Abstract:
Membrane comprising a block copolymer comprising polyarylene ether blocks and polyalkylene oxide blocks, wherein said polyalkylene oxide blocks comprise at least one polyethylene oxide segment and at least one segment of at least one polyalkylene oxide that is different from polyethylene oxide.
Abstract:
A polyarylene ether sulfone comprising in polymerized form A) isosorbide, isomannide, isoidide or a mixture thereof and B) at least one nonsulfonated dihalodiaryl! sulfone (compound B) and C) at least one sulfonated dihalodiaryl sulfone (compound C), a process for its preparation and its use in the preparation of coatings, films, fibers, foams, membranes or molded articles.
Abstract:
A polyarylene ether copolymer comprising i) at least one block comprising in polymerized form A) isosorbide, isomannide, isoidide or a mixture thereof and B) at least one unit comprising at least one difunctional compound comprising at least one dichlorodiaryl sulfone, a dichlorodiaryl ketone or a mixture thereof and ii) at least one block comprising in polymerized form C) at least one polyalkylene oxide, a process for its preparation and its use in the preparation of coatings, films, fibers, foams, membranes or molded articles.
Abstract:
The present invention relates to a thermoplastic molding compound comprising a polyalkylene terephthalate and a polyimide, wherein the molding compound has a single glass transition temperature in DSC measurement. The present invention further relates to the use thereof and to fibers, films and shaped bodies produced from the molding compound.
Abstract:
The invention relates to an elastic membrane comprising an elastomer having an elongation at break of greater than 150% measured according to DIN 53504, wherein the thermoplastic elastomer (P1) comprises a polyurethane elastomer based on the following components: 11 % to 79% by weight of a mixture of at least one diol (D1) and at least one isocyanate (I1), 21% to 89% by weight of at least one compound (C1) having at least two isocyanate-reactive groups.
Abstract:
Described herein is a method of using copolyamides c) produced by polymerization of components A′) 15% to 84% by weight of at least one lactam, and B′) 16% to 85% by weight of a monomer mixture (M) including components B1′) at least one C32-C40-dimer acid and B2′) at least one C4-C12-diamine, where the percentages by weight of the components A′) and B′) are in each case based on the sum of the percentages by weight of the components A′) and B′), the method including using the copolyamides c) to increase an impact strength and/or breaking elongation of molded articles made of molding materials including thermoplastic polyamides, which are different from copolyamides c).
Abstract:
Polyethers (A), whose main chain essentially consists of repeating units of the formulae (1) and (2) in alternating order, are useful as an additive to a porous polymer membrane, or as the main polymer constituent of a porous polymer membrane, for stabilizing said membrane against detrimental effects of oxidizing agents and/or for improving the stability of a filtration module comprising said membrane against detrimental effects of oxidizing agents.
Abstract:
Block copolymer comprising polyarylene ether blocks and polyalkylene oxide blocks, wherein said block copolymer comprises at least two polyalkylene oxide blocks that are endcapped with different endcapping groups.
Abstract:
The present invention relates to a process for the production of a polyaryl ether sulfone polymer (P), comprising the following steps: (I) provision of a solution (PL) which comprises the polyaryl ether sulfone polymer (P) and comprises an aprotic polar solvent (L), (II) separation of the solution (PL) into droplets, (III) transfer of the droplets into a precipitation bath (F) which comprises water, with the result that the polyaryl ether sulfone polymer (P) is obtained in the form of particles, and (IV) isolation of the polyaryl ether sulfone polymer (P) where the temperature of the solution (PL) in step (II) is in the range from 50 to
Abstract:
The present invention is directed to ultrafiltration membranes comprising a membrane substrate layer (S) based on a sulfonated polyaryleneethersulfone polymer and to a method for their preparation. Furthermore, the present invention is directed to ultrafiltration processes making use of said membrane.