摘要:
A magnetic recording medium 1 includes a substrate 11; and a metallic glassy layer 12 that is arranged on the substrate 11 and has a plurality of convex portions 12A and concave portions 12B. The metallic glassy layer 12 has a chemical composition represented by any one of the formulae (1) to (3): FemPtnSixByPz (wherein, 20
摘要:
An amorphous alloy has a specific composition of FeaBbSicPxCuy. Here, the values a-c, x, and y meet such conditions that 73 at %≦a≦85 at %, 9.65 at %≦b≦22 at %, 9.65 at %≦b+c≦24.75 at %, 0.25 at %≦x≦5 at %, 0 at %≦y≦0.35 at %, and 0≦y/x≦0.5.
摘要:
A soft magnetic alloy contains P, B, and Cu as essential components. As a preferred example, an Fe-based alloy contains Fe of 70 atomic % or more, B of 5 atomic % to 25 atomic %, Cu of 1.5 atomic % or less (excluding zero), and P of 10 atomic or less (excluding zero).
摘要:
A second antiferromagnetic layer formed on a free magnetic layer has a blocking temperature lower than that of a first antiferromagnetic layer. The exchange anisotropic magnetic field between the free magnetic layer and the second antiferromagnetic layer is smaller than the exchange anisotropic magnetic field between the first antiferromagnetic layer and the pinned magnetic layer. By applying an annealing treatment utilizing the blocking temperature difference between the first and second antiferromagnetic layers, the magnetization direction and the strength of the pinned magnetic layer and the free magnetic layer can be controlled appropriately.
摘要:
A magnetoresistive sensor includes a plurality of multilayered magnetoresistive films arranged in parallel. Each multilayered magnetoresistive film includes at least one pinned ferromagnetic layer and at least one free magnetic layer. Reversion of magnetization of the pinned ferromagnetic layer is pinned, whereas the vector of magnetization of the free ferromagnetic layer freely reverses in response to an external magnetic field. The vectors of magnetization of the pinned ferromagnetic layers in two adjacent multilayered magnetoresistive films are substantially antiparallel to each other.
摘要:
A hard magnetic alloy obtained by heat treatment, at a heating rate of 20° C./min or more, of a glassy alloy containing Fe as a main component, at least one element R selected from the rare earth elements, at least one selected from Ti, Zr, Hf, V, Nb, Ta, Cr, Mo, W, and Cu, and B, and having a supercooled liquid region having a temperature width &Dgr;Tx of 20° C. or more, which is represented by the equation &Dgr;Tx=Tx−Tg (wherein Tx indicates the crystallization temperature, and Tg indicates the glass transition temperature), and a sintered compact, a cast magnet, a stepping motor and a speaker each of which includes the hard magnetic alloy.
摘要:
The present invention provides a method of producing a glassy alloy which has soft magnetism at room temperature and high resistivity and which can be easily obtained in a bulk shape thicker than an amorphous alloy ribbon obtained by a conventional melt quenching method. In this method, a melted metal having a supercooled liquid temperature width .DELTA.T.sub.x of 35.degree. C. or more, which is expressed by the equation .DELTA.T.sub.x =T.sub.x -T.sub.g (wherein T.sub.x indicates the crystallization temperature, and T.sub.g indicates the glass transition temperature), is sprayed on a cooling body under movement to form a ribbon-shaped glassy alloy material; and the glassy alloy is then heat-treated by heating at a heating rate of 0.15 to 3.degree. C./sec and then cooling.
摘要:
Hard magnetic materials of the present invention contain at least one element of Fe, Co and Ni as a main component, at least one element M of Zr, Nb, Ta and Hf, at least one rare earth element R and B. The texture of the materials has at least 70% of fine crystalline phase having an average grain size of 100 nm or less, and the residue having an amorphous phase, the fine crystalline phase mainly composed of bcc-Fe or bcc-Fe compound, Fe--B compound and/or R.sub.2 Fe.sub.14 B.sub.1.
摘要:
A soft magnetic alloy thin film includes a fine crystalline phase and an amorphous phase. The fine crystalline phase includes an average crystalline grain size of 10 nm or less in diameter and has body-centered cubic structure mainly composed of Fe. The amorphous phase has a nitrogen (N) compound as the main composition and occupies at least 50% of the structure of the thin film. An element M is incorporated at least in the amorphous phase, and includes at least one element selected from the group consisting of Ti, Zr, Hf, V, Nb, Ta, W, and rare earth metal elements. A plane-type magnetic device is made using this thin film.
摘要:
An Fe-based soft magnetic alloy having a high saturated magnetic flux density and having a composition represented by formula (I) below: (Fe.sub.1-a Q.sub.a).sub.b B.sub.x T.sub.y T'.sub.z (I) wherein Q represents at least one element selected from the group consisting of Co and Ni; T represents at least one element selected from the group consisting of Ti, Zr, Hf, V, Nb, Ta, Mo and W, with Zr and/or Hf being always included; T' represents at least one element selected from the group consisting of Cu, Ag, Au, Ni, Pd and Pt; a, b, x, y and z are real numbers satisfying relationships below: 0.ltoreq.a.ltoreq.0.05, 0.ltoreq.b.ltoreq.93 atomic %, 0.5.ltoreq.x.ltoreq.16 atomic %, 4.ltoreq.y.ltoreq.10 atomic %, 0.ltoreq.z.ltoreq.4.5 atomic % provided that when 0
摘要翻译:具有高饱和磁通密度且具有由下式(I)表示的组成的Fe基软磁合金:(Fe1-aQa)bBxTyT'z(I)其中Q表示选自以下的至少一种元素: Co和Ni; T表示选自Ti,Zr,Hf,V,Nb,Ta,Mo和W中的至少一种元素,其中始终包括Zr和/或Hf; T'表示选自Cu,Ag,Au,Ni,Pd和Pt中的至少一种元素; a,b,x,y和z是满足以下关系的实数:0 = a = 0.05,0