dissolve all alloying elements (i.e., 995.degree.-1018.degree. F. for 7-20 hours); and (c) aging the solution treated casting to achieve improved strength characteristics (i.e., in the range of 340.degree.-400.degree. F. for 5-20 hours).

    Abstract translation: 一种铝铸造合金,其重量为7.0-13.0%的铜,0.4-1.2%的锰,0.21-0.40%的钒,0.31-0.70%的锆; 杂质限于:小于0.6%的Si,小于0.8%的Fe,小于0.2%的锌,小于0.1%的Mn,小于0.2%的Ni,余量基本上是铝。 没有钛,钴,钼,钨,铬,硼,钽和铌。 该合金在室温下具有约61ksi的UTS,约49ksi的YS,约6%的拉伸伸长率和约11.5Mii的拉伸模量弹性,约53ksi的压缩屈服强度,压缩屈服强度 弹性模量约18 MSi; 在500°F下耐高温物理性能,在500°F暴露1000小时后,拉伸强度为33ksi或更大,拉伸屈服强度为23ksi或更大,拉伸伸长率约为9% 弹性模量为10 msi。 该合金是通过以下方法制造的:a)挤压铸造具有这种特性的铝合金熔体; (b)从模具中提取凝固的铸件并对铸件进行热处理以溶解所有合金元素(即995°-1018°F 7-20小时); 和(c)使溶液处理的铸件老化以获得改进的强度特性(即在340-400°F的范围内5-20小时)。

    Cu-base sintered alloy
    23.
    发明授权
    Cu-base sintered alloy 失效
    铜基烧结合金

    公开(公告)号:US5114468A

    公开(公告)日:1992-05-19

    申请号:US474748

    申请日:1990-03-23

    Abstract: The present invention relates to a Cu-based sintered alloy which has a composition containing: Zn: 10-40%; Al: 0.3%-6% oxygen: 0.03-1%; any one selected, as an additional element from the group including at least one of Fe, Ni and Co: 0.1-5%, Mn: 0.1-5%, Si: 0.1-3%, and at least one of W and Mo: 0.1-3%; and the remainder including Cu and inevitable impurities. The alloy is superior in wear resistance particularly in air at temperatures ranging from the ordinary temperature to 400.degree. C., has high strength and high toughness, and further excels in the uniform temporal change characteristics with associated members, as evaluated by its friction coefficient. The invention relates also to parts for automotive equipment made of this Cu-base sintered alloy, such as synchronizer rings for transmission, valveguides for engines, bearings for turbo-chargers and so forth.

    Abstract translation: PCT No.PCT / JP89 / 01098 Sec。 371 1990年3月23日 102(e)1990年3月23日PCT PCT 1989年10月26日PCT公布。 出版物WO90 / 04657 日期:1990年5月3日。本发明涉及一种Cu基烧结合金,其组成为:Zn:10-40% Al:0.3%-6%氧气:0.03-1%; 选自Fe,Ni和Co中的至少一种:0.1-5%,Mn:0.1-5%,Si:0.1-3%,以及W和Mo中的至少一种: 0.1-3%; 余量包括Cu和不可避免的杂质。 该合金在常温至400℃的温度范围内,特别是在空气中具有优异的耐磨性,具有高强度和高韧性,并且通过其摩擦系数进行评估,进一步优于相关构件的均匀时间变化特性。 本发明还涉及由该Cu基烧结合金制成的汽车设备的部件,例如用于变速器的同步环,用于发动机的阀导向器,用于涡轮增压器的轴承等。

    Structure of a shoe for a swash plate type compressor
    25.
    发明授权
    Structure of a shoe for a swash plate type compressor 失效
    用于斜盘式压缩机的鞋的结构

    公开(公告)号:US4329913A

    公开(公告)日:1982-05-18

    申请号:US55469

    申请日:1979-07-06

    CPC classification number: F04B27/0882 F05C2201/0475

    Abstract: A round plate shape shoe for incorporation into a swash plate type compressor as an operative engaging element intervened between a rotatable swash plate and a reciprocal piston is structured to have a first flattened face slidably contacting the swash plate and a second face opposite to the first flattened face, the second face being formed with a recess for receiving a ball bearing, which has a spherical shape portion complementary with a part of the ball bearing and a round bore portion with a bottom. The spherical shape portion of the recess is concentric with the round bore portion.

    Abstract translation: 一种用于结合到旋转斜盘式压缩机中的圆板形鞋作为介于可旋转斜盘和往复活塞之间的可操作接合元件构造成具有可滑动地接触斜盘的第一平坦表面和与第一扁平 所述第二面形成有用于接收球轴承的凹部,所述球轴承具有与所述球轴承的一部分互补的球形部分和具有底部的圆孔部分。 凹槽的球形部分与圆孔部分同心。