Laser-assisted alignment of multi-station flexographic printing system
    61.
    发明授权
    Laser-assisted alignment of multi-station flexographic printing system 有权
    多台柔版印刷系统的激光辅助校准

    公开(公告)号:US09021952B2

    公开(公告)日:2015-05-05

    申请号:US13851929

    申请日:2013-03-27

    申请人: Steven A. Miller

    发明人: Steven A. Miller

    摘要: A multi-station flexographic printing system includes a plurality of flexographic printing stations. Each flexographic printing station includes a flexo master. Each flexo master comprises a Fresnel zone pattern in a unique position. A method of aligning a plurality of flexographic printing stations includes printing a Fresnel zone pattern on a substrate in a unique position for each flexographic printing station. Light is directed through the Fresnel zone patterns on the substrate. The light focused by the Fresnel zone patterns is captured with a sensor device.

    摘要翻译: 多台柔版印刷系统包括多个柔版印刷台。 每个柔版印刷机包括柔版印刷机。 每个柔印版主包括一个独特位置的菲涅尔区域图案。 对准多个柔性版印刷站的方法包括在每个柔性版印刷台的唯一位置上在基底上印刷菲涅耳区图案。 光通过基片上的菲涅尔区域图案。 由菲涅尔区域图案聚焦的光被传感器装置捕获。

    Process for preparing metal powders having low oxygen content, powders so-produced and uses thereof
    64.
    发明授权
    Process for preparing metal powders having low oxygen content, powders so-produced and uses thereof 有权
    具有低氧含量的金属粉末的制备方法,如此制备的粉末及其用途

    公开(公告)号:US08226741B2

    公开(公告)日:2012-07-24

    申请号:US12444263

    申请日:2007-10-03

    IPC分类号: B22F1/00

    摘要: The present invention is directed to a process for the preparation of a metal powder having a purity at least as high as the starting powder and having an oxygen content of 10 ppm or less comprising heating said metal powder containing oxygen in the form of an oxide, with the total oxygen content being from 50 to 3000 ppmf in an inert atmosphere at a pressure of from 1 bar to 10−7 to a temperature at which the oxide of the metal powder becomes thermodynamically unstable and removing the resulting oxygen via volatilization. The metal powder is preferably selected from the group consisting of tantalum, niobium, molybdenum, hafnium, zirconium, titanium, vanadium, rhenium and tungsten. The invention also relates to the powders produced by the process and the use of such powders in a cold spray process.

    摘要翻译: 本发明涉及制备纯度至少与起始粉末一样高且氧含量为10ppm以下的金属粉末的方法,包括加热含氧形式的氧的金属粉末, 其总氧含量为50-3000ppmf,在惰性气氛中,压力为1bar至10-7至金属粉末的氧化物变为热力学不稳定的温度,并通过挥发除去所得氧。 金属粉末优选选自钽,铌,钼,铪,锆,钛,钒,铼和钨。 本发明还涉及通过该方法生产的粉末和在冷喷涂方法中使用这种粉末。

    METHOD FOR COATING A SUBSTRATE AND COATED PRODUCT
    66.
    发明申请
    METHOD FOR COATING A SUBSTRATE AND COATED PRODUCT 审中-公开
    涂覆基材和涂层产品的方法

    公开(公告)号:US20100015467A1

    公开(公告)日:2010-01-21

    申请号:US12513715

    申请日:2007-10-12

    摘要: Disclosed is a method of applying coatings to surfaces, wherein a gas flow forms a gas-powder mixture with a powder of a material selected from the group consisting of niobium, tantalum, tungsten, molybdenum, titanium, zirconium, nickel, cobalt, iron, chromium, aluminum, silver, copper, mixtures of at least two thereof or their alloys with at least two thereof or with other metals, the powder has a particle size of from 0.5 to 150 μm, an oxygen content of less than 500 ppm oxygen and a hydrogen content of less than 500 ppm, wherein a supersonic speed is imparted to the gas flow and the jet of supersonic speed is directed onto the surface of an object. The coatings prepared are used, for example, as corrosion protection coatings.

    摘要翻译: 公开了一种将表面涂覆的方法,其中气流与选自铌,钽,钨,钼,钛,锆,镍,钴,铁等的材料的粉末形成气体 - 粉末混合物, 铬,铝,银,铜,其至少两种的混合物或其合金与其至少两种或与其它金属的混合物,粉末的粒度为0.5-150μm,氧含量小于500ppm氧, 氢含量小于500ppm,其中超声速度被赋予气流,并且超音速喷射被引导到物体的表面上。 所制备的涂层例如用作防腐蚀涂层。

    Close-coupled atomization utilizing non-axisymmetric melt flow
    67.
    发明授权
    Close-coupled atomization utilizing non-axisymmetric melt flow 失效
    使用非轴对称熔体流动的近耦合雾化

    公开(公告)号:US5601781A

    公开(公告)日:1997-02-11

    申请号:US415914

    申请日:1995-06-22

    IPC分类号: B22F9/08 C23C4/12

    摘要: Close-coupled atomization systems and methods employing axisymmetric fluid flow and non-axisymmetric melt guide tube exit orifice configuration have demonstrated superior efficiency in the production of fine superalloy powder, such as, for example, nickel base superalloys compared to conventional close-coupled atomization utilizing an axisymmetric annular gas orifice and an axisymmetric guide melt guide tube exit orifice configuration.

    摘要翻译: 使用轴对称流体流动和非轴对称熔体引导管出口孔结构的近耦合雾化系统和方法已经证明了与常规的紧密耦合的雾化利用相比,在细的超级合金粉末(例如镍基超级合金)的生产中具有优异的效率 轴对称环形气体孔口和轴对称引导熔体导管出口孔构造。

    Integral induction heating of close coupled nozzle
    68.
    发明授权
    Integral induction heating of close coupled nozzle 失效
    紧耦合喷嘴的积分感应加热

    公开(公告)号:US5366204A

    公开(公告)日:1994-11-22

    申请号:US898602

    申请日:1992-06-15

    IPC分类号: B22F9/08

    摘要: A method for improved atomization of molten metal having a melting point above 1000.degree. C. is taught. The atomization is carried out in close coupled atomizer. The melt to be atomized is supplied from a reservoir where it is heated to a temperature slightly above the melting point. The molten metal from the reservoir is guided to the atomization zone by a ceramic melt guide tube. The atomization is accomplished with the aid of a shallow draft atomizing nozzle. The melt in the melt guide tube is heated with the aid of an induction coil which is disposed thereabout and between the reservoir and the shallow draft gas nozzle.