摘要:
Thermoplastic molding composition based on thermoplastic polyesters (a.sub.1), graft polymers incorporating acrylate rubbers as grafting base (a.sub.2), copolymers of aromatic vinyl monomers and acrylonitrile or methacrylonitrile (a.sub.3) and glass fibers (B) have particularly good mechanical properties if the (meth)acrylonitrile content in component (a.sub.3), based on the total weight of (a.sub.3), is less than the (meth)acrylonitrile content of component (a.sub.22).
摘要:
The flameproofing agent content of molding compositions containing polyesters (a.sub.1), acrylate graft polymers (a.sub.2), styrene/acrylonitrile copolymers (a.sub.3) and glass fibers can be reduced without affecting the flame resistance by adding finely divided PTFE.
摘要:
A thermoplastic material containing, based in each case on the molding material comprising A and B,A from 30 to 80% be weight of one or more polycarbonates andB from 70 to 20% by weight of a blend of two different components B.sub.1 and B.sub.2, each of which consists of one or more graft copolymers b.sub.11 and b.sub.21 and each of which consists of one or more copolymers (hard matrix) b.sub.12 and b.sub.22, respectively, the graft copolymer b.sub.11 being prepared in emulsion and the graft copolymer b.sub.21 being prepared by another method.
摘要:
Wholly aromatic thermotropic polyesters are based on(A) 30 to 60 mol % of 4-hydroxybenzoic acid,(B) 20 to 35 mol % of terephthalic acid and(C) 20 to 35 mol % of a mixture of(C.sub.1) trimethylhydroquinone and(C.sub.2) resorcinolthe molar ratio of C.sub.1 :C.sub.2 being within the range from 0.4:1 to 0.7:1 and the molar ratio of B:C within the range from 0.9:1 to 1.1:1.
摘要:
Wholly aromatic thermotropic polyesters are based on(A) from 25 to 60 mol % of a mixture of(A.sub.1) 4-hydroxybenzoic acid and(A.sub.2) 3-hydroxybenzoic acid, 4-aminobenzoic acid and/or 3-aminobenzoic acid or their chlorine, bromine, C.sub.1 -C.sub.8 -alkyl or C.sub.1 -C.sub.8 -alkoxy derivatives substituted in the nucleus, the molar ratio of A.sub.1 to A.sub.2 being from 5:1 to 41:1,(B) from 20 to 37.5 mol % of a mixture of(B.sub.1) terephthalic acid and(B.sub.2) isophthalic acid, the molar ratio of B.sub.1 to B.sub.2 being from 1.04:1 to 19:1, and(C) from 20 to 37.5 mol % of a mixture of(C.sub.1) hydroquinone and(C.sub.2) 4,4'-dihydroxydiphenyl, the molar ratio of C.sub.1 to C.sub.2 being from 0.1:1 to 2.67:1 and the molar ratio of B to C being from 0.9:1 to 1.1:1.
摘要:
A process for the preparation of modified polyphenylene ether resins by grafting fumaric acid, preferably at from 270.degree. to 350.degree. C., onto polyphenylene ethers which are mixed with vinylaromatic polymers, and modified polyphenylene ether resins consisting of from 4.95 to 95 parts by weight of polyphenylene ether, from 95 to 4.95 parts by weight of vinylaromatic polymer and from 0.05 to 10 parts by weight of grafted fumaric acid.
摘要:
Fully aromatic themotropic polyesters are based on(A) from 30 to 60 mol % of 4-hydroxybenzoic acid,(B) from 20 to 35 mol % of a mixture of(B.sub.1) terephthalic acid and(B.sub.2) isophthalic acid, the molar ratio of B.sub.1 to B.sub.2 being from 1.04:1 to 19:1, and(C) from 20 to 35 mol % of a mixture of(C.sub.1) hydroquinone,(C.sub.2) 4,4'-dihydroxydiphenyl and(C.sub.3) from 0 to 5 mol % of a dihydroxy compound of the general formula I ##STR1## where R and R' are each C.sub.1 -C.sub.4 -alkyl, halogen or aryl, n is 1, 2 or 3 and m is 0 or 1, the molar ratio of C.sub.1 to C.sub.2 being from 0.1:1 to 2.67:1 and the molar ratio of B to C being from 0.9:1 to 1.1:1.
摘要:
A process for the preparation of finely divided polyolefin molding materials from 100 parts by weight of a polyolefin and from 0.01 to 30 parts by weight of an electrically conductive additive, with or without other additives, wherein the mixture of the finely divided polyolefin particles and the electrically conductive additives is brought to the crystallite melting point of the polyolefin by the heating effect of the mixing action, and is then brought to a temperature which is from 3.degree. to 40.degree. C. above the said crystallite melting point while being subjected to a defined mixing intensity, after which the mixture is either cooled within 120 seconds or is directly compression-molded.
摘要:
A process for the preparation of finely divided polyolefin molding materials from 100 parts by weight of polyolefin and from 1 to 30 parts by weight of a conductive carbon black, with or without other additives, wherein the mixture of polyolefin powder and carbon black is compounded, in a first stage, until the crystallite melting point of the polyolefin is reached, and is then brought, in a second stage, to a temperature which is from 3.degree. to 40.degree. C. above the said crystallite melting point, after which the mixture is discharged from the mixer within from 0.5 to 30 seconds and is cooled within 120 seconds.
摘要:
Branched block copolymers of from 60 to 95 percent by weight of a monovinyl-aromatic compound and from 40 to 5 percent by weight of a conjugated diene. The copolymers have a structure of the general formula(A.sup.1 -B.fwdarw.A.sup.2).sub.n --X--(A.sup.2 .rarw.B).sub.mwhere the A's are non-elastomeric polymer segments based on the monovinyl-aromatic compound, the B's are elastomeric polymer segments based on the conjugated diene, X is the radical of an at least trifunctional coupling agent and n and m are numbers. The copolymers may be used for the manufacture of highly transparent impact-resistant shaped articles, especially packaging materials.