摘要:
An olefin thermoplastic elastomer composition comprises a crystalline polyolefin resin (A) and an ethylene/&agr;-olefin/nonconjugated polyene copolymer rubber (B), and optionally a softener (C) and/or an inorganic filler (D), in a specific ratio. The copolymer rubber (B) is prepared by the use of a metallocene catalyst and comprises ethylene, an &agr;-olefin of 3 to 20 carbon atoms and a nonconjugated polyene. This composition ca provide molded products of more excellent tensile strength, elongation at break, elastomeric properties (elongation set, permanent compression set, etc.), heat resistance and low-temperature properties than the conventional non-crosslinked olefin thermoplastic elastomers, even if the composition is in the non-crosslinked form. The composition in the partially or completely crosslinked form can provided molded products of more excellent low-temperature properties, tensile strength, elongation at break and elastomeric properties than the conventional vulcanized rubbers.
摘要:
The present invention is intended to obtain a viscosity modifier for a lubricating oil, by the use of which a lubricating oil composition of excellent low-temperature properties can be obtained, and to obtain a lubricating oil composition of excellent low-temperature properties containing the viscosity modifier. The viscosity modifier for a lubricating oil comprises an ethylene/propylene copolymer (A) having the properties: the density is in the range of 857 to 882 kg/m3, Mw is in the range of 80,000 to 400,000, Mw/Mn is not more than 2.3, and the density (D (kg/m3)) and the melting point (Tm (° C.)) satisfy the relation Tm≦1.247×D−1037; or comprises an ethylene/propylene copolymer (B) having the properties: the ethylene content is in the range of 70 to 79 wt %, Mw is not less than 80,000 and less than 250,000, Mw/Mn is not more than 2.3, Tm is in the range of 15 to 60° C., and the ethylene content (E (wt %)) and the melting point (Tm (° C.)) satisfy the relation 3.44×E−206≧Tm; or comprises an ethylene/propylene copolymer (C) having the properties: the ethylene content is in the range of 70 to 79 wt %, Mw is in the range of 250,000 to 400,000, Mw/Mn is not more than 2.3, Tm is in the range of 15 to 60° C., and the ethylene content (E (wt %)) and the melting point (Tm (° C.)) satisfy the relation 3.44×E−204≧Tm. The lubricating oil composition comprises the ethylene/propylene copolymer (A) (B) or (C), a lubricating oil base (D), and if necessary, a pour point depressant.
摘要:
There is provided a composition comprising a higher a-olefin copolymer (1) obtained by copolymerization in the presence of a specific olefin polymerization catalyst of a specific higher .alpha.-olefin, a specific .alpha., .omega.-diene of the formula (I) and a specific non-conjugated diene of the formula (II), and a rubber (2) selected from the group consisting of a diene rubber, an ethylene/a-olefin copolymer, a nitrile rubber and a hydrogenated nitrile rubber. The composition is excellent in workability strength characteristics, weatherability, ozone resistance and dynamic fatigue resistance, as well as excellent in adhesive properties to fiber and in vibration-insulating properties and damping properties.
摘要:
Disclosed are vulcanized rubber articles of foamed type and non-foamed type which are prepared by vulcanizing a vulcanizable and foamable (or a vulcanizable) molded product made of a chlorinated ethylene/.alpha.-olefin copolymer rubber, chlorinated polyethylene or chlorosulfonated polyethylene, said vulcanizable and foamable (or vulcanizable) molded product having been surface-treated with a coating solution containing at least one compound selected from alkylammonium halide, alkylphosphonium halide, amine having an acid dissociation constant (pKa) of not less than 10 and amine salt having an acid dissociation constant (pKa) of not less than 10. Also disclosed are processes for the preparation of the vulcanized rubber articles of foamed type and non-foamed type.
摘要:
PCM 24 channel digital voice information received from an incoming trunk are sequentially stored in a speech data memory device for respective channels through an input buffer memory device. The addressed content of the speech data memory device is read out by a control signal which has been stored in a control memory device and adapted to designate an address of the speech data memory device from which information is to be read out, and the read out information is sent to an outgoing trunk through an output buffer memory device thereby operating channel translation. The channel assigned to the outgoing trunk is different from that assigned to the incoming trunk. The speech data memory device, the control memory device and the program memory device are constituted by one memory means and the exchange of signals between the memory means and the input/output buffer memory devices as well as an arithmetic operation unit is effected by a programmed control of a program memory device.
摘要:
A lubricating oil composition for a power transmission system, which is excellent in both of low-temperature viscosity property and shear stability, is provided. The viscosity modifier of a lubricating oil for a power transmission system according to the present invention comprises an ethylene/α-olefin copolymer (B) having the properties: (B1) an ethylene content in the range of 70 to 85% by mol, (B2) an intrinsic viscosity [η] in the range of 0.2 to 1.0 dl/g, (B3) Mw/Mn not more than 2.4, and (B4) a melting point, as measured by DSC, not higher than 60° C., or no melting point observed.
摘要:
Disclosed is a thermoplastic elastomer composition containing 10-60 parts by weight of a non-crosslinkable crystalline polyolefin resin (A), 1-30 parts by weight of a specific propylene 1-butene random copolymer (B) and 89-10 parts by weight of an ethylene α-olefin non-conjugated polyene copolymer rubber (C) which is composed of ethylene, an α-olefin having 3-20 carbon atoms and a non-conjugated polyene, in such amounts that the total of the components (A), (B) and (C) is 100 parts by weight. The thermoplastic elastomer composition is dynamically crosslinked by an extruder. This thermoplastic elastomer is excellent in moldability and economic efficiency, and enables to obtain a molded body exhibiting sufficient adhesion strength to a vulcanized rubber or thermoplastic elastomer without the intermediation of an adhesive layer, as well as a lightweight molded body having sufficient hardness and rubber elasticity.
摘要:
The present invention is a polyolefin polymer containing vinyl groups at both ends thereof, and a composition and a molded product containing the polymer, wherein the polymer contains a constitutional unit derived from at least one selected from the group consisting of ethylene (a), an α-olefin (b) having 3 to 20 carbon atoms, and a cyclic olefin (c), and (1) a ratio of terminal vinylation is 70% or more relative to all of both ends of molecular chains, and (2) an intrinsic viscosity [η] is in the range of 0.01 to 10 dl/g as measured in a decalin solution at 135° C. The polymer of the present invention may be molded by a LIM molding, an injection molding, a transfer molding, a compression molding, and the like, and is excellent in acid resistance, gas permeation resistance, hydrolysis resistance, and dynamic fatigue resistance. From the polymer, a thermoplastic resin composition and a crosslinkable resin composition, and a crosslinked composition having excellent mechanical characteristics are obtained.
摘要:
The present invention provides a lubricating oil composition having excellent low temperature viscosity properties suitable for engine oils for automobiles and industries, gear oils, shock absorber oils, hydraulic fluids and it also provides a lubricating oil for internal-combustion engines formed from the composition.The lubricating oil composition comprises; a lubricating oil base (A) having a kinematic viscosity at 100° C. of 1 to 50 mm2/s and a viscosity index of not less than 80, an ethylene•propylene copolymer (B) having the following properties (B1) to (B4) such that (B1) the ethylene content is from 30 to 75% by weight, (B2) the intrinsic viscosity [η] is from 1.3 to 2.0 dl/g, (B3) the Mw/Mn is not more than 2.4 and (B4) the melting point as measured with DSC is not higher than 30° C., and optionally a pour point depressant (C).