公开(公告)号:US09918898B2
公开(公告)日:2018-03-20
申请号:US13780754
申请日:2013-02-28
Applicant: Corning Incorporated
Inventor: Andrei Gennadyevich Fadeev , Theresa Chang , Dana Craig Bookbinder , Santona Pal , Chandan Kumar Saha , Steven Edward DeMartino , Christopher Lee Timmons , John Stephen Peanasky
IPC: A61J1/00 , B65D65/42 , B65D23/08 , B65D25/14 , C03C17/30 , C03C17/32 , C09D179/08 , C03C17/00 , C03C17/42 , C03C21/00 , A61J1/14
CPC classification number: A61J1/1468 , A61J1/00 , B65D23/0814 , B65D23/0821 , B65D25/14 , B65D25/34 , B65D65/42 , C03C17/005 , C03C17/30 , C03C17/32 , C03C17/42 , C03C21/002 , C03C2217/78 , C03C2218/111 , C09D179/08 , Y10T428/1321 , Y10T428/24942
Abstract: Low-friction coatings and glass articles with low-friction coatings are disclosed. According to one embodiment, a coated glass article may include a glass body comprising a first surface and a low-friction coating positioned on at least a portion of the first surface of the glass body. The low-friction coating may include a polymer chemical composition. The coated glass article may be thermally stable at a temperature of at least about 260° C. for 30 minutes. A light transmission through the coated glass article may be greater than or equal to about 55% of a light transmission through an uncoated glass article for wavelengths from about 400 nm to about 700 nm. The low-friction coating may have a mass loss of less than about 5% of its mass when heated from a temperature of 150° C. to 350° C. at a ramp rate of about 10° C./minute.
-
公开(公告)号:US09725357B2
公开(公告)日:2017-08-08
申请号:US14248868
申请日:2014-04-09
Applicant: CORNING INCORPORATED
Inventor: Kaveh Adib , Robert Alan Bellman , Shandon Dee Hart , Guangli Hu , Robert George Manley , Prantik Mazumder , Chandan Kumar Saha
IPC: C03C17/34 , C03C17/36 , G06F3/041 , B32B17/06 , C03C3/083 , C03C15/00 , C03C17/22 , C03C17/245 , C03C21/00 , C03C23/00
CPC classification number: C03C17/3452 , B32B17/064 , C03C3/083 , C03C15/00 , C03C17/22 , C03C17/245 , C03C17/3417 , C03C17/3435 , C03C17/36 , C03C17/3607 , C03C17/3621 , C03C21/002 , C03C23/0055 , C03C2217/213 , C03C2217/214 , C03C2217/241 , C03C2217/425 , C03C2217/78 , C03C2217/948 , C03C2218/153 , C03C2218/17 , C03C2218/31 , C03C2218/32 , G06F3/041 , Y10T428/24983
Abstract: One or more aspects of the disclosure pertain to an article including a film disposed on a glass substrate, which may be strengthened, where the interface between the film and the glass substrate is modified, such that the article has an improved average flexural strength, and the film retains key functional properties for its application. Some key functional properties of the film include optical, electrical and/or mechanical properties. In one or more embodiments, the interface exhibits an effective adhesion energy of about less than about 4 J/m2. In some embodiments, the interface is modified by the inclusion of a crack mitigating layer containing an inorganic material between the glass substrate and the film.
-
公开(公告)号:US09668936B2
公开(公告)日:2017-06-06
申请号:US14812898
申请日:2015-07-29
Applicant: Corning Incorporated
Inventor: Andrei Gennadyevich Fadeev , Theresa Chang , Dana Craig Bookbinder , Santona Pal , Chandan Kumar Saha , Steven Edward DeMartino , Christopher Lee Timmons , John Stephen Peanasky
IPC: A61J1/00 , B65D65/42 , B65D23/08 , B65D25/14 , C03C17/30 , C03C17/32 , C09D179/08 , C03C17/00 , C03C17/42 , C03C21/00 , A61J1/14
CPC classification number: A61J1/1468 , A61J1/00 , B65D23/0814 , B65D23/0821 , B65D25/14 , B65D25/34 , B65D65/42 , C03C17/005 , C03C17/30 , C03C17/32 , C03C17/42 , C03C21/002 , C03C2217/78 , C03C2218/111 , C09D179/08 , Y10T428/1321 , Y10T428/24942
Abstract: Coated pharmaceutical packages are disclosed. In embodiments, a coated pharmaceutical package may include a glass body comprising a first surface. A low-friction coating may be positioned on at least a portion of the first surface of the glass body. The low-friction coating may include a polymer chemical composition. The coated pharmaceutical package may be thermally stable at a temperature of at least about 260° C. for 30 minutes. The low-friction coating may have a mass loss of less than about 5% of its mass when heated from a temperature of 150° C. to 350° C. at a ramp rate of about 10° C./minute.
-
公开(公告)号:US20160207825A1
公开(公告)日:2016-07-21
申请号:US14915400
申请日:2014-08-27
Applicant: CORNING INCORPORATED
Inventor: Matthew Lee Black , Charles Andrew Paulson , Chandan Kumar Saha
CPC classification number: C03C17/009 , C03C21/002 , C03C2217/445 , C03C2217/475 , C03C2217/78
Abstract: One or more aspects of the disclosure pertain to a laminates including a substrate, such as a glass substrate, which may be strengthened, or a sapphire substrate, and a polymeric scratch resistant layer disposed on the substrate. In one or more embodiments, where a glass substrate is utilized, the average flexural strength of the glass substrate is maintained when combined with the polymeric scratch resistant layer. The polymeric scratch resistant layer may include a polymeric diamond-like carbon. In one or more embodiments, the polymeric scratch resistant layer forms a shearable interface with the glass substrate or comprises a plurality of sub-layers and a plurality of shearable interfaces between such plurality of sub-layers. Methods for forming such laminates are also disclosed.
Abstract translation: 本公开的一个或多个方面涉及包括可被加强的基底(例如玻璃基底)或蓝宝石基底的层压体,以及设置在基底上的聚合物抗划伤层。 在使用玻璃基板的一个或多个实施例中,当与聚合物耐刮擦层组合时,保持玻璃基板的平均弯曲强度。 聚合物耐刮擦层可以包括聚合物类金刚石碳。 在一个或多个实施例中,聚合物耐刮擦层与玻璃基底形成可剪切的界面,或者包括多个子层和多个子层之间的多个可剪切界面。 还公开了形成这种层压板的方法。
-
公开(公告)号:US09327871B2
公开(公告)日:2016-05-03
申请号:US14057697
申请日:2013-10-18
Applicant: Corning Incorporated
Inventor: Andrei Gennadyevich Fadeev , Theresa Chang , Dana Craig Bookbinder , Santona Pal , Chandan Kumar Saha , Steven Edward DeMartino , Christopher Lee Timmons , John Stephen Peanasky , Robert Anthony Schaut , Paul Stephen Danielson , Melinda Ann Drake , Robert Michael Morena , Kaveh Adib , James Patrick Hamilton , Susan Lee Schiefelbein
IPC: B28B11/00 , B28B21/00 , A47G19/22 , B65D23/08 , B65D1/40 , C03C17/00 , C03C17/30 , C03C17/32 , C03C17/42 , C03C21/00 , C09D179/08 , C08G73/10 , B32B17/06 , B65D25/14
Abstract: Delamination resistant glass containers with heat-tolerant coatings are disclosed. In one embodiment, a glass container may include a glass body having an interior surface, an exterior surface and a wall thickness extending from the exterior surface to the interior surface. At least the interior surface of the glass body is delamination resistant. The glass container may further include a heat-tolerant coating positioned on at least a portion of the exterior surface of the glass body. The heat-tolerant coating may be thermally stable at temperatures greater than or equal to 260° C. for 30 minutes.
-
公开(公告)号:US20150360999A1
公开(公告)日:2015-12-17
申请号:US14812898
申请日:2015-07-29
Applicant: Corning Incorporated
Inventor: Andrei Gennadyevich Fadeev , Theresa Chang , Dana Craig Bookbinder , Santona Pal , Chandan Kumar Saha , Steven Edward DeMartino , Christopher Lee Timmons , John Stephen Peanasky
CPC classification number: A61J1/1468 , A61J1/00 , B65D23/0814 , B65D23/0821 , B65D25/14 , B65D25/34 , B65D65/42 , C03C17/005 , C03C17/30 , C03C17/32 , C03C17/42 , C03C21/002 , C03C2217/78 , C03C2218/111 , C09D179/08 , Y10T428/1321 , Y10T428/24942
Abstract: Coated pharmaceutical packages are disclosed. In embodiments, a coated pharmaceutical package may include a glass body comprising a first surface. A low-friction coating may be positioned on at least a portion of the first surface of the glass body. The low-friction coating may include a polymer chemical composition. The coated pharmaceutical package may be thermally stable at a temperature of at least about 260° C. for 30 minutes. The low-friction coating may have a mass loss of less than about 5% of its mass when heated from a temperature of 150° C. to 350° C. at a ramp rate of about 10° C./minute.
Abstract translation: 公开了涂覆的药物包装。 在实施方案中,涂覆的药物包装可以包括包含第一表面的玻璃体。 低摩擦涂层可以位于玻璃体的第一表面的至少一部分上。 低摩擦涂层可以包括聚合物化学组成。 涂覆的药物包装可以在至少约260℃的温度下热稳定30分钟。 当以约10℃/分钟的升温速度从150℃升温至350℃时,低摩擦涂层的质量损失小于其质量的约5%。
-
公开(公告)号:US20140001076A1
公开(公告)日:2014-01-02
申请号:US13827732
申请日:2013-03-14
Applicant: CORNING INCORPORATED
Inventor: Andrei Gennadyevich Fadeev , Theresa Chang , Dana Craig Bookbinder , Santona Pal , Chandan Kumar Saha , Steven Edward DeMartino , Christopher Lee Timmons , John Stephen Peanasky , Robert Anthony Schaut , Paul Steven Danielson , Melinda Ann Drake , Robert Michael Morena , Kaveh Adib
IPC: B65D1/40
CPC classification number: B65D23/0814 , A61J1/1468 , B32B17/06 , B65D1/40 , B65D25/14 , C03C3/087 , C03C17/005 , C03C17/30 , C03C17/32 , C03C17/3405 , C03C17/42 , C03C21/002 , C03C2217/78 , C03C2218/111 , C08G73/105 , C08G73/1071 , C09D179/08 , C08K5/544
Abstract: Delamination resistant glass containers with heat-tolerant coatings are disclosed. In one embodiment, a glass container may include a glass body having an interior surface, an exterior surface and a wall thickness extending from the exterior surface to the interior surface. At least the interior surface of the glass body is delamination resistant. The glass container may further include a heat-tolerant coating positioned on at least a portion of the exterior surface of the glass body. The heat-tolerant coating may be thermally stable at temperatures greater than or equal to 260° C. for 30 minutes.
-
公开(公告)号:US20130171456A1
公开(公告)日:2013-07-04
申请号:US13780740
申请日:2013-02-28
Applicant: Corning Incorporated
Inventor: Andrei Gennadyevich Fadeev , Theresa Chang , Dana Craig Bookbinder , Santona Pal , Chandan Kumar Saha , Steven Edward DeMartino , Christopher Lee Timmons , John Stephen Peanasky
IPC: B32B17/06
CPC classification number: A61J1/1468 , A61J1/00 , B65D23/0814 , B65D23/0821 , B65D25/14 , B65D25/34 , B65D65/42 , C03C17/005 , C03C17/30 , C03C17/32 , C03C17/42 , C03C21/002 , C03C2217/78 , C03C2218/111 , C09D179/08 , Y10T428/1321 , Y10T428/24942
Abstract: Low-friction coatings and glass articles with low-friction coatings are disclosed. According to one embodiment, a coated glass article may include a glass body comprising a first surface and a low-friction coating positioned on at least a portion of the first surface of the glass body. The low-friction coating may include a polymer chemical composition. The coated glass article may be thermally stable at a temperature of at least about 260° C. for 30 minutes. A light transmission through the coated glass article may be greater than or equal to about 55% of a light transmission through an uncoated glass article for wavelengths from about 400 nm to about 700 nm. The low-friction coating may have a mass loss of less than about 5% of its mass when heated from a temperature of 150° C. to 350° C. at a ramp rate of about 10° C./minute.
-
-
-
-
-
-
-